Alloy Digest (2020) 69 (7): Cu-910.
Published: 01 July 2020
... Wieland Duro Elmedur B2 is a heat-treatable copper-beryllium alloy. This alloy exhibits high hardness and good electrical conductivity in the age hardened condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1976) 25 (3): Cu-310.
Published: 01 March 1976
... AMPCOLOY 83 is a wrought copper-base alloy containing nominally 1.8% beryllium. It offers good formability in the unhardened condition and can be strengthened by precipitation hardening. It has a combination of high strength and hardness, good ductility, good electrical and thermal conductivity...
Journal Articles
Alloy Digest (2000) 49 (7): Cu-650.
Published: 01 July 2000
... Brushform 290 is a high-strength beryllium-copper alloy used in electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1987) 36 (12): Cu-532.
Published: 01 December 1987
... BRUSH Alloy 165 has slightly less yield and fatigue strengths than the somewhat higher beryllium-content copper-beryllium alloy. It is cheaper and may be substituted when design requirements are less demanding. It is easily worked to provide complex shapes. This datasheet provides information on...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-717.
Published: 01 June 2004
... Brush 60 is a high-performance, lower-priced copper beryllium alloy offering cost-effective solutions for many applications such as electronic contacts and springs in the computer, datacom, and telecommunications markets. It is available in mill-hardened tempers. This datasheet provides...
Journal Articles
Alloy Digest (1986) 35 (1): Cu-505.
Published: 01 January 1986
... BRUSHFORM 290 is a specially processed, mill-hardened beryllium copper alloy having improved formability while maintaining the strength of other mill-hardened copper beryllium alloys. It was developed for current carrying springs requiring greater formability. It can be used in a number of...
Journal Articles
Alloy Digest (1990) 39 (10): Cu-555.
Published: 01 October 1990
... Copper alloys C17400 and C17410 are high thermal and electrical conductivity materials that reflect modest strengthening from their low alloy contents. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1992) 41 (9): Cu-576.
Published: 01 September 1992
... BRUSH CASTING ALLOYS 165C AND 165CT are beryllium copper alloys of high strength with cobalt as the second alloying element (0.20 to 0.65% Co). Use is in the age-hardened temper. Brush casting alloy 165CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
... BRUSH CASTING ALLOYS 245C AND 245CT are beryllium copper (2.25-2.55% Be) alloys of high strength with cobalt as the second alloying element (0.35-0.70% Co). Use is in the age-hardened temper. Brush casting alloy 245CT is the fine-grained version. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... BRUSH CASTING ALLOYS 275C AND 275CT are beryllium copper alloys of very high strength with cobalt and silicon as the secondary alloying elements. Use is in the age-hardened temper. Brush casting alloy 275CT is the fine-grained version. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-581.
Published: 01 January 1993
... BRUSH CASTING ALLOYS 20C AND 20CT are beryllium copper alloys (1.90-2.15% Be) of very high strength with cobalt as the second alloying element (0.35 to 0.70% Co). Use is in the age-hardened temper. Brush casting alloy 20CT is the fine-grained version. This datasheet provides information on...
Journal Articles
Alloy Digest (1980) 29 (5): Cu-394.
Published: 01 May 1980
... Copper Alloy No. 173 is a precipitation-hardenable beryllium-copper alloy with a lead addition of nominally 0.40% to give it fairly good machinability. By combining work hardening and precipitation hardening, tensile strengths in excess of 200,000 psi can be developed. This alloy is characterized...
Journal Articles
Alloy Digest (1977) 26 (5): Cu-333.
Published: 01 May 1977
... properties tensile properties thermal conductivity welding equipment workability wrought copper alloys Copper Alloy No. 175 Filing Code: cu-333 Copper Alloy MAY 1977 - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbed by Copper Alloy No. 175 Engineering Alloys Digest, Inc. (Age-Hardenable Beryllium...
Journal Articles
Alloy Digest (1966) 15 (6): Cu-165.
Published: 01 June 1966
... Copper Alloy No. 172 is a precipitation hardening beryllium-copper alloy having high elastic and endurance strength, good electrical and thermal conductivity, excellent resistance to wear, and high resistance to general corrosion. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (8): Cu-190.
Published: 01 August 1968
... COPPER Alloy No. 170 is a wrought, heat treatable beryllium-copper alloy offering high strenght, toughness, and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1986) 35 (6): Cu-512.
Published: 01 June 1986
... Copper Alloy No. C82500 is an age-hardenable copper-base casting alloy containing nominally 2% beryllium. It offers high strength, toughness and good resistance to corrosion. It has good fatigue strength in the age-hardened condition. Typical uses include bushings, bearings, valves, cams and...
Journal Articles
Alloy Digest (1987) 36 (4): Cu-523.
Published: 01 April 1987
... Copper Alloy No. C82000 is an age-hardenable copper-base casting alloy containing nominally 0.6% beryllium. Its common name is Beryllium Copper Casting Alloy 10C. It offers fairly high strength and moderate ductility with good resistance to corrosion. Its applications include bearings and bushings...
Journal Articles
Alloy Digest (1987) 36 (6): Cu-525.
Published: 01 June 1987
... Copper Alloy No. C82400 is a copper-base alloy containing nominally 1.70% beryllium. It is characterized by high strength and good resistance to corrosion. Typical applications include safety tools, molds for parts made of plastics, cams, valves and gears. This datasheet provides information on...
Journal Articles
Alloy Digest (1987) 36 (8): Cu-527.
Published: 01 August 1987
... Copper Alloy No. C82600 is an age-hardenable copper-base casting alloy. Nominally it contains 2.3% beryllium. It is characterized by high strength, toughness and good corrosion resistance. Typical uses comprise bearings and molds for plastics. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
..., making it possible to produce an alloy that has both high strength and high conductivity. Alloy 390 combines the best attributes of two separate families of commercial copper-beryllium alloys: the strength of the high-strength alloy C17200 with the conductivity of high-conductivity alloys C17410 and...