Alloy Digest (1968) 17 (2): Cu-185.
Published: 01 February 1968
... COPPER Alloy No. 770 is a spring quality copper-nickel zinc alloy having high resistance to corrosion. It is recommended primarily for optical goods, springs, resistance wire, hardware and similar products. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2009) 58 (5): Cu-770.
Published: 01 May 2009
..., machining, and joining. Filing Code: CU-770. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM International ANSONIA ALLOY C21000 chemical composition heat treatability joinability...
Journal Articles
Alloy Digest (1963) 12 (7): Cu-130.
Published: 01 July 1963
... chemical composition corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability machinability malleability modulus of elasticity physical properties Revere no. 770 tensile properties workability REVERE NO. 770 Filing Code: Cu-130 Copper Alloy JULY 1963...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-715.
Published: 01 June 2004
...-copper alloys. Product Forms Available: Strip Applications: Typical applications are automotive connectors where the strength and relaxation resistance are needed at higher tempera- tures than most bronze alloys can retain. Producer: Olin Brass East Alton, IL 62024-1197 (618) 258-5255 (618) 258-2769 (fax...
Journal Articles
Alloy Digest (1962) 11 (11): Al-120.
Published: 01 November 1962
... IMPALCO 770 is a heat treatable, high strength aluminum alloy available in bar form for machining applications. It is recommended for highly stressed structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (2004) 53 (7): Cu-719.
Published: 01 July 2004
... Alton, IL 62024-1197 (618) 258-5255 (618) 258-2769 (fax) e-mail: Info@olinbrass.com Web: www.olinbrass.com ISSN: 002-614X OLIN ALLOY C5118 Filing Code: Cu-719 Copper July 2004 OLIN ALLOY C5118 (Dispersion-Strengthened Phosphor Bronze) Olin Alloy C5118 is a 4% modified phosphor bronze alloy given both...
Journal Articles
Alloy Digest (2000) 49 (8): Cu-85.
Published: 01 August 2000
... are essentially the same as that of pure copper. CMW 3 sand cast- ings have a high impact strength, which is retained at elevated temperatures. Up to 410 °C (770 °F), the impact strength will not fall below 41 J (30 ft · lbf). The alloy has twice the creep strength of hard drawn copper wire at 100 °C (212 °F...
Journal Articles
Alloy Digest (2018) 67 (7): Cu-875.
Published: 01 July 2018
... Alloy CuSn8 (UNS C52100) is a high-performance copper alloy with 8% tin. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as forming and joining. Filing Code: Cu-875...
Journal Articles
Alloy Digest (2019) 68 (11): Cu-899.
Published: 01 November 2019
... Wieland-K57 (UNS C70350) is copper alloyed with low nickel for good fabricability for parts in the electrical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (2008) 57 (9): Al-417.
Published: 01 September 2008
... joinability machinability physical properties tensile properties workability ALCAN 2024-T3, T351X (Aluminum-Copper-Magnesium Alloy Extruded Bar) This datasheet covers Alcan 2024 alloy in T3 and T351x tempers. The alloy possesses good damage tolerance. Chemical Composition, wt (Typical) Silicon 0.50 max...
Journal Articles
Alloy Digest (2017) 66 (11): Cu-866.
Published: 01 November 2017
... Alloy KAD 442 (UNS C44250) is a high-performance copper alloy. Typical uses are applications where high strength and good formability combined with good stress relaxation resistance and moderate conductivity are required. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2017) 66 (12): Cu-867.
Published: 01 December 2017
... Alloy C688 is a high-performance copper alloy with very high conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming and joining...
Journal Articles
Alloy Digest (2016) 65 (2): Cu-847.
Published: 01 February 2016
... Trojan is a high-strength precipitation hardening copper-nickel-silicon alloy. It also has industrial media for safety in engineering. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear...
Journal Articles
Alloy Digest (2010) 59 (6): Al-429.
Published: 01 June 2010
... This datasheet covers Alcan 2024 alloy in T3 and T351x tempers for drawn tubes. The alloy possesses good damage tolerance. See also Alloy Digest Al-417. ALCAN 2024 T3, T351X TUBES (Aluminum-Copper- Magnesium Alloy) ALCAN 2024 T3, T351X TUBES Chemical Composition, wt (Typical) Silicon 0.50 max Iron 0.50 max...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-844.
Published: 01 November 2015
... Copper bal Physical Properties: Despite having relatively high alloying additions, Nibron still retains respectable thermal and electrical conductivity values. It also offers an exceptionally low magnetic permeability (<1.01) ideal for nonmagnetic instruments and components. Density, kg/m3 (lb/in.3) 8500...
Journal Articles
Alloy Digest (2015) 64 (2): SS-1202.
Published: 01 February 2015
... strength explains why the alloy behaves particularly well in abrasion-corrosion conditions (e.g., agitators, screws, rakes). Super duplex grades are frequently used in mixed acids containing chlorides. Thanks to its copper content, UR2507Cu performs very well in sulfate environments such as flue gas...
Journal Articles
Alloy Digest (2006) 55 (5): Cu-743.
Published: 01 May 2006
... The Hiduron series of alloys are medium-strength copper-nickel alloys that offer excellent corrosion resistance and good impingement erosion resistance. Hiduron 130 has high-strength equivalent to carbon steel with excellent properties in corrosion, wear resistance, and antifriction...
Journal Articles
Alloy Digest (2019) 68 (8): SA-850.
Published: 01 August 2019
... QL1 chemical composition low-temperature alloys physical properties tensile properties aldur® steels are a family of water-quenched, high-strength, fine-grained steels with a minimum yield strength between 500 and 960 MPa (72.5 and 139 ksi) and with excellent toughness at low temperatures...
Journal Articles
Alloy Digest (1982) 31 (1): Cu-429.
Published: 01 January 1982
... tensile properties workability UNS C26000 Filing Code: cu429 MUELLER ALLOY 2600 Copper Alloy JANUARY 1982 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications. Inc. WI rights reserved. MN: 002-614X MUELLER Alloy 2600 (Deep-Drawing Brass) MUELLER Alloy 2600 has the optimum...
Journal Articles
Alloy Digest (1958) 7 (6): Mg-38.
Published: 01 June 1958
... MAGNESIUM AZ92A is a good structural magnesium alloy particularly suitable for castings of variable wall thickness. It responds o an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...