Alloy Digest (1993) 42 (10): TS-520.
Published: 01 October 1993
... THYRODUR 2379 (AISI D2) is an air hardening, high carbon chromium die steel, well suited for long run tool and die applications. It is capable of great hardness and high resistance to abrasive wear. It is non-deforming; consistent in response to all machining, heat treating and production...
Journal Articles
Alloy Digest (1964) 13 (6): TS-147.
Published: 01 June 1964
... Falcon-6 is a shock resistant tool and die steel having extreme toughness combined with wear resistance and fatigue resistance. It is recommended for cold battering tools and hot die applications. This datasheet provides information on composition, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1967) 16 (10): SA-217.
Published: 01 October 1967
... ATLAS BRAKE DIE is an electric furnace alloy steel specifically designed to provide the optimum balance of strength, wear resistance and toughness desired in brake-die applications. It is normally furnished in the heat treated and stress-relieved condition. This datasheet provides information...
Journal Articles
Alloy Digest (1985) 34 (11): TS-449.
Published: 01 November 1985
... CARPENTER H-9 DOUBLE HEADER DIE STEEL was developed specifically to solve chipping, splitting, spalling and cracking in cold header die applications. All billets are acid disc inspected to ensure center soundness and they are tested for hardenability. This datasheet provides information...
Journal Articles
Alloy Digest (1997) 46 (5): Fe-56.
Published: 01 May 1997
..., hot-work die applications and high-pressure hydrogen environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well...
Journal Articles
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
... SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well...
Journal Articles
Alloy Digest (1982) 31 (2): TS-394.
Published: 01 February 1982
... HOTFORM No. 2 is a 5% chromium hot-work tool steel designed to provide an excellent combination of toughness (shock resistance), red hardness and resistance to abrasion. It is recommended for hot-die applications and for structural parts requiring high strength at elevated temperatures...
Journal Articles
Alloy Digest (1995) 44 (6): TS-539.
Published: 01 June 1995
... THYRAPID PM4 ESH is manufactured by the rapid solidification of powder and augmented by Electro Slag Heating. Good wear resistance and toughness lead to cold work punch and die applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and bend...
Journal Articles
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
... Lukens MTD steels are prehardened alloy plate steels developed for mold, tool, and die applications. This datasheet provides information on composition and hardness. It also includes information on heat treating, machining, and joining. Filing Code: SA-484. Producer or source: Lukens Steel Company...
Journal Articles
Alloy Digest (1987) 36 (5): TS-475.
Published: 01 May 1987
... AL TECH ARAPAHO is an air-hardening or oil-hardening tool steel depending on the size, tool geometry and other desired propties. It has exceptional toughness coupled with resistance to softening at moderately high temperatures. It is used for general blanking and forming-die applications; it also...
Journal Articles
Alloy Digest (1992) 41 (7): SA-463.
Published: 01 July 1992
... LADISH D-11 is a low alloy steel of medium carbon content and a balanced alloy composition. The alloy was designed for structural components and hot work tool and die applications as it possesses better higher temperature strength than D-6-A and H-13. This datasheet provides information...
Journal Articles
Alloy Digest (1961) 10 (6): TS-105.
Published: 01 June 1961
... Potomac A is a medium carbon, alloy steel that can maintain strength at elevated temperatures up to 1000 F. It is recommended for hot die applications and for structure components where strength at elevated temperatures is important. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (3): TS-412.
Published: 01 March 1983
... the many uses for this steel are hot-die applications, structural parts for jet engines and missiles, extrusion mandrels and forging dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1984) 33 (7): TS-424.
Published: 01 July 1984
... JESSOP TRUGLIDE is a free-machining, oil-hardening too steel designed primarily for cold-work die applications. Free graphite in this steel gives it excellent machinability and outstanding resistance to galling and seizing in operation. Among its many uses are dies, gages, punches, arbors...
Journal Articles
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
... for a variety of mold, tool, and die applications. This datasheet provides information on composition. It also includes information on forming, machining, and joining. Filing Code: SA-793. Producer or source: ArcelorMittal USA, Plate. Producer or Source: ArcelorMittal USA, Plate Copyright © ASM...
Journal Articles
Alloy Digest (2017) 66 (8): SA-794.
Published: 01 August 2017
... MTD 2 is mold base quality, Mn-Cr-Mo plate steel. It is commonly used in holder blocks, clamping plates, and support plates. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides...
Journal Articles
Alloy Digest (2017) 66 (9): SA-798.
Published: 01 September 2017
... MTD 3 is a Mn-Cr-Mo-V plate steel used in cavity molds. ArcelorMittal USA MTD steels comprise a family of prehardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides information on composition. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1967) 16 (2): Mo-8.
Published: 01 February 1967
... fatigue. It has excellent resistance to erosion in hoc die applications. Case hardening by carbonicriding or oiuidiog has proved feasible in producing a surface hardness of at least 1500 DPH. This surface hardening has proved advantageous in some applications where the relatively low room-temperature...
Journal Articles
Alloy Digest (1971) 20 (6): TS-235.
Published: 01 June 1971
... AISI Type Ol is an oil-hardening, non-deforming, general-purpose tool and die steel. It has a good combination of hardness, toughness and resistance to abrasion and wear. It is recommended for cold forming and shearing applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1999) 48 (11): TS-569.
Published: 01 November 1999
... is suitable for hydraulic and mechanical presses. Die preheating is mandatory. The alloy is used for die inserts or other applications where higher wear and tempering resistance that H11 or H13 die steels have is important. This datasheet provides information on composition, hardness, and tensile properties...