1-20 of 388 Search Results for

drilling components

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2002) 51 (7): SS-857.
Published: 01 July 2002
... procedures, and in make-and-break tests on STABALLOY AG17 Filing Code: SS-857 Stainless Steel July 2002 STABALLOY AG17 (Nonmagnetic Drilling Component Alloy) Staballoy AG17 is a very high manganese stainless steel developed for severe service in downhole drilling conditions. Staballoy AG17 and Datalloy 2...
Journal Articles
Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... beryllium-nickel casting alloy that has been in use for over 40 years. Its many uses include tooling for plastics, glass-mold tooling, fuel-pump impellers, cores for Teflon molding and deep sour-well drilling components. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2002) 51 (9): SS-862.
Published: 01 September 2002
... Datalloy 2 is an enhanced corrosion-resistant nonmagnetic stainless steel. The composition contains a high level of manganese and nitrogen to stabilize the austenite. Applications include replacement of standard chromium-manganese steels in drill string components. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (11): SS-868.
Published: 01 November 2002
... Staballoy AG 17 HS is an improved version of Staballoy AG 17 (see Alloy Digest SS-857, July 2002) with similar characteristics, but with higher yield strength and better fatigue properties. Applications include critical nonmagnetic drill stem components. This datasheet provides information...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
..., tough and readily fabricated with equipment and facilities suited to its high strength. It has a minimum yield strength of 100,000 psi. Among its many uses are structural components in heavy-duty trailers, buildings, bridges. ships, mobile drilling rigs and pressure vessels. *ARMCO and SS 100...
Journal Articles
Alloy Digest (1999) 48 (6): SS-748.
Published: 01 June 1999
... stainless steel commonly used for such applications. The strength of SCF 19 alloy is achieved by warm working on a rotary forge at a temperature below the recrystallization temperature. SCF 19 alloy has been used for many oil and gas well drilling components, including drill collars, stabilizers, and MWD...
Journal Articles
Alloy Digest (2015) 64 (9): Ni-723.
Published: 01 September 2015
.... The alloy is also a candidate for oil and gas industry applications because of its good combination of strength and corrosion resistance. Nonmagnetic oil drilling components, such as drill collars, stabilizers, and measuring/logging-while drilling (MWD/LWD) housings, are typically made using Cr-Mn-N...
Journal Articles
Alloy Digest (2002) 51 (1): Ti-125.
Published: 01 January 2002
..., brine concentration/evaporation units, geothermal brine energy extraction equipment, and offshore/on hydrocarbon production/drilling components. Producer: RMI Titanium Company 1000 Warren Ave. Niles, OH 44446 (330) 652-9952 ISSN: 002-614X Ti-125B ...
Journal Articles
Alloy Digest (2015) 64 (6): SS-1214.
Published: 01 June 2015
... by the ASTM A262 practice E test. Subjecting the exposed surfaces to compressive treatments reduces transgranular stress corrosion tendencies. Material integrity is controlled by ultrasonic inspection per API Spec 7-1 and NS-1. Designed for most drill string components such as drill collars, MWD and LWD...
Journal Articles
Alloy Digest (1975) 24 (9): Zn-22.
Published: 01 September 1975
... NJZ ALLOY No. 25 is a zinc-copper-titanium alloy that offers outstanding high creep resistance and a low coefficient of expansion. It can be severely work hardened. Its applications include architectural building products, sporting equipment components, hardware and automotive trim. This datasheet...
Journal Articles
Alloy Digest (1970) 19 (3): SA-250.
Published: 01 March 1970
... REPUBLIC RSM 250 is an 18% nickel-cobalt-molybdenum age-hardening steel designed to develop 250,000 psi yield strength with good toughness. It is recommended where a combination of strength, toughness and notch resistance is required such as aircraft landing gears and jet engine components...
Journal Articles
Alloy Digest (1969) 18 (6): Ti-58.
Published: 01 June 1969
... Ti-5A1-4FeCr is an alpha-beta type titanium alloy recommended for airframe components. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (2012) 61 (7): SA-658.
Published: 01 July 2012
... RUUKKI RAEX 500 (typical yield strength 1250 MPa) is part of the Raex family of high-strength and wear-resistant steels with favorable hardness and impact toughness to extend life and decrease wear in structural components. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2016) 65 (9): SA-765.
Published: 01 September 2016
.... Machinability: The producer recommends any drilling take place in a machining center using an ultra-hard metal alloy drill. However, for small jobs and working with components, it is often the case that boor-bank drilling machines and high-speed steel drills are used. Below is the recommended approach...
Journal Articles
Alloy Digest (1975) 24 (11): Cu-303.
Published: 01 November 1975
... ATLANTIC 8A Alloy is a cast manganese bronze offering an excellent combination of mechanical properties and resistance to corrosion in fresh and sea water. It is used for applications such as gears, marine hardware and waveguide components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1976) 25 (1): Zn-25.
Published: 01 January 1976
... NJZ Alloy No. 45 is a zinc-copper alloy characterized by high hardness and strength, good ductility and high stiffness. It work hardens easily. Among its many applications are hardware, sporting-equipment components, cable wrappings and watch cases. This datasheet provides information...
Journal Articles
Alloy Digest (1968) 17 (10): Co-56.
Published: 01 October 1968
... HOWMET No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. It is recommended for bushings, scrapers, valve parts, and other machinery components. This datasheet provides information...
Journal Articles
Alloy Digest (2017) 66 (7): SA-790.
Published: 01 July 2017
... Steel HT10 contains lead to make it easier to form, cut, mill, and drill. Applications are in the watch industry. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming. Filing Code: SA-790. Producer or source...
Journal Articles
Alloy Digest (1982) 31 (8): Zn-38.
Published: 01 August 1982
... 10 36000-38000 18 Reverse-bend test (5 x 108 cycles), psi 8C00 Rotating-beam test (5 x 108 cycles), psi 15000 Permanent- Mold Cast 45000-5cWO 31000-32000 1-3 105-125 36000-38ooO - 8imo 15ooo Table 2 - GENERAL SPEED AND FEED RECOMMENDATIONS FOR MACHINlNG ALLOY ZA-12 Drilling: Drilling speeds...
Journal Articles
Alloy Digest (1970) 19 (5): Ni-153.
Published: 01 May 1970
... NIMONIC 93 is a nickel-base alloy having high elevated temperature strength, high oxidation resistance and good corrosion resistance. It is recommended for jet engine and gas turbine components. This datasheet provides information on composition, physical properties, hardness, elasticity...