Alloy Digest (2004) 53 (3): Cu-711.
Published: 01 March 2004
... Wieland-M20 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn products such as lipstick cases. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-716.
Published: 01 June 2004
... Wieland-M37 has excellent cold-working properties and corrosion resistance. The alloy is used in the deep-drawn and stamped condition for electrical products. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... Wieland C21000, also known as gilding metal, is a 95Cu-5Zn alloy. This versatile, low-cost alloy is often the choice of engineers for deep drawn parts such as bullet jackets and coined products. The combination of moderate conductivity and improved strength make C21000 a valuable option...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2004) 53 (5): Cu-714.
Published: 01 May 2004
... Wieland-M33 has excellent cold-working properties and corrosion resistance. The alloy is used in deep-drawn decorative products and in electrical components. The alloy is often called yellow brass, 65%. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (1960) 9 (6): Cu-89.
Published: 01 June 1960
... REVERE No. 140 is a copper-zinc alloy containing 20% zinc. It is recommended for deep drawn and cold formed products. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1975) 24 (4): Zn-18.
Published: 01 April 1975
... by conventional processes including spinning and its applications include such items as deep-drawn cans and jewelry. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1958) 7 (3): Cu-60.
Published: 01 March 1958
... Cartridge Brass is a 70-30 copper-zinc alloy having high strength, maximum ductility and good corrosion resistance. It is recommended for deep drawing operations. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (2003) 52 (4): Cu-700.
Published: 01 April 2003
... Wieland-M28 has excellent cold-working properties. The alloy is used in deep drawn, spun, architectural, and instrument applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2023) 72 (9): SS-1362.
Published: 01 September 2023
... to 870 °C (1600 °F) and in continuous service up to 925 °C (1695 °F). Continuous use of Atlas 304 in the 425 860 °C (795 1580 °F) range is not recommended if subsequent aqueous corrosion resistance is important. Cold Forming Atlas 304 can be severely deep drawn without intermediate annealing, which has...
Journal Articles
Alloy Digest (2004) 53 (8): Fe-131.
Published: 01 August 2004
... to ease of fabrication in parts requiring bending, forming, and deep drawing. For nickel-irons having approximately 30 50% Ni, the tensile strengths for annealed alloys will typically be 450 585 MPa (65 85 ksi) with tensile elongations greater than 25%. For some product forms, the tensile strengths can...
Journal Articles
Alloy Digest (1976) 25 (4): Cu-311.
Published: 01 April 1976
... Copper Alloy No. 370 is a medium-leaded brass (formerly known as Free-Cutting Muntz metal) with good machinability. It is suitable for high-speed screw machine work and is used for a wide variety of products such as gears, nuts and washers. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2009) 58 (5): SS-1036.
Published: 01 May 2009
... of the bar in the most desirable range for machining. This alloy is PRODEC-treated for improved performance important when used in CNC machines making it equally effective with high-speed steel and carbide tooling. Product Forms Available: Cold drawn 316 1 in. round, hex, square Special Features: Diameter...
Journal Articles
Alloy Digest (2002) 51 (11): SS-867.
Published: 01 November 2002
... and deep drawn more easily than some steels due to an increased nickel content that decreases work hardening. It is non- magnetic and cannot be hardened by heat treatment. Product Forms Available: AK Steel produces Type 305 stainless steel in thicknesses from 0.25 3.18 mm (0.01 0.125 in.) and widths up...
Journal Articles
Alloy Digest (1975) 24 (1): Cu-290.
Published: 01 January 1975
... of the standard welding processes. Its machinability rating is 20%, of that of free-cutting brass. making it one of the copper alloys that are rather difficult to machine. Forms Available: Bar, rod. extrusions. sheet, strip. plate, tube and wire. Applications: Fishing reels. deep-drawn writing instruments...
Journal Articles
Alloy Digest (2006) 55 (2): Ni-631.
Published: 01 February 2006
... that provides deep-draw capability. It has good forming characteristics and can be deep drawn. It is not suitable for extended exposure to air at elevated temperatures. HPM 80/20A is available as strip product in thicknesses from 0.001 0.050 in., and width up to 12 in. The material conforms to ASTM B...
Journal Articles
Alloy Digest (1956) 5 (8): Cu-41.
Published: 01 August 1956
... properties with good corrosion resistance. The mechanical properties rriscorrosion resistance are nearly the same as Cartridge Forms Available: Rod, sheet, strip, wire, rolled and drawn flat products. Applications: For deep drawing, stamping, spinning, rolling-in fact for practically all fabricating...
Journal Articles
Alloy Digest (2004) 53 (10): Fe-132.
Published: 01 October 2004
... treatment. They exhibit excellent ductility, which contributes to ease of fabrication in parts requir- ing bending, forming, and deep drawing. For nickel-irons having approx- imately 30 50% Ni, the tensile strengths for annealed alloys will be typically 450 585 MPa (65 85 ksi) with tensile elongations >25...
Journal Articles
Alloy Digest (2004) 53 (11): Fe-133.
Published: 01 November 2004
... ductility, which contributes to ease of fabrication in parts requiring bending, forming, or deep draw- ing. For nickel-irons having approximately 30 50% Ni, the ten- sile strengths for annealed alloys will be typically 448 586 MPa (65 85 ksi) with tensile elongations greater than 25%. For some product forms...
Journal Articles
Alloy Digest (2004) 53 (12): Fe-134.
Published: 01 December 2004
... thermal expansion are austenitic solid solutions that exhibit moderate strength levels and are not hardenable by heat treat- ment. They exhibit excellent ductility, which contributes to ease of fabrication in parts requiring bending, forming, or deep draw- ing. For nickel-irons having approximately 30 50...