Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (2014) 63 (6): Cu-832.
Published: 01 June 2014
... BrushForm 158 is a spinodal alloy that develops exceptionally high elastic strength levels, dimensional stability, and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend...
Journal Articles
Alloy Digest (2018) 67 (8): ts-752.
Published: 01 August 2018
... Böhler (or Boehler) S590 is a high-speed steel with high-wear resistance, high-compressive strength, very good through-hardening properties, good toughness, good dimensional stability on heat treat, and very good temper resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (8): Cu-338.
Published: 01 August 1977
... outstanding advantages: (1) high thermal conductivity, (2) high hardness, (3) high resistance to oxidation and (4) good dimensional stability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1990) 39 (2): Cp-5.
Published: 01 February 1990
... ULTEM 2100, 2200, 2300 and 2400 resins have high heat resistance, inherent flame resistance with low smoke evolution, broad chemical resistance and outstanding processability. Glass reinforcment provides increased rigidity and dimensional stability while maintaining good processing features...
Journal Articles
Alloy Digest (1990) 39 (3): P-16.
Published: 01 March 1990
... LEXAN 500 series resins are tough, high-modulus polycarbonate resins. They have low mold shrinkage and excellent dimensional stability. This datasheet provides information on physical properties, hardness, tensile properties, and compressive and shear strength as well asfracture toughness...
Journal Articles
Alloy Digest (1977) 26 (3): TS-315.
Published: 01 March 1977
... UHB RIGOR AR is a chromium-molybdenum-vanadium tool steel characterized by high surface hardness, high hardenability, high dimensional stability after hardening and tempering, high compression resistance, good machinability, good resistance to tempering and good wear resistance. Its many uses...
Journal Articles
Alloy Digest (2004) 53 (11): CS-145.
Published: 01 November 2004
... Sandvik Bioline 20AP is a high-hardness alloy with dimensional stability and excellent machining properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: CS-145...
Journal Articles
Alloy Digest (2009) 58 (6): SA-601.
Published: 01 June 2009
... Ovako 146S is an ingot cast case-hardening steel with good dimensional stability and high toughness. This datasheet provides information on composition as well as fatigue. It also includes information on casting, heat treating, and machining. Filing Code: SA-601. Producer or source: Ovako North...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-588.
Published: 01 September 1993
... COPPER ALLOY NO. C72900 is a spinodal alloy that develops exceptionally high elastic strength levels; dimensional stability and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1958) 7 (1): Al-61.
Published: 01 January 1958
... APEX 417 is an aluminum-magnesium casting alloy having high strength and ductility, excellent corrosion resistance and good dimensional stability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... GUTERL D-7 is a high-carbon, high-chromium, high-vanadium tool and die steel. It is air hardening and therefore offers an extremely high degree of dimensional stability in heat treatment. In the hardened condition it has extremely high resistance to abrasion and wear. Its many applications include...
Journal Articles
Alloy Digest (1980) 29 (6): TS-364.
Published: 01 June 1980
... GUTERL A-2 is a high-hardenability cold-work tool and die steel with excellent non-deforming properties. It is air hardening and therefore exhibits a high degree of dimensional stability in heat treatment. It is recommended where the application requires a good combination of machinability, wear...
Journal Articles
Alloy Digest (1963) 12 (3): TS-131.
Published: 01 March 1963
... Orbit is a free-machining, low-alloy, air-hardening tool steel providing maximum dimensional stability. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1985) 34 (2): TS-436.
Published: 01 February 1985
... ARNE is a general-purpose, oil-hardening tool steel. It is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include: (1) Good machinability, (2) Good dimensional stability in hardening and (3) A good combination of high...
Journal Articles
Alloy Digest (1973) 22 (8): Al-208.
Published: 01 August 1973
... in combination with excellent wear resistance, dimensional stability, and high strength. Permanent molding is required to control properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1973) 22 (10): Al-15.
Published: 01 October 1973
... TENZALOY is an aluminum casting alloy developed for its high-strength and self-aging characteristics for castings that must have good dimensional stability and good corrosion resistance. Large and small intricate castings can be made without the danger of distortion associated with heat treatment...
Journal Articles
Alloy Digest (1988) 37 (3): TS-488.
Published: 01 March 1988
... COMPAX is a chromium-molybdenum shock-resistant tool steel characterized by high toughness, good wear resistance, good through hardening and good dimensional stability during hardening. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive...
Journal Articles
Alloy Digest (1984) 33 (1): Al-249.
Published: 01 January 1984
... ALUMINUM 712.0 is a high-strength aluminum casting alloy that is self aging at room temperature. It has good machinability, good dimensional stability and good resistance to corrosion and shock. Among its applications are marine castings, high-strength pressure-tight castings, aircraft components...
Journal Articles
Alloy Digest (2023) 72 (4): SS-1357.
Published: 01 April 2023
... Uddeholm RoyAlloy is a is a patented free machining stainless holder steel that is supplied in the prehardened condition. It is the preferred steel of choice of many mold makers and end users. The steel provides enhanced machinability, improved dimensional stability, and superior surface finish...