1-20 of 26 Search Results for

dental instruments

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (10): SS-452.
Published: 01 October 1984
... austenitized and quenched to a hardness of Rockwell C56. Its applications include dental and surgical instruments, cutlery and valve parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1981) 30 (10): SS-394.
Published: 01 October 1981
... CRUCIBLE 420 is a hardenable chromium steel designed particularly for cutlery applications. It is the general-purpose cutlery grade of stainless steel. It is magnetic at all times. Among its many applications are bushings, cutlery, valve trim and dental and surgical instruments. This datasheet...
Journal Articles
Alloy Digest (1982) 31 (10): Ni-279.
Published: 01 October 1982
..., corrosion and oxidation. The applications for Berylco Alloy 42C include cast-to-shape jewelry, surgical instruments, valves, pumps and dental alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (1980) 29 (4): Bi-16.
Published: 01 April 1980
... temperature and controlled-shrinkage characteristics make it highly useful for such applications as low-temperature solder, proof casting of cavities and dental models. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (2001) 50 (7): SS-826.
Published: 01 July 2001
... cavities, plastic extru- sion dies, cutlery, surgical and dental instruments, gages, valves, shafts, cams, and ball bearings. Producer: Timken Latrobe Steel A Timken Company Subsidiary Latrobe, PA (724) 537-7711 (724) 532-6316 (fax) ISSN: 002-614X SS-826B Fig. 1 Tempering temperature with resulting...
Journal Articles
Alloy Digest (2000) 49 (5): SS-783.
Published: 01 May 2000
... resistance are available only in the hardened or hardened and stress relieved conditions, so the alloy is not used in the annealed or annealed and tempered conditions. Applications: Dental and surgical instruments and cutlery are frequent applica- tions for type 440A. Product Forms Available: Armco produces...
Journal Articles
Alloy Digest (2005) 54 (11): SS-946.
Published: 01 November 2005
... condition. Available Product Forms: This alloy is produced as precision wire in all of the forms of sup- ply shown in Table 1. Applications: Sandvik Bioline 4C27A is suitable for the manufacture of preci- sion components such as watch parts, measuring points, dental tools, precision instruments, and drilled...
Journal Articles
Alloy Digest (1968) 17 (10): SS-215.
Published: 01 October 1968
.... wire and wire rods, cold drawn bars, annealed or tempered strip. Applications: Pivot pins. dental and surgical instruments, cutlery. valve parts, ball bearings. Manufacturer: Practically all stainless steel mills produce this type alloy either under their own proprietary name or under AISI Type 440.4...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1323.
Published: 01 July 2020
... polish- ability; magnetic in both the annealed and the quenched and tempered condition. Product Forms Bars, profiles, wire Applications Bone cutters, burrs; cutting tools, e. g. doctor blades, scissors; dental instruments, e.g. burrs, curettes, and cutters; medical screwdrivers; surgical instruments...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
... extraction forceps, dental tweezers, filling instruments, gouges, knives, laboratory and orthodontic pliers, raspatories, rongeurs, root elevators, scal- ers, scalpels, scissors. Information on applications sourced from Zapp AG, ISO 7153-1:2016, and ASTM F899:2019. Supplier Zapp AG Zapp-Platz 1 40880...
Journal Articles
Alloy Digest (2015) 64 (6): SS-1212.
Published: 01 June 2015
...: Applications requiring good corrosion resistance and high hardness are ideal for this alloy. Typical uses include cutlery, surgical and dental instruments, scissors, tapes, and straight edges. The alloy is not normally used at temperatures exceeding 427 °C (800 °F) due to rapid softening and loss of corrosion...
Journal Articles
Alloy Digest (2000) 49 (4): SS-781.
Published: 01 April 2000
... hard- ness are ideal for this alloy. Typical uses include cutlery, surgical and dental instruments, scissors, tapes, and straight edges. The al- loy is not normally used at temperatures exceeding 427 °C (800 °F) due to rapid softening and loss of corrosion resistance. Producer: Armco Inc. Specialty...
Journal Articles
Alloy Digest (2020) 69 (6): SS-1320.
Published: 01 June 2020
...- ditions. Product Forms Bars, wire, profiles Applications Bone cutters; burrs; cutting tools, for example: scissors, doc- tor blades; dental instruments, for example: cutters, burrs, and curettes; medical screwdrivers; surgical instruments. Supplier Zapp AG Zapp-Platz 1 40880 Ratingen, Germany Tel: +49...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1321.
Published: 01 July 2020
... bars; strip; wire rod; wire Applications CarTech 420 is used for ball bearings, ball check valves, cams, cutlery, gauges, gears, magnets, needle valves, piv- ots, scissors, shafts, surgical and dental instruments, tapes and straight edges, tempered rules, etc. It is also used at moderately elevated...
Journal Articles
Alloy Digest (1981) 30 (9): Bi-26.
Published: 01 September 1981
... water is circulated through the platen until the alloy has solidified. The delicate parts are now ready for machining or grinding. Dental, Home and Medical Aids: Because of its low melting temperature of 117OF, Indalloy 117 is frequently used for dental models, prosthetic development work, radiopaque...
Journal Articles
Alloy Digest (1978) 27 (2): Bi-3.
Published: 01 February 1978
... grinding optical lenses and components. Models and Molds: Belmont alloys 2451 and 2491 are used for dental models and as molds for prosthetic development work. Miscellaneous Aids: Belmont alloys 2451 and 2491 are used in the following miscellaneous applications: (1) Fixtures for assembly, checking, die...
Journal Articles
Alloy Digest (1973) 22 (4): Sn-3.
Published: 01 April 1973
... castings for dairy machinery, dental appliances, surgical instruments, soda fountain equipment. Alloy 2: Bearings, most widely used tin-base bearing alloy in the automotive field. AJloy 3: Bearings for high-load applications, hardest of standard Tin- Babbit alloys and has greatest load-carrying capacity...
Journal Articles
Alloy Digest (1955) 4 (12): SS-38.
Published: 01 December 1955
..., hot rolled bars and forgings, ground bars, wire and wire rods, cold drawn bars, annealed or tempered suip. Applications: Pivot pins, dental and surgical instruments, cutlery, valve parts, ball bearings, general applications where both strength and ductility are required. Manufacturer: Allegheny Ludlum...
Journal Articles
Alloy Digest (2004) 53 (9): SS-908.
Published: 01 September 2004
... a delivery. Contact the producer for tol- erances. Applications: The combination of properties, surface finish, and sterilizability make this grade of steel suitable for use in the fabrication of torque wrenches, bone drills, surgical tools and other microsurgi- cal medical and dental devices...
Journal Articles
Alloy Digest (1978) 27 (9): Bi-7.
Published: 01 September 1978
.... Models and Patterns: Belmont alloy 2562 is used for (1) Dental models and (2) Duplicate patterns for foundry match plates, cera- mics, plastics and pottery. Belmont alloy 2581 is used for tracer models for pantograph engraving and dupli- cating, and for proof casting of patterns. Molds: Belmont ahoy 2581...