1-20 of 22 Search Results for

diesel exhaust valves

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (2): Ni-630.
Published: 01 February 2006
... Nicrofer 7016TiAl (also known as alloy 751) is an age-hardening Ni-Cr-Fe alloy with both good corrosion resistance and high rupture strength. It is a slight modification of alloy Nicrofer 7016TiNb (alloy X-750) and is used in diesel exhaust valves. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (5): SS-310.
Published: 01 May 1975
... CARPENTER 21-12 is an austenitic chromium-nickel stainless steel which offers an excellent combination of high-temperature strength and corrosion resistance for exhaust valve applications. It is used widely as the head material in two-piece valves for both diesel and gasoline engines...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (8): SS-316.
Published: 01 August 1975
... as the head material in two piece exhaust valves for both diesel and gasoline engines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (8): Ni-116.
Published: 01 August 1966
... INCONEL alloy 751 is a high-strength, high-temperature nickel-chromium alloy. It is essentially the same as INCONEL alloy X-750, except that its slightly modified composition imparts increased rupture properties at 1600 F. It is used for diesel engine exhaust valves. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (1): Ni-213.
Published: 01 January 1975
... ALLOY VMS-513 is a nickel-base alloy developed to meet the tough operating conditions of gasoline and diesel engines. It combines high-temperature strength with good resistance to corrosion and wear, plus good fatigue strength. It is used in valves for gasoline-fueled industrial engines...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (2): Ni-536.
Published: 01 February 1998
... Pyromet 31V is a sulfidation resistant, precipitation hardenable superalloy with unusual combination of corrosion resistance and strength to 816 C (1500 F). It has excellent resistance to hot sulfidation attack and has been used in truck and locomotive diesel valve service. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (2): SS-381.
Published: 01 February 1981
..., Thorndale, Pennsylvania. For plates less than 2-in. (51~mm) thick, consult the manufacturer. Applications: Diesel and gasoline internal-combustion-engine exhaust valves (especially for trucks and other heavy-duty engines), heat- treating furnace componenrs and tooling for the hot-press diffusion bonding...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (11): Ni-387.
Published: 01 November 1990
...) higher than NICKELVAC X-750, a result of its higher aluminum content (0.9-1.50 vs 0.4- 1 .O Heat treatment is shorter and simpler than that of NICKELVAC X-750. Forms Available: Bar Applications: Exhaust valves in diesel engines and conventional aircraft reciprocating engines. Manufacturer: Teledyne...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (11): Co-86.
Published: 01 November 1992
... tothccastcollntaparls.TlletypesofcarbidesplesentiuSTELLlTE 12PM. M6C and M7C3 are similar to those present in S lELL.ITB 12 cast Applkations: Typical qplicaticms include vane plugs, fuel metering pins, and spacer bushings for the aerospace industly. ball blanks and radt blanks for bearings; diesel exhaust components and fluid valve seats for valve seat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (2): Co-88.
Published: 01 February 1993
... plugs, fuel metering pins, and spacer bnsbings for the aaoqaccindustry;ballblanksandrack blanks for bearings: diesel exhaust componmts and fluid valve seats for valve seat W, saw cum insertr; and o&r wear parts. Producer: DdcrostdliteIllc. St Louis. MO 63105 /Tel: (314) 721-5573 Ill- D&m stdlite Inc...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (10): Co-94.
Published: 01 October 1993
... blanks and rack blanks for bearings; diesel exhaust components and fluid valve seats for valve seat inserts; saw cutter inserts; and other wear parts. Producer: Machining: STELLITE 190 PM can be machined with relative ease. Gen- erally, alloys having hardnesses less than Rc55 can almost always...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (10): Ni-776.
Published: 01 October 2021
... is for automotive There are several ways to heat treat ATI X-751, depending exhaust valves. It can also be used for many of the applica- upon what properties are to be maximized: tions for which ATI X-750 is used. For optimum creep-rupture strength, solution heat Supplier treating is done at 1150 °C (2100 °F...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (4): Co-91.
Published: 01 April 1993
....-IhetypesofurMespruentinSteBite6PM,l &C andM7C3arcsimilar~othosepm.semin~6~ Applications: TyPicslqPlicationsincludevMepluss.fuelmchugpim,md~ bushingsfadte~ccindumy,brllbhksadnckbhksfa bcaings; diesel exhaust annpataus and fluid valve seats fa v&e seUinsats:xwauerinsxtqaodothawexpuls. Produoar: DelolostdlimInc. St. Lamis. MO 63105...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (12): Ni-656.
Published: 01 December 2007
... 750 1382 69 10 78 11 800 1472 73 11 815 1499 27 3.9 29 4.2 30,000 650 1202 216 31 700 1292 108 16 750 1382 49 7.1 815 1499 20 2.9 shafts, combustion chambers for diesel engine exhaust and inlet valves, hot work tools, forging hammers, swaging dies, pressing tools, shear blades, springs, bolts...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (12): Co-87.
Published: 01 December 2019
... bushings for the aerospace induslry; ball blanks and rack blanks for bearings; diesel exhaust componmts and fluid valve seats for valve seal inserts; saw cutter inserts; and other wear parts. Producer: Welding: Thhe cob&-base alloys cm be welded by gas tungsten arc (GTA). gas metal arc (GMA). shielded...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (6): Co-92.
Published: 01 June 1993
... present in STELLITE 31 Cast Applications: Typical applications include vane plugs. fuel metering pins, and spacer bushings for the aerospace industry; ball blanks and rack blanks for bearings: diesel exhaust components and fluid valve seats for valve seat inserts; saw cutter inserts; and other wear parts...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
... blanks and rack blanks for bearings; diesel exhaust components and fluid valve seats for valve seat inserts; saw cutter inserts; and other wear parts. Producer: Deloro Stellite Inc. St. Louis. MO 63105-(314) 721-5573 In Canada: Deloro Stellite Inc. Bellevile. Gntario-(613) 968-3481 ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... the effects of chromium. During heat treatment, niobium, aluminum, and titanium form the precipitates required for strengthening. Potential appli- cations include advanced powder production boiler tubes and diesel-engine exhaust valves. This alloy is still under development. While the composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (11): SS-478.
Published: 01 November 1986
... to minimrze sensitivny to intergranular corrosion. Corrosion Resistance: When properly heat treated. the corrosion resistance of AISI No. 65 I is excellent up to I 250G F against all atmospheres encountered in aircraft. automotive. diesel and jet engines. Oxidation resrstnce is considered good under...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
... in STELLlTE 3 CasL Applications: Typical applications include vane plugs, fuel mtering pins, and spacer bushings for the aerospace industry; ball Manks and rack blanks for bearings; diesel exhaust components and fluid valve scauforvavcseatinsats;sawcuatrinseru;andotherwcarparrs. Producer: Deloro stellite Inc...