Alloy Digest (1980) 29 (5): Cu-395.
Published: 01 May 1980
...* Alloy 260 (Deep-Drawing Alloy; Cartridge Brass) ANACONDA AlIoy 260 nominally contains 70% copper and 30% zinc. This alloy is the most ductile of the brasses and also has fairly high strength; it is used in greater quantity than any other copper-zinc alloy. It takes its tradename (Cartridge Brass) from...
Journal Articles
Alloy Digest (1982) 31 (1): Cu-429.
Published: 01 January 1982
... tensile properties workability UNS C26000 Filing Code: cu429 MUELLER ALLOY 2600 Copper Alloy JANUARY 1982 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications. Inc. WI rights reserved. MN: 002-614X MUELLER Alloy 2600 (Deep-Drawing Brass) MUELLER Alloy 2600 has the optimum...
Journal Articles
Alloy Digest (1964) 13 (4): SS-154.
Published: 01 April 1964
... 1964 -DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbd by Engineering Alloys Digest, Inc. Upper Montclait. New Jersey Al9 Type 305 (Deep Drawing Stainless Steel) AISI Type 305 is an austenitic chromium nickel stainless steel with lower race of work hardening than Type 302 ot 304 and less change...
Journal Articles
Alloy Digest (1975) 24 (4): Zn-18.
Published: 01 April 1975
... NJZ ALLOY No. 1 is produced from high-grade, high-purity zinc with additions of lead, cadmium and iron. It gives excellent deep-drawing performance because of a combination of low hardness and strength, high ductility and very little tendency to work harden. It can be formed readily...
Journal Articles
Alloy Digest (1958) 7 (3): Cu-60.
Published: 01 March 1958
... Cartridge Brass is a 70-30 copper-zinc alloy having high strength, maximum ductility and good corrosion resistance. It is recommended for deep drawing operations. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1971) 20 (9): Cu-241.
Published: 01 September 1971
... ALLOY No. 260 CopparA w SEPTEMBER 1971 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS En&:h&%i k upper Bfoarclair. New Jency COPPER ALLOY No. 260 (Deep Drawing Brass) COPPER ALLOY No. 260 is a 70% copper-30% zinc alloy having high strength. excellent ductility, and good corrosion minance. Composition...
Journal Articles
Alloy Digest (2022) 71 (11): Cu-935.
Published: 01 November 2022
.... It has excellent deep drawing characteristics and resistance to pitting corrosion when exposed to severe weather and water environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1987) 36 (6): Zn-41.
Published: 01 June 1987
... Plus is ideal for a variety of tough applications. It is excellent for products that require deep drawing and it combines extra corrosion resistance with superior formability. This datasheet provides information on composition and physical properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1987) 36 (11): Al-284.
Published: 01 November 1987
... AA 3003 is a wrought non-heat-treatable aluminum alloy with excellent resistance to corrosion. It is used widely in deep-drawing and forming applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-356.
Published: 01 June 1978
... BRUSH Alloy 25 attains the highest strength and hardness of any copper-base alloy. In the age-hardened condition, its tensile strength can exceed 200,000 psi and its Rockwell C hardness can reach 45. Its many applications include springs, deep-drawing parts, current-carrying springs connectors...
Journal Articles
Alloy Digest (1985) 34 (5): CS-106.
Published: 01 May 1985
... AISI 1010 is a low-carbon steel having good formability and weldability. It is recommended for sheet stock for deep-drawing operations and in sheet and stock for structural shapes and carburized parts. Among its many applications are bushings, clutch discs, flanges, thrust washers, tinplate, nails...
Journal Articles
Alloy Digest (2002) 51 (1): SS-840.
Published: 01 January 2002
... Allegheny Ludlum Type 305 (S30500) stainless steel is used for applications requiring a low rate of work hardening during severe cold-forming operations such as deep drawing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2002) 51 (11): SS-867.
Published: 01 November 2002
... AK Steel Type 305 has the advantage of economical fabrication. Its chief characteristics are minimum work-hardening tendencies and maximum ductility. The alloy is especially suited to operations involving severe cold work such as deep drawing and spinning. It can be annealed to greater softness...
Journal Articles
Alloy Digest (2009) 58 (9): SS-1043.
Published: 01 September 2009
... Nirosta 4303 is a modification of Nirosta 4301 with higher nickel content. It is often used for precision deep-drawing applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2010) 59 (3): TS-687.
Published: 01 March 2010
... and forming, cold extrusion, deep drawing, and powder pressing. UDDEHOLM VANCRON 40 (Nitrided Powder Metal Tool Steel) UDDEHOLM VANCRON 40 Chemical Composition, wt (Typical Analysis) Carbon 1.1 Silicon 0.5 Manganese 0.4 Chromium 4.5 Molybdenum 3.2 Tungsten 3.7 Vanadium 8.5 Nitrogen 1.8 Iron bal Physical...
Journal Articles
Alloy Digest (2020) 69 (8): Cu-911.
Published: 01 August 2020
... for an electrical conductivity of 100% IACS minimum, as well as no susceptibility to hydrogen embrittlement. Due to the absence of oxides in the structure, Cu-OF is capable of withstanding extra deep drawing and severe forming, and is superior to Cu-ETP in this respect. This datasheet provides information...
Journal Articles
Alloy Digest (1973) 22 (12): Al-31.
Published: 01 December 1973
... ALUMINUM 3003 is a wrought non-heat-treatable aluminum alloy with excellent resistance to corrosion. It is used widely in deep-drawing and forming applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1957) 6 (4): Cu-49.
Published: 01 April 1957
... NICKEL SILVER, 65-18 is a deep drawing grade of nickel silver. It has high resistance to corrosion and tarnish. It is used primarily for drawn, spun and similar cold-worked parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1972) 21 (1): SS-266.
Published: 01 January 1972
... ALLEGHENY TYPE 211 is a copper-bearing, austenitic, chromium-nickel-manganese stainless steel with a low work-hardening rate. It is used for many deep-drawing applications, such as automotive trim, and broiler pans, mixing bowls, sinks, and door hardware. This datasheet provides information...
Journal Articles
Alloy Digest (1961) 10 (5): Cu-100.
Published: 01 May 1961
... REVERE No. 533 is an 18% nickel silver alloy having high ductility, malleability and resistance to corrosion. It is recommended for deep drawing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...