Alloy Digest (1983) 32 (8): CS-96.
Published: 01 August 1983
... AISI 1117 is a resulfurized carbon steel for use where a free-machining carburizing steel is required. Its manganese content (nominally 1.15%) provides some increase in hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized parts...
Journal Articles
Alloy Digest (1974) 23 (8): CS-55.
Published: 01 August 1974
... AISI 1118 is a resulfurized carbon steel for applications requiring a free-machining carburizing steel. Its relatively high manganese content provides increased hardenability in all applications and increased hardness and strength in uncarburized uses and in the core of carburized components. This...
Journal Articles
Alloy Digest (2021) 70 (3): Cu-918.
Published: 01 March 2021
... percentage of the machinability of UNS C36000, free-cutting brass. The rating is based on relative speed for equivalent tool life See Table 5. Information on annealing sourced from C36000, Copper Applications Development Association. Adapters; bolts, screws, and nuts; faucet components; fit- Stress Relieving...
Journal Articles
Alloy Digest (1984) 33 (4): CS-101.
Published: 01 April 1984
... performed with high-speed-steel drills of standard design at cutting speeds of 7@90 sfpm for I /2-in. drills. Thread chasing can be done at 30-65 sfpm using a I& I5 deg hook grind on the chaser. Thread chasing with carbide- tipped thread chasers can be done at 375 sfpm. Typical applications are screws...
Journal Articles
Alloy Digest (1985) 34 (1): Cu-489.
Published: 01 January 1985
... MUELLER Alloy 3602 is a leaded brass of moderate strength and ductility. It is suitable for moderate thread rolling. Also, because of its free-cutting characteristics, it is suitable for high-speed screw-machine products. Among its many applications are hardware, unions, bolts, screws and nuts...
Journal Articles
Alloy Digest (1960) 9 (5): CS-12.
Published: 01 May 1960
... JALCASE 100 is an improved high-strength, stress-stabilized, wear resistant, cold drawn bar steel having free-cutting characteristics. JALCASE 100-L has a lead content of 0.15-0.35% for applications requiring superior machinability. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1980) 29 (3): CS-82.
Published: 01 March 1980
... AISI 1139 is a carbon steel containing 1.35-1.65% manganese and 0.13-0.20% sulfur to furnish free-machining characteristics. It is recommended especially for high-production machined products. Among its many applications are splined shafts, screws, arbors, tool holders and propeller shafts. This...
Journal Articles
Alloy Digest (1980) 29 (12): Al-182.
Published: 01 December 1980
... ALUMINUM 6262 is an alloy with an excellent combination of machinability, strength and resistance to corrosion. Lead and bismuth are added to provide free-machining characteristics. Its many applications include screw-machine products, housewares, marine parts. aerospace fittings and general...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1323.
Published: 01 July 2020
... Zapp Ergste 1.4035YU is a medium-carbon, 13% chromium, free-cutting martensitic stainless steel that is designed for applications requiring high strength and hardness, along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2011) 60 (4): Cu-797.
Published: 01 April 2011
...) 303 (44) 32 75 HRB DOI: 10.31399/asm.ad.cu0797 Products Available: The standard forms available are rod, wire, and shapes. Although C36000 is typically designed for free cutting applications, the producer supplies this alloy with special chemistry or temper if needed to meet particular requirements...
Journal Articles
Alloy Digest (2014) 63 (6): Cu-831.
Published: 01 June 2014
... C37000 has excellent machining characteristics and is low lead, no silicon, and no bismuth. MUELLER ALLOY C37000 (Free Cutting Muntz Metal) MUELLER ALLOY C37000 Chemical Composition, wt (Typical analysis) Copper 59.0 62.0 Lead 0.8 1.5 Iron 0.15 max Zinc bal Physical Properties: Electrical resistivity, 20...
Journal Articles
Alloy Digest (1966) 15 (7): Cu-166.
Published: 01 July 1966
... Revere No. 145 is a free-cutting grade of copper recommended for high conductivity parts, such as electrical connectors, relays, fasteners, contacts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
... and coolant Approximate Cutting Speeds with HSS Tools Operatioo Speed, sfm Automatic screw machine Turret lathe :g::g Shaving or skiving 120-150 Milling 50-80 Drilling FgY:; g lo-25 2s;; lo-25 15-30 Cutting rates may be greatly increased with carbide tools, when applicable. Cast alloy or carhide tools...
Journal Articles
Alloy Digest (1976) 25 (4): Cu-311.
Published: 01 April 1976
... because of its good machinability, relatively low cost, excellent solder- ability, good brazeability and good resistance to cor- rosion. Its cold workability is better than that of Free- Cutting Brass but only fair; this is quite sufficient for many applications. Copper Alloy No. 370 rods are suit- able...
Journal Articles
Alloy Digest (1971) 20 (5): SA-265.
Published: 01 May 1971
... Steel-Alloy MAY 1971 - DATA ON WORLD WIDE METALS AND ALLOYS Pvblirbd by Engineering Alloys Digest, Inc. Upper Montclair. New Jersey USS CARlLLOY* FC (Free-Cutting Steel) USS CARILLOY FC is a resulphurized, mediumcarbon, manganesechromium-molybdenum steel with good machinability and high strength. It is...
Journal Articles
Alloy Digest (1974) 23 (7): Cu-281.
Published: 01 July 1974
... COPPER ALLOY No. 544 is a leaded phosphor bronze with a machinability rating of 80% of free-cutting brass. It is suitable for screw machine products and has many uses such as valve parts, shafts, bearings and gears. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1954) 3 (5): Cu-16.
Published: 01 May 1954
... 2142 - 250 2290 1170 280 1273 300 1427 Revolutions per Minute 1528 879 2 1070 1145 7030 586 7640 714 8570 764 439 9170 477 535 573 high production rate without a major sacri6ce of con- ductiviy. In many applications it can profitably replace tough machining copper, for the cutting characteristics of...
Journal Articles
Alloy Digest (1956) 5 (12): SA-51.
Published: 01 December 1956
... NITRALLOY EZ is a special alloy steel which can be nitrided, that is, surface hardened, without final quenching, by the action of ammonia gas at relatively low temperatures. It is the free-cutting grade of the nitriding steels. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (6): SA-305.
Published: 01 June 1974
... Nitriding BM is a free-cutting grade of nitriding steel that can be surface hardened by the standards nitriding processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as...
Journal Articles
Alloy Digest (1969) 18 (6): SS-226.
Published: 01 June 1969
... tests against Type 303, Type 203EZ has permitted a 12% to 50% increase in cutting speeds, increased drill life 2 to 4 times, and extended the form tool life 2 to 9 times at a combination of equivalent or increased speeds. With the higher permissible speeds, an improvement in surface finish has resulted...