Alloy Digest (2000) 49 (10): TS-581.
Published: 01 October 2000
... Boehler W302 VMR is a hot tool steel that is manufactured and certified to meet an average impact toughness of 20 J (15 ft·lbf) minimum in Charpy V-notch testing. This die steel achieves that toughness by vacuum melting and remelting. Applications include dies, die holders, liners, and stems...
Journal Articles
Alloy Digest (2010) 59 (11): TS-694.
Published: 01 November 2010
... Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also...
Journal Articles
Alloy Digest (1972) 21 (1): Co-64.
Published: 01 January 1972
... Tool Ste&: AK1 Types Hl 1, H12, H20, H21 and H23 hot-work tool steels are recommended as holders for the BUDERUS 58-28 inserts. Accurate machining of die holder and die is required for BUDERUS 58-28 inserts to be effectively shrunk into the holder. The inserts must be in complete contact with the die...
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
... THYSSEN 4140 HOLDER material is supplied preheat treated to Rc24/32 (248-302 BHN). It is a free machining alloy tool steel designed especially for plastic mold base material and for holder blocks for die casting dies. It can also be used in non-critical molds where a #2 finish is acceptable...
Journal Articles
Alloy Digest (2008) 57 (6): TS-666.
Published: 01 June 2008
.... Applications: Extrusions tools, including containers, mantels, liner holders, die holders, bolsters, mandrel holders, and large mandrels. Fig. 4 Tempering graph Producer: Schmidt & Clemens, Inc. Houston, TX 77046 (713) 629-7770 (713) 629-7373 (fax) In Germany: Schmidt + Clemens GmbH + Co. KG Lindlar Germany...
Journal Articles
Alloy Digest (2012) 61 (9): TS-707.
Published: 01 September 2012
... primarily as a holder material for plastic molds and for die casting dies. It is not intended for tools that require a high surface finish. Contact the producer for additional information. Weldability: Preheat to 427 482 ºC (800 900 ºF). Maintain temperature above 427 ºC (800 ºF) during welding. After...
Journal Articles
Alloy Digest (1994) 43 (2): TS-523.
Published: 01 February 1994
... to or better than P20 as is its photo- etching capability. Its chemistry enables the hardness to be maintained into the center of even large blocks. It has a higher temperature resistance than P20, enabling it to be used as holder material in die castings. Impact strength is exceptionaUy high being in excess...
Journal Articles
Alloy Digest (2017) 66 (8): SA-794.
Published: 01 August 2017
... MTD 2 is mold base quality, Mn-Cr-Mo plate steel. It is commonly used in holder blocks, clamping plates, and support plates. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides...
Journal Articles
Alloy Digest (2009) 58 (7): TS-681.
Published: 01 July 2009
...: Extrusion tools, particularly for light metals, including liners, extrusion stems, mandrels, pressure pads, liner holders, container mantles, die holders and extrusion dies; pressure die- casting moulds for light metal; forging tools, including dies and dies inserts. Producer: Schmidt & Clemens, Inc...
Journal Articles
Alloy Digest (1974) 23 (2): SA-301.
Published: 01 February 1974
... condition as high as 300 BrineU. It can be welded by any of the conventional welding methods. Forms Available: Billets, bars and forgings. Applications: Typical applications are: backers for forging dies, brake dies, die holders, frames for plastic molds, holders for forging dies and molds requiring...
Journal Articles
Alloy Digest (2018) 67 (2): TS-747.
Published: 01 February 2018
... in extrusion dies with hardness HRC 45 49 in aluminum extraction for the die, container type, outer sleeve, inner sleeve, stem, die holder, mandrel, dummy block, and bolster. Producers Hitachi Metals America, Ltd. Purchase, NY 10577, USA Tel: (914) 694-9200 Fax: (914) 694-9279 www.hitachimetals.com In Japan...
Journal Articles
Alloy Digest (2017) 66 (11): TS-743.
Published: 01 November 2017
... sleeve, inner sleeve, stem die holder, mandrel, dummy block, and bolster. Producers: Hitachi Metals America, Ltd. Purchase, NY 10577, USA Tel: (914) 694-9200 Fax: (914) 694-9279 www.hitachimetals.com In Japan: High Grade Metals Company Tokyo, Japan 105-8614 Tel: 81-3-5765-4410 Fax: 81-3-5765-8317...
Journal Articles
Alloy Digest (2013) 62 (6): TS-717.
Published: 01 June 2013
... a very hot strength and temper resistance while retaining good thermal conductivity. Applications: Extrusion tools for heavy metals, including liners, extrusion stems, mandrels, pressure pads, extrusion dies, and die holders; pressure die casting dies for brass; forming dies; forging dies and die inserts...
Journal Articles
Alloy Digest (2012) 61 (2): TS-700.
Published: 01 February 2012
..., compression molds, blow molds, mold bases, die holders ...
Journal Articles
Alloy Digest (1976) 25 (6): TS-302.
Published: 01 June 1976
..., strip and other flat-rolled metallic and non- metallic materials; many machine parts requiring a steel with high mechanical properties; back-up and support tooling; die holders; and short run stamping and bending dies. Manufacturer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016. Weldability...
Journal Articles
Alloy Digest (1966) 15 (9): TS-182.
Published: 01 September 1966
... roughness. Forms Available: Billets, bars and forgings. Applications: Die casting dies and cores, dummy blocks, extrusion liners, heading dies, drop forging inserts, hot punches, backer blocks, die holders, brass extrusion dies, gripper dies in upsetters for forging steel, press forging dies and inserts...
Journal Articles
Alloy Digest (2011) 60 (10): TS-699.
Published: 01 October 2011
..., cores, and inserts for the high pressure die casting of aluminum, magnesium, and zinc alloys. The material is also used for hot forging, shearing, pressing, and extrusion tooling including dies, die holders, liners, and stems. The excellent polishability and toughness properties of W302 Superior also...
Journal Articles
Alloy Digest (1983) 32 (12): TS-419.
Published: 01 December 1983
... and forgings. Appkafions: Jessop Dica B Vanadium is used for aluminum die casting (cores, diecasting dies, die-holder blocks and plunger slides), hot-forging dies, hot-press dies, hot- work punches and molding dies for plastics. Manufacturer: Jessop Steel Company Washington, Pennsylvania 15301. ...
Journal Articles
Alloy Digest (1995) 44 (7): SS-600.
Published: 01 July 1995
... © ASM International® 1996 Weidabiliity: Weld overlays of worn areas and repair welds up to 1 deep can be made on Ultrachem in any of the below listed aged conditions using shielded metal arc welding with W 17-4 PH electrodes. In contrast to other die holder block steels no preheating is required...
Journal Articles
Alloy Digest (1968) 17 (3): TS-203.
Published: 01 March 1968
... cations: Aluminum extrusion dies, die holders, dummy blocks, rams, bulldozer dies, forging dies exposed LO shock, heavy duty compression tools, die casting dies, hot piercing and forming dies. Manufacturer: The Carpenter Steel Company Reading, Pennsylvania ...