Alloy Digest (1983) 32 (4): Al-245.
Published: 01 April 1983
... for such items as cover plates and instrument cases. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1997) 46 (10): SA-488.
Published: 01 October 1997
... ASTM 514 covers quenched and tempered alloy steel grades of structural quality and primarily is intended for use in welded plate work in fabricated bridge and building members. This datasheet provides information on composition and tensile properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (1991) 40 (5): SA-459.
Published: 01 May 1991
... ASTM A514 covers quenched and tempered alloy steel grades of structural quality. A514 is intended primarily for welded plate work in bridges and other structures. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on heat treating...
Journal Articles
Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
... expansion, 10 6/K (10 6/°F) 25 100 °C (77 212 °F) 16.5 (9.2) 25 500 °C (77 932 °F) 18.2 (10.1) Specific heat capacity, 460 (0.11) J/kg K (Btu/lb °F) Resistivity, µ m 0.79 (475) ( circular-mil/ft) Magnetic permeability, 1.003 H = 200 Oe, fully annealed 13 mm (0.5 in.) plate Mechanical Properties...
Journal Articles
Alloy Digest (1968) 17 (2): Al-172.
Published: 01 February 1968
..., instrument cases and housings, cover plates, general purpose castings. Manufacturer: Swiss Aluminium Ltd. Neuhausen am Rheinfall, Switzerland ...
Journal Articles
Alloy Digest (1961) 10 (5): Al-103.
Published: 01 May 1961
... Available: Die castings Applications: Cover plates, instrument cases, general purpose castings. Manufnciurer: Aluminum Company of America Pittsburgh, Pennsylvania ...
Journal Articles
Alloy Digest (2008) 57 (1): Al-409.
Published: 01 January 2008
... Alcan 2027 was developed to provide better properties than incumbent alloy 2024. It is an aerospace alloy for cover panels. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and machining. Filing Code: AL-409...
Journal Articles
Alloy Digest (1990) 39 (3): CS-126.
Published: 01 March 1990
... covers rolled carbon steel for structural purposes. Chemical Requirements (Single figures are maxima) Product Carbon Manganese shapes All thick. 0.26 a Phosphorus 0.04 Sulfur 0.05 Silicon b Copper** 0.20 Plate thickness, in. To >3/4- >l l/2- >2 l/2- 3/4 1 l/2 2 l/2 4 >4 - -- 0.25 0.25 0.26 0.27 0.29...
Journal Articles
Alloy Digest (2016) 65 (12): SA-775.
Published: 01 December 2016
... properties pressure vessels tensile properties workability This datasheet covers 7% nickel alloy steel plates for use in the water quenched and tempered condition intended for the fabrication of welded pressure vessels. Chemical Composition, wt (Maximum) Carbon 0.13 Manganese, heat analysis 0.90...
Journal Articles
Alloy Digest (2023) 72 (8): Al-501.
Published: 01 August 2023
... motor parts, instrument cases, cover plates, a wide variety of general-purpose castings, and aircraft and marine items of many types. Information on applications sourced from 360.0 and A360.0: Al-Si-Mg General-Purpose Die-Casting Alloys, Properties and Selection of Aluminum Table 3 Ratings of casting...
Journal Articles
Alloy Digest (1990) 39 (7): SA-448.
Published: 01 July 1990
... ASTM A572 covers low-alloy, high-strength steels of four different yield strength levels, 42, 50, 60 and 65 ksi. Strengthening is provided by small additions of columbium, vanadium, columbium+vanadium or vanadium+nitrogen. Maximum carbon is at 0.21 to 0.26%, depending on thickness, as shown...
Journal Articles
Alloy Digest (2011) 60 (6): SA-627.
Published: 01 June 2011
...@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Steel Alloy June 2011 SA-627 The data sheet covers material produced to API Grade 2MT1 steel plate. SSAB API GRADE 2MT1 (Intermediate Strength Steel Plate) SSAB API GRADE 2MT1 Chemical Composition(a), wt. %: Carbon 0.12 Manganese 1.15 1.60...
Journal Articles
Alloy Digest (2017) 66 (3): Al-455.
Published: 01 March 2017
... is covered by AMS 4473. Material design allowables are available for both tempers in the MMPDS Handbook. General Characteristics: Alcoa developed aluminum alloy AA 2624 for use in aerospace plate applications requiring very high damage tolerance properties. Compared to alloy 2024 and 2324 plate properties...
Journal Articles
Alloy Digest (1991) 40 (5): SA-460.
Published: 01 May 1991
... ASTM A588 covers low strength, high-alloy steel grades. They are used primarily in boldly exposed situations, architecturally without painting. These steels are commonly referred to as weathering steels. This datasheet provides information on composition and tensile properties. It also includes...
Journal Articles
Alloy Digest (2008) 57 (4): Al-412.
Published: 01 April 2008
... Alcan 7040 alloy is an Al-Mg-Zn-Cu-Zr plate alloy, developed to improve strength-toughness over incumbent alloys 7010 and 7050. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and fatigue. It also includes information...
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
...: Transformer covers, controller covers, switch covers, transformer cones and wedges, turbine division s acers, circuit breaker dome adapters, motor shafts, era nl! -shafts for refrigerator units, journal boxes, liners, wearing plates, shovels, conveyors and crusher hammers. Manufacturer: Jessop Steel Company...
Journal Articles
Alloy Digest (2008) 57 (8): Al-416.
Published: 01 August 2008
.... Copyright © ASM International® 2008 2008 ASM International ALCAN 7056 ALCAN T7951 chemical composition corrosion-resistant alloys fracture toughness heat treatability physical properties tensile properties workability ALCAN 7056-T7951 (Aluminum Plate Alloy) This data sheet covers Alcan...
Journal Articles
Alloy Digest (2008) 57 (7): Al-415.
Published: 01 July 2008
... International® 2008 2008 ASM International ALCAN 2297-T87 chemical composition corrosion-resistant alloys elasticity fatigue properties heat treatability physical properties tensile properties workability ALCAN 2297-T87 (Aluminum-Lithium Plate Alloy) This datasheet covers Alcan 2297 alloy...
Journal Articles
Alloy Digest (2008) 57 (10): Al-418.
Published: 01 October 2008
... Alcan 7040 is an Al-Mg-Zn-Cu-Zr alloy, developed to provide an improved strength-toughness balance versus incumbent 7010 and 7050 alloys. This datasheet covers Alcan 7040 alloy in T7651 temper. The alloy is used in aerospace structures. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1971) 20 (12): CS-45.
Published: 01 December 1971
... As-Rolled Yield Strength (0.2% offset), ps+ RQC-90 As-Rolled Temperature Piate oF Steel Constructional Steels* plate Steel Constictional Steels* 75 113000 200 107000 400 107000 600 110000 800 88000 1000 58000 1200 28000 *Range in steels covered by Heat Tmtment: Quench and Temper: Heat to 16500F minimum...