1-20 of 38 Search Results for

drawability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1976) 25 (3): Zn-26.
Published: 01 March 1976
... NJZ Alloy No. 35 is a zinc-lead-cadmium-iron alloy possessing good ductility, bending and work-hardening characteristics with excellent drawability and formability. Its applications include jar caps and hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1970) 19 (9): Cu-219.
Published: 01 September 1970
... ALCOLOY ALLOY 688 is a high-strength cobalt-aluminum modified brass alloy with good drawability and formability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1975) 24 (11): Zn-23.
Published: 01 November 1975
... NJZ Alloy No. 30 is a zinc-lead-cadmium alloy that offers good ductility, low tensile strength and good drawability. Its applications include battery cans, cosmetic containers and hardware. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1976) 25 (11): Zn-29.
Published: 01 November 1976
... MICROZINC Alloy 190 is a zinc-copper alloy with good atmospheric corrosion resistance and a low coefficient of sliding friction to eliminate galling in service. It has maximum strength commensurate with good ductility and drawability. Processing differences give two commercial products or classes...
Journal Articles
Alloy Digest (2022) 71 (8): CS-229.
Published: 01 August 2022
... of these steel grades, strength and hardness will increase with increase in carbon and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1005 and C4C are widely used for lightly stressed parts where cold formability or drawability...
Journal Articles
Alloy Digest (2022) 71 (8): CS-228.
Published: 01 August 2022
... of these steel grades, strength and hardness will increase with increase in carbon and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1008 and C8C are widely used for lightly stressed parts where cold formability or drawability...
Journal Articles
Alloy Digest (2022) 71 (10): CS-232.
Published: 01 October 2022
... grade, both strength and hardness will increase with increase in carbon and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1006 is widely used for lightly stressed parts where cold formability or drawability is the primary...
Journal Articles
Alloy Digest (2017) 66 (2): SS-1257.
Published: 01 February 2017
... to SUS 304J1 General Characteristics: NSSC 27A is superior to SUS 304 in deep drawability and stretchability. NSSC 27AS exhibits high performance in formability by softening NSSC 27A. Product Forms Available: Sheet and strip Copyright © 2017, ASM International®. All rights reserved. SUMITOMO NSSC 27A...
Journal Articles
Alloy Digest (2001) 50 (11): Ni-575.
Published: 01 November 2001
... strength Yield strength, 0.2 Elongation, Alloy Condition Hardness MPa ksi MPa ksi % Magnifer Cold rolled(a) 350 HV5 1250 181 1250 181 3 8105 Deep drawable 160 HV5 700 102 310 45 32 or soft annealed(b) After final annealing 100 HV5 510 74 160 23 32 Magnifer Cold rolled(a) 365 HV1 1300 189 1300 189 1 8105 So...
Journal Articles
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
...(a) Alkr6naialm!al . . . . . 2so 17 240 9&110 x-63 (a) The quid ccdition deep drawable Q soft -shouldbcrpci6ed these diagrams are characteristic of the alloy in the heat-nested condition. The heat treatment is described ahove. Variations in theseheat~enentswiuresultinchangesinthepropertiesofthe alloy. The main...
Journal Articles
Alloy Digest (1976) 25 (12): Zn-30.
Published: 01 December 1976
... Company Copyright © ASM International® 1996 1996 ASM International castability chemical composition corrosion-resistant alloys creep properties drawability ductility fatigue properties hardness heat treatability high stiffness joinability machinability medallions NJZ ALLOY No. 55...
Journal Articles
Alloy Digest (1984) 33 (5): Fe-70.
Published: 01 May 1984
... induction. T(G) Saturation magnetostriction PROPERTIES Table 1 - MECHANICAL PROPERTIES Cold Rolled Deep Drawable* After Final Property About SO %c (Malleable Anneal) Anneal Tensile strength. psi (M Pa) 110000 (750) 80000 (560) 75000 (530) Yield point. psi (MPa) I00000 (700) 40000 (290) 30000 (220...
Journal Articles
Alloy Digest (1975) 24 (1): SA-312.
Published: 01 January 1975
... an indication of drawability; the flat bottom cup test gives an indication of stretchability and the Fukui Test an indication of formability in a stretch-draw operation. Heat Treatment: Maxi-Form 80 is used in the hot-rolled condition without an) further heat treatment. Machinability: The forms available...
Journal Articles
Alloy Digest (2013) 62 (11): SA-687.
Published: 01 November 2013
... is widely used for M steels, and this also permits smaller radii compared to those achieved when bending. Pressing. The high work hardening of M steels results in good stretchability and drawability. Usual consideration when designing details in Docol are to make the radii slightly larger and optimize...
Journal Articles
Alloy Digest (2010) 59 (3): SA-615.
Published: 01 March 2010
... can be used. General Characteristics: Docol 1000 LCE (LCE = low carbon equivalent) is a cold-rolled ultrahigh-strength dual-phase steel. The low carbon content means that the steel has excellent welding properties. Docol 1000 LCE also offers increased drawability. The steel is a dual- DOI: 10.31399...
Journal Articles
Alloy Digest (2007) 56 (12): Fe-142.
Published: 01 December 2007
...). Heat Treatment: For best dimensional stability, the alloy should be annealed 850 1000 °C (1562 1832 °F) under a protective atmosphere. Fabricability: After annealing, the cold-rolled strip has good drawability. See Table 3 for Erichsen test data. Weldability and Brazeability: Brazing. Hard brazing...
Journal Articles
Alloy Digest (1996) 45 (6): Fe-110.
Published: 01 June 1996
... atmosphere. Workability: All conventional processes can be used. Fabrication data may be obtained from the Table 1 on mechanical properties. in the deep drawable condition. the minimum Erichsen depth is 8 for sheets of 1 mm thickness. The magnetic. final-annealed condition is only the final condition...
Journal Articles
Alloy Digest (1972) 21 (10): SS-281.
Published: 01 October 1972
... of 200400 sfpm are used for roughing and finishing with tipped-carbide single point turning tools. Use sulphurized cutting oils. Workability: The alloy can be formed by bending, deep drawing and similar standard procedures. Its deep drawability can be characterized by an Erichsen cup depth of 8 mm...
Journal Articles
Alloy Digest (1972) 21 (6): SA-275.
Published: 01 June 1972
... drawability elasticity fatigue properties fracture toughness heat treatability joinability low-temperature alloys machinability physical properties shear strength tensile properties weldability workability Filing Code: SA-275 AWHF STEEL Steel-Alloy JUNE 1972 DIGESTa - DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (1968) 17 (10): SS-214.
Published: 01 October 1968
... of the chlorinated type. Workabi Iity: Very good drawability. The combination of low yield strength and high elongation permits successful forming of complex shapes. This steel work hardens ver) readily. To remove forming stresses in formed parts, full anneal- ing or stress-relieving heat treatment should be applied...