Skip Nav Destination
Close Modal
Search Results for
cutting tools
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 3569
Search Results for cutting tools
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1963) 12 (1): Co-35.
Published: 01 January 1963
... Digest. IN. Upper Mondtir. Near Jersey ALX ALLOY (Cutting Tool & Die Alloy) ALX is a composition of non-ferrous materials with a cobalt base containing chromium, tungsten and carbon. This alloy is commonly supplied in the cast-to-shape form, having an as-cast hardness of Rock- well C60-62 and requiring...
Abstract
View articletitled, ALX ALLOY: <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> and Die Alloy
View
PDF
for article titled, ALX ALLOY: <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> and Die Alloy
ALX is a composition of nonferrous materials with a cobalt base containing chromium, tungsten and carbon. This alloy is commonly supplied in the cast-to-shape form, having an as-cast hardness of Rockwell C60-62 and requiring no further heat treatment. ALX is also supplied as cast tool bit material and is useful where conventional high-speed steels or carbides do not function effectively. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, heat treating, and machining. Filing Code: Co-35. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1958) 7 (5): Co-13.
Published: 01 May 1958
... HAYNES STELLITE No. 19 is a cobalt-base cutting tool alloy having high resistance to severe shock and excellent red-hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Abstract
View articletitled, HAYNES STELLITE ALLOY No. 19: Non Ferrous Cast <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> Alloy
View
PDF
for article titled, HAYNES STELLITE ALLOY No. 19: Non Ferrous Cast <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> Alloy
HAYNES STELLITE No. 19 is a cobalt-base cutting tool alloy having high resistance to severe shock and excellent red-hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on corrosion resistance as well as machining. Filing Code: Co-13. Producer or source: Haynes Stellite Company.
Journal Articles
Alloy Digest (1960) 9 (7): Co-22.
Published: 01 July 1960
... ON WORLD WIDE METALS AND ALLOYS Pmblisbd b7 HAYNES STELLITE 98M2 Alloy (Cast Noderrous Cutting Tool Alloy) HAYNES SELLITE 98M2 Alloy is a cobalt-base alloy having higher compressive strength and higher hardness than all the other cobalt-base alloys at room temperature and in the red heat range. Composition...
Abstract
View articletitled, HAYNES STELLITE ALLOY No. 98M2: Cast Nonferrous <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> Alloy
View
PDF
for article titled, HAYNES STELLITE ALLOY No. 98M2: Cast Nonferrous <span class="search-highlight">Cutting</span> <span class="search-highlight">Tool</span> Alloy
HAYNES STELLITE 98M2 Alloy is a cobalt-base alloy having higher compressive strength and higher hardness than all the other cobalt-base alloys at room temperature and in the red heat range. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: Co-22. Producer or source: Haynes Stellite Company.
Journal Articles
Alloy Digest (1979) 28 (10): TS-355.
Published: 01 October 1979
... combination of cutting ability and toughness. Its many uses include drills, reamers, milling cutters, lathe tools, punches, dies and springs for use at elevated temperature. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well...
Abstract
View articletitled, RED <span class="search-highlight">CUT</span> SUPERIOR: High-Speed <span class="search-highlight">Tool</span> Steel, Type T1
View
PDF
for article titled, RED <span class="search-highlight">CUT</span> SUPERIOR: High-Speed <span class="search-highlight">Tool</span> Steel, Type T1
RED CUT SUPERIOR is a high-speed steel of the 18% tungsten-4% chromium-1% vanadium type. Many consider it to be the best type of high-speed steel for general purposes. It is comparatively easy to fabricate and simple to heat treat. It has a minimum tendency to decarburize and an excellent combination of cutting ability and toughness. Its many uses include drills, reamers, milling cutters, lathe tools, punches, dies and springs for use at elevated temperature. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-355. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1980) 29 (8): TS-367.
Published: 01 August 1980
... RED CUT COBALT steel is made by adding 5% cobalt to the conventional 18% tungsten -4% chromium-1% vanadium high-speed steel. Cobalt increases hot or red hardness and thus enables the tool to maintain a higher hardness at elevated temperatures. This steel is best adapted for hogging cuts or where...
Abstract
View articletitled, RED <span class="search-highlight">CUT</span> COBALT: High-Speed <span class="search-highlight">Tool</span> Steel, Type T4
View
PDF
for article titled, RED <span class="search-highlight">CUT</span> COBALT: High-Speed <span class="search-highlight">Tool</span> Steel, Type T4
RED CUT COBALT steel is made by adding 5% cobalt to the conventional 18% tungsten -4% chromium-1% vanadium high-speed steel. Cobalt increases hot or red hardness and thus enables the tool to maintain a higher hardness at elevated temperatures. This steel is best adapted for hogging cuts or where the temperature of the cutting point of the tool in increased greatly. It is well adapted for tools to be used for reaming cast-iron engine cylinders, turning alloy steel or cast iron and cutting nonferrous alloys at high speeds. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-367. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1983) 32 (1): TS-410.
Published: 01 January 1983
... RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended...
Abstract
View articletitled, RED <span class="search-highlight">CUT</span> SUPERIOR J: Hot Work <span class="search-highlight">Tool</span> Steel, Type H26
View
PDF
for article titled, RED <span class="search-highlight">CUT</span> SUPERIOR J: Hot Work <span class="search-highlight">Tool</span> Steel, Type H26
RED CUT SUPERIOR J is a tungsten-type of hot-work tool and die steel; in fact, it is the 18 tungsten-4 chromium-1 vanadium high-speed composition with carbon lowered to provide more toughness. It is characterized by high red hardness and good resistance to abrasion. It is recommended for applichations in which hardness must be maintained at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-410. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1998) 47 (2): TS-560.
Published: 01 February 1998
... Thyrapid 3343 is a standard high-speed steel grade with balanced alloy composition, high toughness, good cutting power, and consequently versatile applications. Thyssen Thyrapid 3343 is suitable for all metal-cutting tools for roughing or finishing, such as twist drills, milling cutters of all...
Abstract
View articletitled, THYRAPID 3343: High-Speed Steel
View
PDF
for article titled, THYRAPID 3343: High-Speed Steel
Thyrapid 3343 is a standard high-speed steel grade with balanced alloy composition, high toughness, good cutting power, and consequently versatile applications. Thyssen Thyrapid 3343 is suitable for all metal-cutting tools for roughing or finishing, such as twist drills, milling cutters of all types, taps, cutting tools, broaches, reamers, countersinks, chasens, segments for circular saws, shaping tools, and woodworking tools. This datasheet provides information on composition and physical properties. It also includes information on heat treating and machining. Filing Code: TS-560. Producer or source: Thyssen Specialty Steels Inc.
Journal Articles
Alloy Digest (1981) 30 (6): TS-383.
Published: 01 June 1981
... A1 Tech LMW is a molybdenum type of high-speed containing molybdenum and tungsten in the approximate ratio of 4 to 1. It is outstanding in high-speed cutting tool applications because of its machinability, toughness and good cutting qualities. It is used for numerous types of cutting tools...
Abstract
View articletitled, AL TECH LMW: High-Speed Steel, Type M1
View
PDF
for article titled, AL TECH LMW: High-Speed Steel, Type M1
A1 Tech LMW is a molybdenum type of high-speed containing molybdenum and tungsten in the approximate ratio of 4 to 1. It is outstanding in high-speed cutting tool applications because of its machinability, toughness and good cutting qualities. It is used for numerous types of cutting tools such as twist drills, reamers, milling cutters, gears cutters, broaches, lathe tools and wood-working tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-383. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1979) 28 (7): TS-351.
Published: 01 July 1979
... VASCO 8-N-2 is a molybdenum high-speed steel containing a low percentage of tungsten. It can be used successfully for a variety of cutting tools; in fact, it is a general-purpose high-speed steel. Its composition represents the first molybdenum high-speed steel to be manufactured and find...
Abstract
View articletitled, VASCO 8-N-2: High-Speed Steel, Type M1
View
PDF
for article titled, VASCO 8-N-2: High-Speed Steel, Type M1
VASCO 8-N-2 is a molybdenum high-speed steel containing a low percentage of tungsten. It can be used successfully for a variety of cutting tools; in fact, it is a general-purpose high-speed steel. Its composition represents the first molybdenum high-speed steel to be manufactured and find practical use in the field of cutting tools. Its many uses include drills, milling cutters, lathe tools, blanking dies and special shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-351. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1979) 28 (9): TS-353.
Published: 01 September 1979
... AL Tech LMW-V is a molybdenum-type high-speed steel used extensively by domestic cutting-tool makers. It was designed to offer increased wear resistance while retaining the toughness characteristic of molybdenum-type high-speed steels. It is suitable for a wide variety of cutting-tool applications...
Abstract
View articletitled, AL TECH LMW-V: High-Speed Steel, Type M7
View
PDF
for article titled, AL TECH LMW-V: High-Speed Steel, Type M7
AL Tech LMW-V is a molybdenum-type high-speed steel used extensively by domestic cutting-tool makers. It was designed to offer increased wear resistance while retaining the toughness characteristic of molybdenum-type high-speed steels. It is suitable for a wide variety of cutting-tool applications where improved resistance to abrasion is desired. Typical applications include twist dri milling cutters. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-353. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1985) 34 (12): TS-452.
Published: 01 December 1985
... TATMO V-N is an AISI Type M7 high-speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting-tool applications requiring an optimum balance of red hardness, edge toughness and wear resistance...
Abstract
View articletitled, TATMO V-N: High-Speed Steel, Type M7
View
PDF
for article titled, TATMO V-N: High-Speed Steel, Type M7
TATMO V-N is an AISI Type M7 high-speed steel modified by alloy balancing and a nitrogen addition to develop superior hardness response in heat treatment. It is an excellent grade for many cutting-tool applications requiring an optimum balance of red hardness, edge toughness and wear resistance, such as drills, taps, end mills, reamers and milling cutters. Its combination of outstanding properties and high hardness makes Tatmo V-N a logical alternate for cobalt high-speed steels in many cutting-tool applications. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-452. Producer or source: Latrobe Steel Company.
Journal Articles
Alloy Digest (1986) 35 (7): TS-461.
Published: 01 July 1986
... MAXITE is a tungsten-cobalt-vanadium high-speed tool steel. It is best used when maximum chip removal with single-point cutting tools is of primary importance. Tools made from Maxite will cut tough and hard materials such as stainless steels and hardened alloy steels with relative ease...
Abstract
View articletitled, MAXITE: Tungsten Cobalt High-Speed <span class="search-highlight">Tool</span> Steel, Type T8
View
PDF
for article titled, MAXITE: Tungsten Cobalt High-Speed <span class="search-highlight">Tool</span> Steel, Type T8
MAXITE is a tungsten-cobalt-vanadium high-speed tool steel. It is best used when maximum chip removal with single-point cutting tools is of primary importance. Tools made from Maxite will cut tough and hard materials such as stainless steels and hardened alloy steels with relative ease. It is excellent for cutting weld flashings and gritty, scaly hard castings. Among its many applications are drills, lathe tools, planer tools, cutoff tools and roll-turning tools. This datasheet provides information on composition and hardness. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-461. Producer or source: Columbia Tool Steel Company.
Journal Articles
Alloy Digest (1981) 30 (10): TS-389.
Published: 01 October 1981
... AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions...
Abstract
View articletitled, AISI TYPE T5: Heavy Duty High-Speed Steel
View
PDF
for article titled, AISI TYPE T5: Heavy Duty High-Speed Steel
AISI Type T5 is a tungsten high-speed steel to which cobalt (8.9%) is added to provide high and unusual red hardness. It is particularly well adapted for heavy-duty cutting and high-production cutting tools. Because of its high red hardness, a cutting edge can be maintained under conditions of speed, feed and depth of cut that would not be possible with ordinary high-speed steels. Typical applications of AISI Type T5 are lathe and planer tools, reamers, milling cutters and twist drills for heavy-duty cutting. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-389. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1972) 21 (11): TS-247.
Published: 01 November 1972
... AISI Type M30 is a high-speed tool steel containing 8% molybdenum and 5% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and superalloys, and is recommended for cutting tools requiring a good combination of suitable toughness with optimum cutting...
Abstract
View articletitled, AISI TYPE M30: Molybdenum Cobalt High-Speed Steel
View
PDF
for article titled, AISI TYPE M30: Molybdenum Cobalt High-Speed Steel
AISI Type M30 is a high-speed tool steel containing 8% molybdenum and 5% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and superalloys, and is recommended for cutting tools requiring a good combination of suitable toughness with optimum cutting qualities. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-247. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1983) 32 (11): TS-418.
Published: 01 November 1983
... VASCO M-30 is a high-speed tool steel containing nominally 8.70% molybdenum and 4.75% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and super-alloys. It is recommended for cutting tools requiring a good combination of suitable toughness...
Abstract
View articletitled, VASCO M-30: High-Speed Steel
View
PDF
for article titled, VASCO M-30: High-Speed Steel
VASCO M-30 is a high-speed tool steel containing nominally 8.70% molybdenum and 4.75% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and super-alloys. It is recommended for cutting tools requiring a good combination of suitable toughness with optimum cutting qualities. Typical applications of VASCO M-30 comprise milling cutters, broaches, drills, hobs, turning tools and dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-418. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1982) 31 (9): TS-404.
Published: 01 September 1982
... AISI Type O7 is a high-carbon, low-alloy tools designed for many types of cold-work cutting tools where the high-alloy, high-speed steels are not required. It has moderate hardenability, develops high hardness, holds a keen cutting edge and has excellent resistance to abrasion. Type O7 is used...
Abstract
View articletitled, AISI TYPE O7: Oil Hardening Cold Work <span class="search-highlight">Tool</span> Steel
View
PDF
for article titled, AISI TYPE O7: Oil Hardening Cold Work <span class="search-highlight">Tool</span> Steel
AISI Type O7 is a high-carbon, low-alloy tools designed for many types of cold-work cutting tools where the high-alloy, high-speed steels are not required. It has moderate hardenability, develops high hardness, holds a keen cutting edge and has excellent resistance to abrasion. Type O7 is used for a wide range of cold-working tools such as broaches, blanking dies, punches, thread-rolling dies, paper knives and wood-working tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-404. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1987) 36 (10): TS-483.
Published: 01 October 1987
... AISI Type M7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over AISI Type M1 in cutting characteristics without a significant loss in toughness. It is suitable for a wide...
Abstract
View articletitled, AISI TYPE M7: High-Speed Steel
View
PDF
for article titled, AISI TYPE M7: High-Speed Steel
AISI Type M7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over AISI Type M1 in cutting characteristics without a significant loss in toughness. It is suitable for a wide variety of cutting-tool applications where improved resistance to abrasion is required. The many uses of Type M7 include twist drills, end mills, shear blades, punches, milling cutters, lathe tools, taps and reamers. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-483. Producer or source: Tool steel mills. See also Alloy Digest TS-468, January 1987.
Journal Articles
Alloy Digest (1988) 37 (5): TS-490.
Published: 01 May 1988
... UNS No. T11310 is the high vanadium type of molybdenum high-speed steel. It is a deep-hardening steel and offers high cutting ability and excellent finishing properties. It is a general-purpose steel for cutting tools and is used in such applications as taps, lathe tools and reamers...
Abstract
View articletitled, UNS T11310: High-Speed <span class="search-highlight">Tool</span> Steel, Type M10
View
PDF
for article titled, UNS T11310: High-Speed <span class="search-highlight">Tool</span> Steel, Type M10
UNS No. T11310 is the high vanadium type of molybdenum high-speed steel. It is a deep-hardening steel and offers high cutting ability and excellent finishing properties. It is a general-purpose steel for cutting tools and is used in such applications as taps, lathe tools and reamers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating and machining. Filing Code: TS-490. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1977) 26 (7): TS-321.
Published: 01 July 1977
... AISI Type M10 is the high vanadium type of molybdenum high-speed steel. It is a deep-hardening steel and offers high cutting ability and excellent finishing properties. It is a general-purpose steel for cutting tools and is used in such applications as taps, lathe tools and reamers. This datasheet...
Abstract
View articletitled, AISI TYPE M10: Molybdenum High-Speed Steel
View
PDF
for article titled, AISI TYPE M10: Molybdenum High-Speed Steel
AISI Type M10 is the high vanadium type of molybdenum high-speed steel. It is a deep-hardening steel and offers high cutting ability and excellent finishing properties. It is a general-purpose steel for cutting tools and is used in such applications as taps, lathe tools and reamers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-321. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1980) 29 (9): TS-370.
Published: 01 September 1980
... GUTERL M-7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over M1 in cutting characteristics without a significant loss in toughness. It is used widely for cutting-tool...
Abstract
View articletitled, GUTERL M-7: High-Speed Steel, Type M7
View
PDF
for article titled, GUTERL M-7: High-Speed Steel, Type M7
GUTERL M-7 is a molybdenum type of high-speed steel. It is somewhat similar to AISI Type M1 tool steel but with higher percentages of carbon and vanadium to provide an improvement over M1 in cutting characteristics without a significant loss in toughness. It is used widely for cutting-tool applications that require improved resistance to abrasion. Its many uses include reamers, twist drills, taps, lathe tools, end mills and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-370. Producer or source: Guterl Special Steel Corporation.