Alloy Digest (1955) 4 (7): Cu-28.
Published: 01 July 1955
... CUPALOY is an age hardenable, high conductivity copper alloy with higher mechanical properties than copper, especially at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as deformation, and fatigue...