Publisher: Journals Gateway
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (12): TS-467.
Published: 01 December 1986
... NU-DIE XL is a manufactured to meet the demanding specifications for long-run die-casting dies for aluminum. Sound centers are produced in both large and smaller sizes. Its many applications include die-casting dies, die inserts, cores and extrusion dies for aluminum and magnesium. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (6): TS-194.
Published: 01 June 1967
... LUMDIE is a tungsten-chromium hot work steel recommended for die casting dies, forging and extrusion dies. It is an air hardening steel having high temperature properties and heat resistance. It is particularly suited for long run die casting dies, brass forging dies, and for various extrusion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (10): TS-15.
Published: 01 October 1986
... CASCADE is a precipitation-hardening steel which is very popular as a mold steel for injection molding of thermoplastics. It is also an excellent choice for many zinc die-casting dies because of its resistance to heat checking and wash. A further wide usage for Cascade is as a holding-block...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (5): TS-440.
Published: 01 May 1985
... for Hotform Ultra include die-casting dies, core pins and inserts, piercing dies and hot-extrusion dies. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: TS-440...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (8): TS-150.
Published: 01 August 1964
... Seneca Hot Die is a tungsten-chromium-vanadium type hot work steel having good red hardness and abrasion resistance. It is recommended for forging dies, copper extrusion dies, die casting dies, and other hot work tools and dies. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (1): TS-420.
Published: 01 January 1984
... hot-work applications include extrusion dies for copper and brass, long-running die-casting dies, piercer points and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (2): TS-227.
Published: 01 February 1970
... THERMOLD-H23 is a chromium-tungsten hot work tool and die steel characterized by high strength at elevated temperatures and good resistance to heat checking. It is recommend for extrusion dies and die casting dies. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (4): TS-191.
Published: 01 April 1967
... PRESSURDIE-1 is an air-hardening hot work tool and die steel having high heat resistance and good high temperature strength properties. It is recommended for die casting dies, extrusion and forging dies. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (7): TS-106.
Published: 01 July 1961
... PAR-EXC is a medium-carbon low-alloy tool and die steel recommended for hubbing dies, punches, small die casting dies, hot work tools and other parts requiring moderate hardness and high toughness. This grade can be carburized to produce a wear resisting surface with a high strength, high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (1): TS-393.
Published: 01 January 1982
.... It is produced to high-quality tool-steel standards to permit a high luster to be achieved on the surface of the polished die cavity. P20 is used for molds for plastics and for die-casting dies for zinc and other low-temperature casting alloys. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (9): TS-197.
Published: 01 September 1967
... Thermold 75 is a chromium-molybdenum-cobalt hot work steel that has outstanding resistance to softening when tempering, and also very good thermal fatigue characteristics. It is recommended for aluminum die casting dies, forging dies and extrusion dies. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (3): TS-203.
Published: 01 March 1968
... CARPENTER No. 345 is a chromium-molybdenum-tungsten hot work steel for applications which require extreme toughness. It is recommended for aluminum extrusion work, forging dies, die casting dies, forming dies, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (2): TS-747.
Published: 01 February 2018
... YSS DAC 55 is a standard grade for die casting dies. Tool steel for large or squeeze die casting molds with excellent heat crack resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (12): TS-564.
Published: 01 December 1998
... CPM Nu-Die EZ is a die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition and is easily machined using conventional chip-making methods. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (4): TS-162.
Published: 01 April 1965
... A. M. 3 Die Steel is a medium-carbon, 5% chromium tool and die steel having high resistance to heat checking and erosion of die-casting dies and other hot work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (1): TS-696.
Published: 01 January 2011
... DH31-EX was developed to extend the life of aluminum die cast dies, and other hot forging or pressing dies. This datasheet provides information on physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-696. Producer or source: International Mold Steel Inc...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (3): SA-494.
Published: 01 March 1998
... DH2F is a prehardened modification of H13 tool steel for die casting dies and components for aluminum and zinc dies. The alloy has excellent machinability with abrasion and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... BOFORS BP20-2 is a vacuum-degassed (BOVAC) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat...