Alloy Digest (1976) 25 (1): TS-295.
Published: 01 January 1976
... APACHE is an air-hardening, cold-work die steel that exhibits less distortion during heat treatment than water or oil-hardening steel and many other air-hardening steels. Its low-distortion characteristic makes it attractive for applications where close size tolerance is important. This datasheet...
Journal Articles
Alloy Digest (1987) 36 (3): TS-472.
Published: 01 March 1987
... AL TECH APACHE is an air-hardening, cold-work die steel that exhibits less distortion during heat treatment than water or oil-hardening steels and most high-alloy, air-hardening die steels. Its low-distortion characteristic makes it particulary attractive for applications where close size...
Journal Articles
Alloy Digest (1989) 38 (8): SS-267.
Published: 01 August 1989
... SANDVIK 4C54 is a ferritic stainless steel with extremely good resistance to reducing sufurous gasses and to oxidation in air. It is useful to about 1100 C (2010 F) provided allowance is made for creep to avoid distortion due to its dead weight. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1989) 38 (10): SS-75.
Published: 01 October 1989
... ARMCO PH 15-7 Mo is a semi-austenitic stainless steel that is precipitation hardenable, providing high strength and hardness with minimum heat treat distortion. It has good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1990) 39 (1): P-14.
Published: 01 January 1990
... ISOPLAST 201 is an opaque, impact modified thermoplastic polyurethane engineering resin for extrusion and injection molding. Its high heat distortion temperature sets it apart from ISOPLAST 101(described in Alloy Digest P-10, October 1989). It has high notched impact strength, excellent chemical...
Journal Articles
Alloy Digest (1992) 41 (7): TS-511.
Published: 01 July 1992
... THYROTHERM 2799 is a maraging tool steel with extremely low heat treat distortion and high resistance to thermal shock and excellent weldability. The alloy also possesses resistance to heat checking a high work temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1976) 25 (12): TS-310.
Published: 01 December 1976
... DEWARD is an oil-hardening, non-deforming, manganese die steel that is characterized by uniformity, good machinability and satisfactory performance in service. Its composition permits a relatively low hardening temperature to give minimum distortion after heat treatment and little danger...
Journal Articles
Alloy Digest (1977) 26 (5): TS-318.
Published: 01 May 1977
... and distortion during heat treatment. Its well-balanced high-temperature mechanical properties make it useful for many other applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (2021) 70 (7): Al-478.
Published: 01 July 2021
... production problems, such as distortion, blistering, property variations, and heat treatment logistics. The application of this alloy is limited to simple-shaped components due to its high hot cracking tendency. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1968) 17 (6): TS-207.
Published: 01 June 1968
... AIR HARD is an air or oil hardening, high-carbon tool and die steel for minimum distortion after hardening. It is used for blanking and forming dies, rolls, punches, and other such applications where a deep hardening, non-deforming steel with good resistance to wear is desired. (Also furnished...
Journal Articles
Alloy Digest (2006) 55 (7): SS-967.
Published: 01 July 2006
... tool life, better surface finish, less distortion problems, more homogeneity in microstructures, and marginally increased resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1993) 42 (7): SS-547.
Published: 01 July 1993
... surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-547. Producer or source: Avesta Sheffield...
Journal Articles
Alloy Digest (1993) 42 (11): SS-553.
Published: 01 November 1993
...; better surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-553. Producer or source: Avesta...
Journal Articles
Alloy Digest (1993) 42 (12): SS-557.
Published: 01 December 1993
...; better surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-557. Producer or source: Avesta...
Journal Articles
Alloy Digest (1993) 42 (9): SS-549.
Published: 01 September 1993
... surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-549. Producer or source: Avesta Sheffield...
Journal Articles
Alloy Digest (1957) 6 (11): TS-64.
Published: 01 November 1957
... RY-DIE is an air-hardening tool and die steel of the 5% chromium type. Basically a general purpose air-hardening tool steel. It is designed for a wide variety of applications for which its safe hardening and minimum distortion characteristics or its excellent wear resistance are important...
Journal Articles
Alloy Digest (1958) 7 (3): SS-71.
Published: 01 March 1958
...-45. Cracking, distortion, decarburization, scaling and similar problems encountered after machining are virtually eliminated due to the low heat treatment temperature required for hardening. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1958) 7 (7): TS-72.
Published: 01 July 1958
... HWD No. 3 is an air-hardening hot work steel recommended for dies where a minimum amount of distortion during hardening is required. It is equivalent to AISI Type H13. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep...
Journal Articles
Alloy Digest (1978) 27 (8): TS-336.
Published: 01 August 1978
... SIMONDS D-2 is an air-hardening tool and die steel of the high-carbon, high-chromium type. It is characterized by high resistance to abrasion, fair toughness, minimum distortion in hardening and high compressive strength. Its many uses include a wide range of cutting and forming dies, rolls...
Journal Articles
Alloy Digest (1979) 28 (3): TS-346.
Published: 01 March 1979
... CYCLOPS SCK is a cold-work tool steel with a balanced composition to provide air hardening and an optimum combination of toughness, wear resistance and minimum distortion during heat treatment. Typical applications are shear blades, trimming dies and forming rolls, including grade rolls...