Alloy Digest (1987) 36 (1): TS-469.
Published: 01 January 1987
... CARPENTER 883 PLUS is a premium quality die-casting die steel. It is electroslag remelted and this together with processing adaptations give it metallurgical consistency and improved isotropic properties. This datasheet provides information on composition, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1954) 3 (8): Mg-11.
Published: 01 August 1954
... DOMAL AZ91Z is a 9% Al, 1% Zn, magnesium die casting alloy. It combines good mechanical properties, casting characteristics and resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (2020) 69 (10): Al-469.
Published: 01 October 2020
... Alcoa EZCast-NHT A152 and A153 are proprietary, non-heat-treatable, high-pressure die casting (HPDC) aluminum alloys in which magnesium is the principal alloying element. These alloys develop the required strength and toughness in the as-cast condition, thus eliminating or minimizing numerous...
Journal Articles
Alloy Digest (1972) 21 (5): Zn-14.
Published: 01 May 1972
... ILZRO 16 is a zinc-base die-casting alloy which was developed to have superior creep resistance at both ambient and elevated temperatures for processing in cold-chamber die-casting machines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1975) 24 (10): Al-218.
Published: 01 October 1975
... ALUMINUM 384.0 is a general-purpose alloy for making intricate die castings. It has good castability and foundry characteristics, good machinability and good strength. It is an excellent alloy for large thin-walled castings, and is suitable for castings requiring pressure tightness. This datasheet...
Journal Articles
Alloy Digest (1957) 6 (4): Al-50.
Published: 01 April 1957
... ALUMINUM 380 and A380 are copper-silicon types of aluminum die casting alloys having excellent castability and improved machinability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1957) 6 (8): Mg-33.
Published: 01 August 1957
... ECLIPSALOY 130 is a magnesium die casting alloy having improved ductility, high corrosion, and impact resistance. The alloy was developed primarily to obtain an alloy of magnesium for die casting with less hot cracking tendency than those in use at the time of its development. This datasheet...
Journal Articles
Alloy Digest (1957) 6 (8): Al-54.
Published: 01 August 1957
... APEX 418 is an aluminum die casting alloy having excellent combination of high strength and corrosion resistance, also high ductility and finishing qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1957) 6 (9): Al-56.
Published: 01 September 1957
... ALSILOY No. 1 is a 12% silicon-aluminum die casting alloy having excellent castability, good corrosion resistance and fair machinability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1958) 7 (1): Mg-36.
Published: 01 January 1958
... MAGNESIUM AZ91B is a standard magnesium die casting alloy patterned for the needs of the commercial casting industry. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... APEX 36 is a high silicon, aluminum die casting alloy having high fluidity, excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1958) 7 (10): Al-71.
Published: 01 October 1958
... APEX Z39 is an aluminum-copper-silicon-zinc die casting alloy having excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes...
Journal Articles
Alloy Digest (1958) 7 (11): Al-72.
Published: 01 November 1958
... ALUMINUM 13 is a die casting alloy having excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature...
Journal Articles
Alloy Digest (1959) 8 (1): Al-75.
Published: 01 January 1959
... APEX 39 is an aluminum die casting alloy ingot containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1960) 9 (12): Al-98.
Published: 01 December 1960
... Birmal P.83 is an aluminum-copper-silicon die casting alloy, having excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1961) 10 (2): Al-100.
Published: 01 February 1961
... APEX 39-11 is an aluminum die casting alloy containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1961) 10 (5): Al-103.
Published: 01 May 1961
... Aluminum Alloys 360 and A360 are die casting alloys having good strength, good corrosion resistance, and excellent castability. Alloy A360 is a purer form of Alloy 360, having lower impurity maximums. This datasheet provides information on composition, physical properties, elasticity, tensile...
Journal Articles
Alloy Digest (2009) 58 (11): TS-684.
Published: 01 November 2009
... www.asminternational.org Filing Code: Tool Steel November 2009 TS-684 Kapstar is through-hardened steel of uniform hardness for molds and dies. KAPSTAR is a registered trademark of Nippon Koshuha Steel Company, Ltd. KAPSTAR® (Die-Casting Tool Steel) KAPSTAR® Chemical Composition, wt (Typical) Carbon 0.12 Chromium 0.50...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1956) 5 (10): Mg-28.
Published: 01 October 1956
... APEX 910 is a magnesium die casting alloy containing about 9% aluminum. It combines good mechanical properties, good casting characteristics, and good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...