1-20 of 201 Search Results for

copper alloy no. 752

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1969) 18 (11): Cu-208.
Published: 01 November 1969
... COPPER Alloy No. 752 is a deep drawing grade of nickel silver. It has high resistance to corrosion and tarnish. It is used primarily for drawn, spun and similar cold-worked parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2008) 57 (3): Cu-752.
Published: 01 March 2008
...%, H04 331 48 303 44 20 48 2 Half-hard, 15%, H02 290 42 269 39 35 42 Wire 0.08 0.035 mm grain size, OS035 228 33 76 11 40 0.08 1/8 Hard, H00 262 38 207 30 20 0.08 ½ Hard, H02 352 51 283 41 6 0.08 Hard, H04 386 56 352 51 3 DATA ON WORLDWIDE METALS AND ALLOYS Filing Code: Cu-752 Copper March 2008 Copyright...
Journal Articles
Alloy Digest (2005) 54 (8): SA-550.
Published: 01 August 2005
... S-TEN1 is a steel alloy containing copper and antimony to make it more resistant to dew-point corrosion than conventional carbon steels. It is used as tubing in economizers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2009) 58 (12): SS-1048.
Published: 01 December 2009
... DMV 928 is a nickel-base alloy with high alloying elements of chromium, molybdenum, and copper for excellent corrosion resistance in reducing and oxidizing media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (2007) 56 (12): Ti-144.
Published: 01 December 2007
... Timetal 230 is a binary alloy of titanium with 2.5% Cu to produce a cold-formable medium-strength alloy that can be used up to 350 deg C (660 deg F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also...
Journal Articles
Alloy Digest (1984) 33 (3): Cu-99.
Published: 01 March 1984
... circuit breakers commutators corrosion-resistant alloys creep properties elasticity electrical conductivity hardness heat treatability high-temperature alloys joinability machinability oxygen-free copper physical properties power rectifiers power transmitters switches tensile properties...
Journal Articles
Alloy Digest (2020) 69 (9): Ni-762.
Published: 01 September 2020
... Special Metals Inconel 740H (UNS N07740) is a precipitation hardenable, nickel-base superalloy that offers a unique combination of high strength and creep resistance at elevated temperatures along with resistance to coal ash corrosion. This alloy was originally targeted for use in advanced ultra...
Journal Articles
Alloy Digest (2010) 59 (8): Fe-152.
Published: 01 August 2010
... Intermediate component Copper 470 30 10 General Characteristics: Kanthal 135 R05 is a thermostatic bimetal which is recommended for use in the temperature range 20 to +250 °C ( 4 to 482 ºF) with extreme case capability to a maximum of +400 ºC (752 ºF). See also Table 3. Available Products: Kanthal offers...
Journal Articles
Alloy Digest (2015) 64 (4): SS-1205.
Published: 01 April 2015
... and discs, shafts, pins, bolts, screws, springs, exhaust reheaters, housing components, thrust nozzles. Liners for containers for tube and rod extruding of copper and copper-alloys; billet temperature higher than 700 °C (1292 °F). Producer: Böhler-Uddeholm Specialty Metals, Inc. South Boston, VA 24592, USA...
Journal Articles
Alloy Digest (2014) 63 (5): SS-1174.
Published: 01 May 2014
... max Nitrogen 0.15 0.35 Niobium 0.20 0.60 Manganese 2.00 max Copper 1.00 max Carbon 0.04 0.10 Iron bal Physical Properties: Density, kg/cm3 (lb/in.3) 8100 (0.29) Coefficient of thermal expansion, 10 6/K (10 6/°F) RT 300 °C (RT 572 °F) 16.9 (9.4) RT 400 °C (RT 752 °F) 17.2 (9.6) RT 500 °C (RT 932 °F...
Journal Articles
Alloy Digest (2009) 58 (11): SS-1047.
Published: 01 November 2009
... DMV 931 is an alloy for general and chloride corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... WRM ALLOY 5248 (Phosphor Bronze Alloy) WRM alloy 5248 is a phosphor bronze alloy with higher strength and better stress relaxation resistance than 10% tin alloys. WRM Alloy 5248 is patent pending. Chemical Composition, wt Copper Balance Tin 9 11 Iron 0.05 0.2 Nickel 0.05 0.2 Phosphorus 0.02 0.10 Lead...
Journal Articles
Alloy Digest (1998) 47 (4): SS-711.
Published: 01 April 1998
...: Carpenter type 204Cu is a copper-containing, low-nickel, nitrogen-strengthened, austenitic stainless steel. The nitrogen ad- dition results in higher annealed strength than type 304. The cop- per addition reduces the work hardening rate to provide cold worked properties similar to type 304. The alloy...
Journal Articles
Alloy Digest (2000) 49 (7): W-5.
Published: 01 July 2000
... and Anviloy are registered trademarks of CMW Inc. Moly-Dee is a trademark of Castrol Inc. Chemical Composition, wt (Nominal) Nickel 3.5 Copper 1.5 Tungsten bal Physical Properties: Density, kg/m3 (lb/in.3) 18,000 (0.65) Coefficient of linear expansion, 10 6/K (10 6/°F) 20 400 °C (68 752 °F) 4.43 (2.46) 20 800...
Journal Articles
Alloy Digest (1996) 45 (11): SS-660.
Published: 01 November 1996
... CLI-50A is a Korean 6 Mo superaustenitic stainless steel with improved corrosion resistance properties. The chromium additions have been increased up to 22% together with high nitrogen additions. The PREN value [%Cr] + 3.3 [%Mo] + 16[%N] is higher than 45. The alloy is copper free. This alloy...
Journal Articles
Alloy Digest (2012) 61 (10): Ni-702.
Published: 01 October 2012
... DMV 600L is a nickel alloy with 15.5 Cr. The alloy is used mainly as a material resistant to aqueous corrosion at temperatures below 450 deg C (842 deg F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2000) 49 (9): W-11.
Published: 01 September 2000
..., or welding, although mechanical join- ing is preferred. Sinter brazing can also used to join one CMW 3950 part to another when in the green state. Copper brazing is best performed at 1095 1120 °C (2000 2500 °F) in a reducing atmosphere using pure copper or a 92% Cu-8% Ni alloy. Stan- dard practice can...
Journal Articles
Alloy Digest (2014) 63 (12): SS-1194.
Published: 01 December 2014
... superduplex stainless steels and is less expensive than nickel base alloys. Moreover, the copper content increases its corrosion resistance in sulfuric acid solutions. It may be used in acidified solution polluted by very high chloride or fluoride additions, as can be seen on the guide map of material...
Journal Articles
Alloy Digest (2018) 67 (12): Ni-747.
Published: 01 December 2018
... Alloy 2120 MoN has a wide range of applications in the chemical, petrochemical, and pharmaceutical industries, as well as in energy production and environmental technologies. This alloy is also referred to as Nicrofer 5821 hMoN. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2017) 66 (3): Al-454.
Published: 01 March 2017
... Composition, wt (Nominal) Silicon 0.40 Iron 0.40 Copper 0.10 Manganese 0.50 Magnesium 2.60 3.60 Chromium 0.30 Zinc 0.20 Titanium 0.15 max Others, each 0.05 max Others, total 0.15 max Aluminum bal In order to achieve maximum homogeneity and consistent quality, the actual tolerances on both alloy...