Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
... Kaiser Alloy 6063 is a magnesium/silicon alloy. One of the most popular of the heat treatable alloy group. Products include extruded and drawn tube, pipe, rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-711.
Published: 01 March 2004
... Wieland-M20 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn products such as lipstick cases. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2002) 51 (3): Cu-678.
Published: 01 March 2002
... Wieland-N37 is a leaded nickel silver with excellent machining properties. It is available either as an extruded or drawn product. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat...
Journal Articles
Alloy Digest (2018) 67 (7): Cu-876.
Published: 01 July 2018
... Wieland-K14 is a machinable high-copper alloy available as extruded and drawn products. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2015) 64 (9): Cu-841.
Published: 01 September 2015
... Wieland-SW1 is a lead-free special brass made in extruded and drawn products. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-716.
Published: 01 June 2004
... Wieland-M37 has excellent cold-working properties and corrosion resistance. The alloy is used in the deep-drawn and stamped condition for electrical products. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... Wieland C21000, also known as gilding metal, is a 95Cu-5Zn alloy. This versatile, low-cost alloy is often the choice of engineers for deep drawn parts such as bullet jackets and coined products. The combination of moderate conductivity and improved strength make C21000 a valuable option...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1989) 38 (5): CS-124.
Published: 01 May 1989
... UNS G10370 is a medium carbon, plain carbon steel. In bar form the steel is often used in the as-hot rolled condition. Cold drawn bars have attractive combinations of mechanical and dimensional properties and are widely used in mass production of machined and other parts. UNS G10370 is also used...
Journal Articles
Alloy Digest (2004) 53 (5): Cu-714.
Published: 01 May 2004
... Wieland-M33 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn decorative products and in electrical components. The alloy is often called yellow brass, 65%. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (1960) 9 (6): Cu-89.
Published: 01 June 1960
... REVERE No. 140 is a copper-zinc alloy containing 20% zinc. It is recommended for deep drawn and cold formed products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2021) 70 (10): Cu-925.
Published: 01 October 2021
... as well as for a wide variety of drawn and formed parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating. Filing Code: Cu-925. Producer or source: Wieland Rolled...
Journal Articles
Alloy Digest (1990) 39 (6): CS-127.
Published: 01 June 1990
... UNS G10370 is a medium carbon, plain carbon steel. In bar form the steel is often used in the as-hot rolled condition. Cold drawn bars have attractive combinations of mechanical and dimensional properties and are widely used in mass production of machined and other parts. UNS G10370 is also used...
Journal Articles
Alloy Digest (2002) 51 (9): Cu-688.
Published: 01 September 2002
... and hardness, good wear and corrosion resist- ance, and a relatively high electrical conductivity. The alloy is good to hot stamp and forge, typically followed by precipitation hardening. Welding, brazing, and soldering may be performed. Product Forms Available: Delivery is in the form of extruded and drawn...
Journal Articles
Alloy Digest (2000) 49 (7): Cu-651.
Published: 01 July 2000
... mm with a tolerance of ±3% on nominal thickness. Widths are 5 100 mm with a tolerance range from 0 to +0.2 mm to ±0.4 mm depending on thickness. Other sizes are available on request. Extruded and drawn products include drawn rod in Condition C available in 10 80 mm diameter. Drawn rod in Condition D...
Journal Articles
Alloy Digest (1971) 20 (2): Cu-226.
Published: 01 February 1971
... equivalents. - 100 100 100 100 - - - - - - 100 - - - - - - - - - - DOI: 10.31399/asm.ad.cu0226 Copyright © ASM International® 1996 Form Strip, Rolled Strip. Drawn Flat Wire. Rolled FLAT Flat Wire. Drawn PRODUCTS Bar. Rolled Bar. Drawn Sheet Plate ROD \VIRE TUBE PIPE SHAPES Nominal Grain Size mm. Rolled...
Journal Articles
Alloy Digest (2004) 53 (7): Ti-134.
Published: 01 July 2004
...: Allvac 38-644 titanium alloy has good fabricability when form- ing in the hot or warm condition in the preheat range of 816 1038 °C (1500 1900 °F). Cold formability is very good, and ductility levels of 60 70% reduction in area (RA) for a 30% cold- drawn product are possible after solution annealing...
Journal Articles
Alloy Digest (2014) 63 (12): Co-124.
Published: 01 December 2014
... °F). Air cool. For optimum properties, cold worked KC35N alloy should be aged at 540 600 °C (1004 1112 °F). The influence of the treatment on annealed materials is negligible but becomes very important on cold drawn products. Weldability: This alloy can be successfully TIG welded. In general, welding...
Journal Articles
Alloy Digest (2009) 58 (4): Cu-768.
Published: 01 April 2009
...) On extruded/drawn products, soft annealed and cold worked (hard 30%) properties can be found in Table 1. Fig. 2 Dependence of the resistance on the temperature of FY2 Fig. 3 Long-term stability of the resistance at 140 °C (285 °F). Measurement at RT after X h heat influence at 140 °C (285 °F) Table 1...
Journal Articles
Alloy Digest (2013) 62 (12): Cu-829.
Published: 01 December 2013
... = Solution heat treated, calibrated. Guaranteed form tolerances. Table 2 Available product form Extruded and drawn products Material condition A, C, and G Material condition B, D, and F Round rod, diameter, mm (in.) 10.2 80.0 (0.40 3.15) 4.06 80.0 (0.16 3.15) 16.0 102 (0.63 4.00) Drawn Round wire, diameter...