1-20 of 1994 Search Results for

cutting rolls

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (1): Cu-489.
Published: 01 January 1985
... MUELLER Alloy 3602 is a leaded brass of moderate strength and ductility. It is suitable for moderate thread rolling. Also, because of its free-cutting characteristics, it is suitable for high-speed screw-machine products. Among its many applications are hardware, unions, bolts, screws and nuts...
Journal Articles
Alloy Digest (2021) 70 (3): Cu-918.
Published: 01 March 2021
... Mueller Brass C36000 is a wrought, Cu-Zn-Pb alloy (leaded brass) that is suitable for high-speed screw machining applications and moderate thread rolling. On the basis of strength alone, it can safely be substituted for leaded steel in many applications. UNS C36000 is the most important commercial...
Journal Articles
Alloy Digest (2007) 56 (4): TS-646.
Published: 01 April 2007
... Weartec SF is a spray formed cold-work tool steel offering a combination of high wear resistance and very good resistance to chipping, along with good toughness and ductility. Weartec SF is suitable for the production of cutting rolls and slitter knives. This datasheet provides information on...
Journal Articles
Alloy Digest (1994) 43 (7): SA-227.
Published: 01 July 1994
...-227 Steel Alloy Revised JULY 1994 - DIGEST- JUNE 1969 DATA ON WORLD WIDE METALS AND ALLOYS LEDLOYAX Puliishsdby: ABoy Digesl. Inc 1201-677-9161 27 Canfiild Slmet. Orange. N.J. 070501 USA (Free-cutting steel) LEDLOY-AX is a lead and tellutium-bearing steel, having superior free-machining...
Journal Articles
Alloy Digest (1960) 9 (6): CS-13.
Published: 01 June 1960
...-Cutting Manganese Steel I AISI Cl141 is a tough, carbon-manganese steel characterized by its free-machining qualities. It is especially recommended for high production automatic machine products. Composition: carbon Manganese Phosphorus Sulphur 0.37 - 0.45 1.35 - 1.65 0.045 max. 0.080 - 0.13 Balance...
Journal Articles
Alloy Digest (1957) 6 (6): CS-6.
Published: 01 June 1957
... Characteristics: AISI Cl144 is not a through-hardening steel on heat treat- ment except in very thin sections and should not be used where it is essential that properties be approximately the same throughout the full section. It is a free-cutting steel. Forms Available: Hoc rolled and cold drawn bars...
Journal Articles
Alloy Digest (1983) 32 (3): CS-93.
Published: 01 March 1983
... reserved. ISSN : 002-614X AISI 1141 (Free-Cutting Carbon Steel) AISI II41 is a resulfurized carbon steel containing nominally l.SO?c manganese and 0.08-o. 13% sulfur to give it free- machining characteristics. It has relatively low hardenability. Its ductility and toughness are fairly good in the...
Journal Articles
Alloy Digest (1984) 33 (7): CS-102.
Published: 01 July 1984
... - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engineering Publications. Inc. Ail rights reserved. Published b! ISN:OO2-614X Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey AISI 1146 (Free-Cutting Carbon Steel) AlSl I 146 is a resulfttrized carbon steel containing nominally...
Journal Articles
Alloy Digest (1985) 34 (1): CS-103.
Published: 01 January 1985
... reserved. UN: 002-614X Filing Code: CS-103 Carbon Steel JANUARY 1995 Published bv Alloy Digest. Inc. 27 Canfield Street AISI 1151 (Free-Cutting Carbon Steel) Orange. New Jersey 07050 (201) 761-1090 AISI 115 1 is a resulfutized carbon steel containing nominally 0.85% manganese and a range of 0.08-O. 13...
Journal Articles
Alloy Digest (1963) 12 (1): Co-35.
Published: 01 January 1963
... be increased from 25% to 50% over high speed steels, but where the machine tool or nature of the cut will not permit the use of carbide. ALX is commonly used in the cast-to-shape form as extrusion dies and special hot rolls. It is recommended for service where the ambi- ent temperature does not...
Journal Articles
Alloy Digest (1983) 32 (10): CS-97.
Published: 01 October 1983
... characteristics. Heat the steel to 190~2200° F for hot forging or hot rolling. This steel also has good characteristics for the cold drawing of rods and bars. Weldability: AISI I137 is a free-cutting sreel high in manganese and sulfur. The non-metallic sulfides lower the ductility of the metal, causing the chip...
Journal Articles
Alloy Digest (1980) 29 (3): CS-82.
Published: 01 March 1980
... workability UNS G11390 AMI 1139 Filing Code: c8-82 carbon steel I I MARCH 1990 - DATA ON WORLD WIDE MnALS AND ALLOYS PlSbbk?dby @ Copyright 1980. Engineering Publications. Inc. Ail rights resected. Ellgkhag AIIoys DIgcst# Ia. POStOffkXBOI823 Upper Montclair, New Jmcy AlSl 1139 (Free-Cutting Carbon Steel...
Journal Articles
Alloy Digest (1984) 33 (4): CS-101.
Published: 01 April 1984
... Steel APRIL 1994 - DATA ON WORLD WIDE METALS AND ALLOYS 0 Copyright 1980. Engineering Publications. Inc. Ail rights reserved. UN: 002-614X Published b,r Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey AlSl1140 (Free-Cutting Carbon Steel) AlSl I 140 is a resulfurized carbon steel. It...
Journal Articles
Alloy Digest (1959) 8 (10): CS-10.
Published: 01 October 1959
... JALCASE No. 8 is a carbon-manganese cold finished steel having free-cutting characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: CS...
Journal Articles
Alloy Digest (1955) 4 (12): CS-4.
Published: 01 December 1955
... hardness heat treatability JALCASE no. 7 machinability tensile properties Filing Code: CS-4 Carbon Steel DECEMBER 1955 - DATA ON WORLD WIDE METALS AND ALLOYS P&is&d by Enghering AUoys Digest, Inc Upper Monrclair, New Jersey JALCASE NO. 7 (Free-Cutting Manganese Steel, Type Cl 137) JALCA!SE NO. 7 is...
Journal Articles
Alloy Digest (1973) 22 (12): CS-53.
Published: 01 December 1973
... Engineering Alloys Digest. Inc Upper Montclair, New Jew AISI 1132 (Free-Cutting Manganese Steel) AISI 1132 is a relatively tough, manganese alloy steel characterized by its free-machining qualities. It is recommended especial- ly for high production machine products. Composition: Carbon 0.27-0.34 Manganese...
Journal Articles
Alloy Digest (1960) 9 (10): CS-14.
Published: 01 October 1960
... physical properties tensile properties AM cm7 Filing Code: CS-14 Carbon Steel OCTOBER 1960 -DATA ON WORLD WIDE METALS AND ALLOYS AIS1 Cl117 (Free-Cutting Carburizing Steel) Pnblisbd by Engineering Alloys Digest, Inc. Upper Montclair, New Jersey AI81 Cl117 is a low-carbon free-machining case-hardening...
Journal Articles
Alloy Digest (1994) 43 (8): SA-212.
Published: 01 August 1994
... LEDLOY 4140 is a lead and/or tellurized chromium-molybdenum alloy steel having free cutting characteristics. It is recommended for gears, shafts, fasteners and similar machinery parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as...
Journal Articles
Alloy Digest (1958) 7 (5): CS-7.
Published: 01 May 1958
... toughness hardness heat treatability machinability physical properties tensile properties Filing Code: C5-7 Carbon 5teel AIS1 Cl137 MAY 1958 -DATA ON WORLD WIDE METALS AND ALLOYS Psblisbed k EngineeringAIloys~)iecst.Inc. Upper Montclair, New Jmp AISI Cl 137 (Free-Cutting Manganese Steel) AISI Cl137...
Journal Articles
Alloy Digest (1983) 32 (8): CS-96.
Published: 01 August 1983
... chasers threads can becut at 400 sfpm. Use emulsions and soluble oils for light cutting, and sulphurized mineral oils for more severe operations. Workability: AISI I I I7 should be hot forged or hot rolled in the range of 225G l95oC F. Cold-linished bars can be produced readily; as usual, cold working...