1-20 of 1313

Search Results for dies

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2014) 63 (9): SA-708.
Published: 01 September 2014
... MX01 is a steel grade developed to achieve useful properties to minimize the cost of forging dies. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-708. Producer or source...
Journal Articles
Alloy Digest (2002) 51 (3): TS-597.
Published: 01 March 2002
...). CARMO Filing Code: TS-597 Tool Steel March 2002 CARMO (Prehardened Cold-Work Steel for Car Body Dies) CARMO is the prehardened version of CALMAX (see Alloy Digest TS-177). It is particularly suitable for flame and induction hardening of large press work tooling where excessive distortion after heat...
Journal Articles
Alloy Digest (2003) 52 (6): CS-137.
Published: 01 June 2003
... Di-Form 140T is an ultrahigh-strength steel that offers a combination of high strength and high ductility, making it an excellent choice for parts consolidation programs. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: CS-137. Producer...
Journal Articles
Alloy Digest (2006) 55 (9): SA-556.
Published: 01 September 2006
... Mittal Di-Form T500 is a dual-phase steel intended primarily for exposed outer automotive body panels (door, hoods, and fenders). Dual-phase steels are one of the important advanced high-strength steel products developed for the automotive industry. Their microstructure typically consists...
Journal Articles
Alloy Digest (2007) 56 (1): SA-558.
Published: 01 January 2007
... MITTAL DI-FORM T590 and T600 are low-carbon dual-phase steels containing manganese and silicon. Dual-phase (DP) steels are important advanced high-strength steel (AHSS) products developed for the automotive industry. Their microstructure typically consists of a soft ferrite phase with dispersed...
Journal Articles
Alloy Digest (2007) 56 (2): SA-561.
Published: 01 February 2007
... MITTAL DI-FORM T700 and HF80Y100T are low-carbon steels with a manganese and silicon composition. Dual-phase (DP) steels are one of the important advanced high-strength steel (AHSS) products developed for the automotive industry. Their microstructure typically consists of a soft ferrite phase...
Journal Articles
Alloy Digest (2007) 56 (3): SA-563.
Published: 01 March 2007
... MITTAL DI-FORM T780 and T980 alloys are low-carbon steels with a manganese and silicon composition. Dual-phase (DP) steels are one of the important advanced high-strength steel (AHSS) products developed for the automotive industry. Their microstructure typically consists of a soft ferrite phase...
Journal Articles
Alloy Digest (2007) 56 (4): SA-566.
Published: 01 April 2007
... MITTAL DI-FORM 140T and HB T965 are low carbon steels with dual phase manganese and silicon composition. Dual-phase (DP) steel microstructures typically consist of a soft ferrite phase with dispersed islands of a hard martensite phase. The martensite phase is substantially stronger than...
Journal Articles
Alloy Digest (2014) 63 (12): SA-714.
Published: 01 December 2014
... DI-MC 355 is a weldable fine-grained thermomechanically rolled steel for structural design. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing...
Journal Articles
Alloy Digest (2015) 64 (1): SA-717.
Published: 01 January 2015
... DI-MC 460 is a weldable fine-grained thermomechanically rolled steel for structural design. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1999) 48 (1): Fe-88.
Published: 01 January 1999
... Armco DI-MAX nonoriented electrical steels have practically identical magnetic properties in any direction of magnetism in the plane of the material. They have superior permeability at high inductions, low average core loss, good gage uniformity, excellent flatness, and a high stacking factor...
Journal Articles
Alloy Digest (1967) 16 (6): TS-194.
Published: 01 June 1967
... LUMDIE is a tungsten-chromium hot work steel recommended for die casting dies, forging and extrusion dies. It is an air hardening steel having high temperature properties and heat resistance. It is particularly suited for long run die casting dies, brass forging dies, and for various extrusion...
Journal Articles
Alloy Digest (1964) 13 (8): TS-150.
Published: 01 August 1964
... Seneca Hot Die is a tungsten-chromium-vanadium type hot work steel having good red hardness and abrasion resistance. It is recommended for forging dies, copper extrusion dies, die casting dies, and other hot work tools and dies. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2019) 68 (12): TS-783.
Published: 01 December 2019
... YSS YXR7 is a high-speed tool steel with good toughness and wear resistance. It is used for blanking dies, forging dies, heading dies, and thread forming dies. This datasheet provides information on composition, physical properties, hardness, and bend strength. It also includes information on heat...
Journal Articles
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... AISI Type H12 is a general-purpose, low-carbon, chromium-molybdenum-tungsten hot-work steel for tools and dies that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat checking and may...
Journal Articles
Alloy Digest (1985) 34 (5): TS-440.
Published: 01 May 1985
... for Hotform Ultra include die-casting dies, core pins and inserts, piercing dies and hot-extrusion dies. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: TS-440...
Journal Articles
Alloy Digest (1985) 34 (6): TS-442.
Published: 01 June 1985
... AISI Type H10 is a hot-work tool steel of the chromium type, although it contains a substantial amount of molybdenum. It is a high-hardenability steel and possesses a combination of high tensile strength and hardness with excellent toughness. Typical hot work applications include forging dies...
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
...-work applications where machinability is of primary importance. Its many uses include forging and heading dies, aluminum extrusion dies, mandrels and mold dies for plastics. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information...
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation...