Alloy Digest (1972) 21 (10): Cu-259.
Published: 01 October 1972
... COPPER No. 104, 105 and 107 are oxygen-free coppers containing silver to raise the softening temperature and improve the elevated-temperature properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well...
Journal Articles
Alloy Digest (1961) 10 (7): Cu-104.
Published: 01 July 1961
... joinability machinability physical properties tensile properties workability -DATA ON WORLD WIDE METALS Filing Code: Cu-104 Copper Alloy CUNISIL - 837 JULY 1961 i AND ALLOYS CUNISIL - 837 (High-Strength Copper Alloy) Cunisil-837 is a copper-nickel-silicon alloy having high strength and corrosion...
Journal Articles
Alloy Digest (1994) 43 (10): Al-328.
Published: 01 October 1994
... Melting range, OF ( C) 950-1110 (510-600) TImmal coef. expansio#F (68-212OF) (20-100) 11.9 (21.4) x10-6 (68-572OF) (20-300) 12.7 (22.9) x 104 Tbamd conductivity, cd/cm s C (W/mOC), at 2YC 25 (104) PROPERTIES Table 1 - MECHANICAL PROPERTIES OF PERMANENT MOLD CASTINGS (Typical values) Ultimate tensile...
Journal Articles
Alloy Digest (1991) 40 (12): Cu-567.
Published: 01 December 1991
... resistance alloy with near constant resistance over the range 15 to 40°C (59 to 104°F). It is used in precision electrical components. Composition (Nominal): Copper Manganese Nickel 84 12 4 Physical Properties: Density, lb/cu in. Specific gravity Melting point (Approximate) C OF Thermal coef. expansionK (20...
Journal Articles
Alloy Digest (1989) 38 (6): Cu-547.
Published: 01 June 1989
... COPPER No. C15715 is a dispersion hardened copper fabricated by powder metallurgy techniques. Its electrical conductivity is 92% IACS and its annealed tensile strength (0.050 in. diameter wire) is 52000-66000psi, depending on annealing temperature. This datasheet provides information...
Journal Articles
Alloy Digest (1989) 38 (7): Ni-373.
Published: 01 July 1989
... EVANOHM alloy S offers optimum stability and flexibility with regard to both size and required temperature coefficient of resistance. Its extremely low electromotive force vs copper together with its high electrical resistivity are highly desirable properties in a precision resistance wire...
Journal Articles
Alloy Digest (1991) 40 (9): Cu-564.
Published: 01 September 1991
... Copper Alloy No. C62500 is a high strength extruded aluminum bronze. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (1992) 41 (4): Cu-570.
Published: 01 April 1992
... Copper Alloy No. C19210 has a nominal copper content of 99.9%. It is not heat-treat hardenable but it can be hardened by cold work. Its electrical conductivity is 80% IACS @ 68 F and it has good heat resistant characteristics. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2019) 68 (1): Cu-883.
Published: 01 January 2019
... Alloy 7026 is a copper-nickel-silicon alloy for the electrical industry. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion resistance. Filing Code: Cu-883. Producer or source: Gebr...
Journal Articles
Alloy Digest (1989) 38 (12): Cu-544.
Published: 01 December 1989
... COPPER No. C15700 is a dispersion hardened copper fabricated by powder metallurgy techniques. It has good strength and electrical conductivity. It has applicability at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2007) 56 (1): SS-983.
Published: 01 January 2007
...-FG46 fracture toughness hardness machinability physical properties tensile properties workability thermal properties UNS S25500 Chemical Composition, wt Carbon 0.030 max Chromium 24.50 26.50 Copper 1.50 2.00 Molybdenum 3.10 3.80 Manganese 0.80 1.20 Nitrogen 0.20 0.25 Nickel 5.50 6.50...
Journal Articles
Alloy Digest (2018) 67 (6): Cu-873.
Published: 01 June 2018
... Alloy CuSn6 (UNS C51900) is a high-performance copper alloy. Typical uses include components for the electronics industry such as connector springs, relays, leaf springs, and switches as well as machine parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2000) 49 (7): Cu-650.
Published: 01 July 2000
... + nickel 0.20 min Cobalt + nickel + iron 0.6 max Lead 0.02 max Copper bal Physical Properties: Density, before aging, kg/m3 (lb/in.3 ) 8250 (0.298) Density, age-hardened, kg/m3 (lb/in.3 ) 8360 (0.302) Thermal conductivity, age hardened, W/m · K (Btu/(ft · h · °F)) 104 (60) Coefficient of thermal expansion...
Journal Articles
Alloy Digest (2018) 67 (8): Cu-877.
Published: 01 August 2018
... Alloy CuSn10 is a high-performance copper alloy. The alloy is characterized by good electrical and thermal conductivity and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength...
Journal Articles
Alloy Digest (1994) 43 (10): Cu-552.
Published: 01 October 1994
... Copper Alloy No. C15100 is an age-hardenable zirconium-copper lead frame alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (2003) 52 (7): Cu-705.
Published: 01 July 2003
... 0.015 max Phosphorus 0.020 0.040 Nickel (including cobalt) 1.3 1.7 Silicon 0.22 0.30 Copper bal Copper + sum of named elements 99.5 min Physical Properties: Density, kg/m3 (lb/in.3 ) 8890 (0.321) Specific gravity 8.88 Coefficient of linear thermal 17.6 (9.8) expansion, 10 6/K (10 6/°F) Electrical...
Journal Articles
Alloy Digest (1990) 39 (1): Al-233.
Published: 01 January 1990
... ALCOA ALUMINUM ALLOY 7050 is an aluminum-zinc-copper-magnesium alloy with a superior combination of strength, stress-corrosion cracking resistance and toughness, particularly in thick sections. In thin sections it also possesses an excellent combination of properties that are important...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... Alloy CuSn5 (UNS C51000) is a high-performance copper alloy. The alloy is characterized by good tensile strength, good electrical conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1989) 38 (3): Cu-545.
Published: 01 March 1989
... solution in the copper matrix. Including silver. Physical Constants: Density, Ibku in. (At 68OF) 0.319 Specific gravity 8.83 Melting point, ?F 1981 C 1083 Specific heat, J/kg/T 0.09 BtuPb/ F 380 Thermal coef. expansion/OF (68-572°F) 9.2 x 104 PC (20-3OOOC) 16.6 x 106 Thermal conductivity, Btu/ft2/ft/h/ F...
Journal Articles
Alloy Digest (1988) 37 (8): Ni-360.
Published: 01 August 1988
... JESSOP JS Alloy 400 is a nickel-copper alloy with an excellent combination of high strength, ductility and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well...