1-20 of 20 Search Results for

cover panels

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (1): Al-409.
Published: 01 January 2008
... Alcan 2027 was developed to provide better properties than incumbent alloy 2024. It is an aerospace alloy for cover panels. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and machining. Filing Code: AL-409...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (8): Al-405.
Published: 01 August 2007
... Alcan 2098 and 2x98 are Al-Cu-Li-Mg-Ag alloys designed to provide a balanced combination of high strength, low density, fatigue resistance, and fracture toughness for aerospace applications. This data sheet covers Alcan 2098 and 2x98 Al-Li fuselage sheets. The O and T82P tempers show improvement...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (3): Al-455.
Published: 01 March 2017
... resistance (ASTM G47) in the LT direction typically ranges from 152 to 200 MPa (22 29 ksi). The same or similar corrosion protection measures currently used on 2024-T351 and 2324-T39 parts should be applied to 2624-T351 and 2624-T39. Specification Equivalents: 2624-T351 is covered by AMS 4464, and 2624-T39...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (4): Al-442.
Published: 01 April 2015
... Magnesium 2.0 2.7 Manganese 0.10 Copper 1.9 2.5 Manganese 0.3 Chromium 0.04 Zirconium 0.08 0.15 Iron 0.15 Silicon 0.12 Titanium 0.15 Others, each 0.05 Others, total 0.15 Aluminum bal Mechanical Properties: Mechanical properties are shown in Tables 1 and 2 for plate, while Table 3 covers extrusions...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (12): SA-481.
Published: 01 December 1994
.... and subsequent re-heating, the material maintains dimensional stability. Applications: Rubber molds . . . 0 Rings, Seals Plastic Molds . . . Washer Dial Plates, Decorative Lighting Covers, Panels, Keyboards, Reels, Cases etc. for VCRs. Tape Players, Computers, Automobile Steering Wheels. Ash Trays, Electrical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (2): Al-453.
Published: 01 February 2017
... in yield strength (Fty) when compared to 2524-T3. The plane stress fracture toughness is also greatly improved as demonstrated by the guaranteed minimum Kapp values from 406 mm (16 in.) wide panels in the table and in the plots of typical Kapp vs. Fty and typical R-curves from 762 mm (30 in.) wide...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (7): SA-482.
Published: 01 July 1996
... must be carried out in such a manner that dilution of the components is kept under control in order to obtain a weld with optimal corrosion resistance and mechanical properties. A suitable welding method is MhIA (SMAW) welding with covered electrodes. Manual TIG (GTAW) welding is recommended...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (12): Al-419.
Published: 01 December 2008
... Alcan 6056 alloy is an Al-Si-Mg-Zn-Cu-Mn weldable alloy, developed to provide medium strength similar to the incumbent 2024 alloy, with a lower density. This datasheet covers ALCAN 6056 in several tempers as thin extrusions. The alloy possesses, in several tempers, a superior combination...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (8): Al-416.
Published: 01 August 2008
... Alcan 7056 is an Al-Mg-Zn-Cu-Zr alloy developed to provide an improved static/toughness balance versus incumbent 7150 and 7449 alloys. This data sheet covers Alcan 7056 alloy in the overaged T7951 temper. The alloy possesses very high toughness with improved corrosion resistance over 7150...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (8): Al-424.
Published: 01 August 2009
... Alcan 2027 is an Al-Cu-Mg-Mn-Zr alloy, developed to provide higher strength and damage tolerance than the incumbent 2024 alloy. Alcan 2027 T3511 possesses good damage tolerance. This datasheet covers Alcan 2027 T3511 in both thin and the heavier cross sections. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (5): Al-403.
Published: 01 May 2007
... Alcan 7449 is an Al-Mg-Zn-Cu-Zr alloy, developed to provide higher-strength properties than incumbent 7175 and 7150 alloys. This data sheet covers the Alcan alloy 7449 in the forms of thick extrusions and extruded bars. Tempers are presented that show improvement over both 7150 and 7175 aluminum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (3): Al-206.
Published: 01 March 1973
... ALUMINUM 5050 is a wrought, non-heat treatable aluminum alloy of excellent workability and high corrosion resistance. (This alloy is covered under its old designation, ALUMINUM 50S, in Alloy Digest Al-6, March 1953.) This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (8): Ni-460.
Published: 01 August 1994
... filler metal) NICROBRAZ 50 is a low-melting, free-flowing filler metal for honeycomb structures and thin-walled tube assemblies. It has low solubility. Covered under U.S. Patent Nos. 2868639 and 3188203. @NICROBRAZ is a registered trademark of Wall Colmonoy Corp. Nominal Composition, Wt, %: Chromium 14.0...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (7): SS-648.
Published: 01 July 1996
... for pressure vessel applica- tiOnS. The alloy is particularly suitable for applications covering the -50 C/+300°C (-58 F/572 F) mnpetmm interval. Lower tem- peratures may also be considereQ but need some restrictions. particularly when considering welded structures. Due to its duplex microstructure. with low...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (10): Zn-34.
Published: 01 October 1978
... components, injection molding dies, machine guards, decorative holloware, automotive components such as instrument covers, door linings and panels, watchcases and parts requiring precise detail. Manufacturer: The New Jersey Zinc Company, G+W Natural Resources Group Bethlehem, Pennsylvania 18017. ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (4): P-2.
Published: 01 April 1989
... by glass fiber reinforcement. Applications: Injection molded automotive body components such as instrument panels and wheel covers. They have a potential for use in appliance housings, impellers, propellers, lawn and garden equipment and others. Manufacturer: The Dow Chemical Company Midland, Michigan...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (8): Be-2.
Published: 01 August 1972
..., the average airborne beryllium concentrations in the occupational envuonment should not exceed the limiting value recommended by the American Conference of Government Industrial Hygienists. Forms Available: Sheet, 0.020 to 0.249-in. thick. Applications: Panels, formed structural members. fairing and skin...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1953) 2 (3): Al-6.
Published: 01 March 1953
... higher than that of 3s alloy. This alloy is covered by ASTM B209-51T and m B178-51T. Forms Available: Flat and coil sheet, rod and wire in annealed, fuIl hard, and intermediate tempers, and welded and seamless tubing. Applications: Trim molding, inside and outside panels for refrigera- tors, awnings...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (5): SS-311.
Published: 01 May 1975
..., and 201 stainless steels, while, in stronger acids, USS TENELON is equal fo, or better than Type 430. After about six years exposure of USS TENELON, test panels indicate this stainless steel is comparable to AISI Type 304 stainless in rural and in industrial atmospheres. After about three years exposure...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (8): CS-228.
Published: 01 August 2022
... by Soils. The corrosion rate of non-alloy steels in soils is varied and hard to predict owing to the multitude of variables involved. Extensive field tests conducted at various locations in the United States, covering almost all types of soils, showed that the overall corrosion rates of steel specimens...