Journal Articles
Alloy Digest (1963) 12 (4): TS-132.
Published: 01 April 1963
... HYCC is a high-carbon high-chromium tool steel having high wear and abrasion resistance combined with non-deforming characteristics. It is particularly adaptable for blanking dies and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It...
Journal Articles
Alloy Digest (1953) 2 (4): TS-6.
Published: 01 April 1953
... VAIRLOY is a manganese-chromium-molybdenum tool and die steel capable of being air-hardened at low temperatures with minimum distortion and deformation. It is strong, tough and wear resistant. This datasheet provides information on composition and hardness. It also includes information on forming...
Journal Articles
Alloy Digest (1960) 9 (6): TS-94.
Published: 01 June 1960
... COLONIAL No. 6 is an oil hardening, non-deforming, general purpose tool and die steel. It has good combination of abrasion resistance, hardness and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (1961) 10 (7): TS-107.
Published: 01 July 1961
... BADGER is an oil hardening, non-deforming tool and die steel having good hardenability characteristics. Tungsten and chromium additions increase its wear resistance over the straight manganese oil hardening type die steel. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1962) 11 (11): TS-126.
Published: 01 November 1962
... KISKI is a non-deforming, oil-hardening tool and die steel of high manganese content. It has good combination of toughness, high hardenability, wear and abrasion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It...
Journal Articles
Alloy Digest (1967) 16 (2): TS-189.
Published: 01 February 1967
... thermal shock. It hardens sarisfactorily in air with minimum distortion. It has high resistance to heat checking when repeatedly heated and cooled, also high resistance co scaling. It possesses sufficient compressive strength after heat treatment co resist deformation due to high operating pressures...
Journal Articles
Alloy Digest (1960) 9 (8): TS-96.
Published: 01 August 1960
... KETOS is an oil-hardening non-deforming tool steel having deep hardening qualities with a fine grain structure. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as deformation. It also includes information on forming...
Journal Articles
Alloy Digest (1954) 3 (12): TS-28.
Published: 01 December 1954
... VULCAN NON-SHRINKABLE is a standard manganese type of oil hardening tool steel for use where non-shrinking and non-deforming properties are important. This is an ASM Class II-A2 and SAE Type 02 Alloy. This datasheet provides information on composition and hardness as well as fracture toughness. It...
Journal Articles
Alloy Digest (2009) 58 (2): SS-1030.
Published: 01 February 2009
... International Alkrothal 3 braking resistors chemical composition elasticity electrical heating elements hardness high-temperature alloys physical properties rheostats tensile properties workability thermal properties ALKROTHAL® 3 (Ferritic Resistance Alloy) Alkrothal 3 is a ferritic FeCrAl...
Journal Articles
Alloy Digest (2009) 58 (3): SS-1032.
Published: 01 March 2009
... Alkrothal 14 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low temperature performance as well as forming...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1136.
Published: 01 February 2013
... Alkrothal 720 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as...
Journal Articles
Alloy Digest (2009) 58 (9): SS-1044.
Published: 01 September 2009
... Nikrothal 20 is an austenitic nickel-chromium alloy (NiCr alloy) for use at temperatures up to 1050 C (1920 F). The alloy is characterized by high resistivity and moderate oxidation resistance. It has good ductility after use and excellent weldability. This datasheet provides information on...
Journal Articles
Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... Kanthal APM HP is an advanced high-purity powder metallurgical dispersion-strengthened resistance heating or high-temperature alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1996) 45 (2): SS-639.
Published: 01 February 1996
... heat or in preventing thermal deformations during heating and cooling cycles. In these instances. the higher aluminum Ohmaloy 40 alloy is used. Nominally. the room temperature specific resistivity of Ohmaloy 30 alloy is 107 micro-ohm-centimeters (505 ohm sq-miYft). The change in resistivity of Ohmaloy...
Journal Articles
Alloy Digest (1996) 45 (4): SS-641.
Published: 01 April 1996
... to assist in the dissipation of heat or in preventing thermal deformations during heating and cooling cycles. In these instances. the higher aluminum Ohmaloy 40 alloy is used. Ohmaloy 40 alloy has a nominal mom tempemmre specific resistivity of 116 p&m (550 Qsq mil/ft). The change in resistiv- ity of...
Journal Articles
Alloy Digest (1953) 2 (5): Co-1.
Published: 01 May 1953
... F to 2100 F. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as creep, deformation, and fatigue. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Co-1. Producer or source...
Journal Articles
Alloy Digest (1987) 36 (4): TS-473.
Published: 01 April 1987
... SILICO ALLOY is a silicon-manganese shock-resisting tool steel; it has high toughness at relatively high operating hardnesses. It is primarily an oil-hardening steel because of its molybdenum content (0.45%); however, it may be water hardened. It is a low-cost, high-quality steel that combines...
Journal Articles
Alloy Digest (1990) 39 (10): TS-502.
Published: 01 October 1990
... CIRCLE C (AISI T5) tool steel combines increased wear resistance from higher vanadium and carbon contents with higher red hardness due to 8 to 9% cobalt content. This datasheet provides information on composition and hardness as well as fracture toughness, and deformation. It also includes...
Journal Articles
Alloy Digest (2003) 52 (12): SS-897.
Published: 01 December 2003
... chemical composition corrosion-resistant alloys deformation properties DURAFOIL-CLAD elasticity heat treatability joinability physical properties tensile properties workability thermal properties Chemical Composition, wt%: Steel Aluminum alloy Chromium 21.0 23.0 Carbon 0.03 max Manganese...
Journal Articles
Alloy Digest (1995) 44 (4): SS-384.
Published: 01 April 1995
..., hardness, elasticity, and tensile properties as well as fracture toughness, and deformation. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-384. Producer or source: Carpenter. Originally published March 1981, revised April...