1-20 of 53 Search Results for

copper alloy no.510

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1971) 20 (8): Cu-238.
Published: 01 August 1971
... COPPER ALLOY No. 510 is a tin bronze containing about 0.25% phosphorus. It combines high strength and toughness with excellent fatigue properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-510.
Published: 01 May 1986
... composition compressive strength Copper alloy no. C86100 corrosion-resistant alloys ductility elasticity fracture toughness gears hardness heat treatability joinability machinability physical properties tensile strength UNS C86100 I P Copper Alloy No. C86100 Filing Code: Cu-510 -- Copper...
Journal Articles
Alloy Digest (1986) 35 (8): Ni-338.
Published: 01 August 1986
..., chromates, nitrates, peroxides, cupric salts, etc., can cause attack in a medium which would otherwise be relatively mild for the alloy. Specification Equivalents: UNS No. NO4405. QQ-N-28 1 D Class B. ASTM B 164-81. General Characteristics: CARPENTER NICKEL-COPPER ALLOY 405 is a sulfur-modified solid...
Journal Articles
Alloy Digest (1993) 42 (5): Cu-583.
Published: 01 May 1993
... Copper No. C15710 is a dispersion strengthened alloy with alumina. The strength is higher than copper while maintaining good electrical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-620.
Published: 01 October 1999
... WRM Alloy 194-9 is a modified C19400 with mechanical properties far exceeding the conventional composition (see COPPER ALLOY No. 194, Alloy Digest Cu-233, May 1971). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-319.
Published: 01 August 1985
... (476) 42 79 10 83000 (572) 74000 (510) 37 82 15 90000 (621) 85000 (586) 30 83 20 99000 (683) 92000 (634) 23 86 30 IllOOO(765) I05000 (724) 21 82 40 I 17000 (807) 112000 (772) 19 79 Heat Treatment: In both the cold-worked and hot-worked conditions, Carpenter Nickel-Copper Alloy 400 may be annealed or...
Journal Articles
Alloy Digest (1981) 30 (12): Cu-427.
Published: 01 December 1981
... prove more satisfactory as both a lubricant and coolant. Workability: Hot Working: Anaconda Alloy 226 can be hot worked with no difficulty in the temperature range 1400-l 6S0°F by procedures similar to those used for copper. Cold Working: The capacity of this alloy is excellent for cold working; in fact...
Journal Articles
Alloy Digest (1985) 34 (6): Cu-498.
Published: 01 June 1985
... temperature depend on the amount of cold working. Stress Relief: Heat to 650-950 F (343-510°C) and cool at any desired rate. Hardening: This alloy cannot be hardened or strengthened by any thermal treatment. It can be hardened and strengthened only by cold working. Copper Alloy No. C61500 has a fair...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-476.
Published: 01 May 1984
... Copper Alloy No. C34200 contains nominally 2% lead and has a machinability rating approaching that of Free-Cutting Brass. It is noted for its excellent thread-rolling and knurling properties. It is used for many screw-machine applications and it has good resistance to corrosion in many...
Journal Articles
Alloy Digest (2018) 67 (11): cu-881.
Published: 01 November 2018
... workability thermal properties UNS C42500 Alloy CuSn3Zn9 is a bronze alloy. Chemical Composition, wt.% (Nominal) Tin 1.5 3.5 Zinc 7.5 10.0 Phosphorus 0.2 max Copper bal Physical Properties Electrical Conductivity. Depending on temper. IACS: International Annealed Copper Standard Density, 20 °C (68 °F...
Journal Articles
Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
... MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Copper October 2010 Cu-789 Ampcoloy 95 has slightly higher mechanical properties than most alloys in its class. Applications include spot welding electrodes. AMPCOLOY® 95 (Extruded High-Performance Copper Alloy) AMPCOLOY...
Journal Articles
Alloy Digest (1959) 8 (8): Cu-79.
Published: 01 August 1959
...) (Hardened at 750°F.) Time in Hours No Gold Work 80 % Reduction i! 97-100 30 300-320 450 6 375 480 9 415 495 12 435 510 15 450 515 :Y 465 70 521 18 24 475 524 Table 5 -EFFECT OF AGING TEMPEIUTURE ON VICKERS HARDNESS (Samples had no cold work before hardening) (Hardness for Various Times at Indicated...
Journal Articles
Alloy Digest (1964) 13 (7): Cu-143.
Published: 01 July 1964
...-magnetic copper-base alloy chat responds to an age-hardening hear treat- ment. It is easily fabricated, welded and soldered. High strength and elastic limits are obtained with little or no distortion during the hardening oper- ation. The use of elecrrolytic metals in making this alloy (which insures low...
Journal Articles
Alloy Digest (2006) 55 (5): Cu-743.
Published: 01 May 2006
... The Hiduron series of alloys are medium-strength copper-nickel alloys that offer excellent corrosion resistance and good impingement erosion resistance. Hiduron 130 has high-strength equivalent to carbon steel with excellent properties in corrosion, wear resistance, and antifriction. This...
Journal Articles
Alloy Digest (2002) 51 (8): Cu-687.
Published: 01 August 2002
... CN8) (Hardenable Copper Alloy) Swissmetal alloy SM275H is a hardenable Cu-Ni-Sn alloy with good workability and corrosion resistance. It is often used in the automotive industry for springs, contacts, and clips. Swissmetal is a registered trademark of The Swissmetal Group. Table 1 Mechanical...
Journal Articles
Alloy Digest (1999) 48 (1): Cu-627.
Published: 01 January 1999
... elasticity electrical conductivity hardness joinability Olin C197 physical properties tensile properties thermal conductivity wear resistance workability OLIN C197 (Higher Conductivity Copper) Olin C197 is a second-generation high performance alloy developed by Olin Brass. It has a strength and...
Journal Articles
Alloy Digest (1954) 3 (1): Cu-14.
Published: 01 January 1954
... C.D.C. MANGANESE ALLOY No. 720 is a copper-manganese-nickel alloy that responds to hardening by heat treatment. It has high tensile and fatigue strength, wide hardness range, and excellent corrosion resisting characteristics. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1988) 37 (6): Ni-109.
Published: 01 June 1988
... INCOLOY alloy 825 is a nickel-chromium-iron alloy with additions of molybdenum, copper, and titanium. It is resistant to chloride-ion stress-corrosion cracking, to pitting and crevice attack, and to corrosion in both oxidizing and reducing media. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1979) 28 (7): Cu-377.
Published: 01 July 1979
... ANACONDA Alloy (A) 510 is the most widely used of the phosphor bronzes, and is noteworthy among the copper alloys for its resilience and fatigue strength. It is well adapted to all forms of cold work, is rugged and durable in severe service and provides an excellent bearing surface that limits...
Journal Articles
Alloy Digest (1983) 32 (2): Ni-283.
Published: 01 February 1983
... NICROFER 4221 is a fully austenitic nickel-chromium-iron-molybdenum-copper alloy that is stabilized (against intergranular corrosion) by an addition of titanium. It is resistant to stress-corrosion cracking, pitting corrosion and oxidizing and non-oxidizing hot acids. It has good mechanical...