Alloy Digest (1971) 20 (11): Cu-245.
Published: 01 November 1971
... COPPER ALLOY No. 774 is a nickel silver press-forging alloy that has a forgeability rating of 85% of that of Forging Brass. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
... Special Metals Inconel G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to yield increased resistance to heat affected-zone (HAZ) corrosion and improved weldability. Special Metals Inconel G-3 has excellent corrosion resistance...
Journal Articles
Alloy Digest (2009) 58 (9): Cu-774.
Published: 01 September 2009
... on forming, heat treating, machining, and joining. Filing Code: CU-774. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM International ANSONIA ALLOY C24000 chemical composition elasticity...
Journal Articles
Alloy Digest (2016) 65 (12): SA-774.
Published: 01 December 2016
... Physical Properties: Density, 20 °C (68 °F), kg/m3 (lb/in.3) 7830 (0.282) See Table 1. Copyright © 2016, ASM International®. All rights reserved. DUREHETE® 1055 (Bolting Alloy) Filing Code: SA-774 Steel Alloy :: December 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.8542...
Journal Articles
Alloy Digest (2002) 51 (10): SS-863.
Published: 01 October 2002
... AvestaPolarit LDX 2101 bridges chemical composition corrosion-resistant alloys heat treatability joinability tensile properties Chemical Composition, wt (Typical) Carbon 0.03 Silicon 0.7 Manganese 5.0 Chromium 21.5 Nickel 1.5 Molybdenum 0.3 Copper 0.3 Nitrogen 0.22 Iron bal Mechanical Properties: LDX...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
..., rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. KAISER ALLOY 6063 (High Strength Extruded and Drawn Products) KAISER ALLOY 6063 Chemical Composition, wt (Nominal) Silicon 0.20 0.6 Iron 0.35 max Copper 0.1 max Manganese 0.1 max...
Journal Articles
Alloy Digest (1970) 19 (4): Ni-152.
Published: 01 April 1970
... solid-solution alloy with excellent high-temperature properties which make it attractive for many application in aerospace and process industries. *Registered Trademark of International Nickel. Composition: Nickel Chromium Iron Aluminum Carbon Manganese Sulfur Silicon Copper 60.5 23.0 14.1 1.35 0.05 0.5...
Journal Articles
Alloy Digest (2010) 59 (7): SS-1070.
Published: 01 July 2010
... Copyright © ASM International® 2010 2010 ASM International chemical composition corrosion-resistant alloys elasticity fracture toughness hardness heat treatability high-temperature alloys joinability microstructure NAS 74N physical properties tensile properties workability thermal...
Journal Articles
Alloy Digest (1991) 40 (5): Ni-66.
Published: 01 May 1991
... Alloy) NIMONIC ALLOY 105 is a wrought nickel-cobalt-chromium-base alloy strengthened by additions of molybdenum, aluminum and titanium. It has been developed for service up to 950 C (1742°F). Composition*: Carbon 0.12 Silicon 1.0 Copper 0.2 Iron 1.0 Manganese 1.0 Chromium 14.0-15.7 Titanium 0.9-1.5...
Journal Articles
Alloy Digest (2006) 55 (2): Ni-630.
Published: 01 February 2006
... Nicrofer 7016TiAl (also known as alloy 751) is an age-hardening Ni-Cr-Fe alloy with both good corrosion resistance and high rupture strength. It is a slight modification of alloy Nicrofer 7016TiNb (alloy X-750) and is used in diesel exhaust valves. This datasheet provides information...