Alloy Digest (1968) 17 (1): Cu-184.
Published: 01 January 1968
... COPPER Alloy No. 704 is a 5% nickel-copper alloy characterized by resistance to corrosion by high velocity sea water, resistance to stress-corrosion cracking, and retention of strength at moderately elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1998) 47 (6): Cu-617.
Published: 01 June 1998
... International® 1998 1998 ASM International chemical composition joinability Monel Electrode 187 tensile properties welding electrodes UNS W60715 - DIGEST A DATA ON WORLD WIDE METALS AND ALLOYS Filing code: W-617 MONEL@ ELECTRODE 187 (Copper-Nickel Welding Electrode) Monel Electrode 187 is an all...
Journal Articles
Alloy Digest (1967) 16 (3): Al-164.
Published: 01 March 1967
... BA.704 is a heat treatable aluminum extrusion alloy having high tensile and fatigue strengths. It is recommended for aircraft components, gears, fittings and machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1999) 48 (10): Cu-640.
Published: 01 October 1999
... WRM ALLOY 5248 (Phosphor Bronze Alloy) WRM alloy 5248 is a phosphor bronze alloy with higher strength and better stress relaxation resistance than 10% tin alloys. WRM Alloy 5248 is patent pending. Chemical Composition, wt Copper Balance Tin 9 11 Iron 0.05 0.2 Nickel 0.05 0.2 Phosphorus 0.02 0.10 Lead...
Journal Articles
Alloy Digest (2016) 65 (3): SS-1239.
Published: 01 March 2016
... when compared to other 17% chromium ferritics. The high silicon and manganese copper-added alloy reduces spalling when exposed to cyclic high THERMAK 17 (High-Temperature Ferritic Stainless) Filing Code: SS-1239 Stainless Steel :: March 2016 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax...
Journal Articles
Alloy Digest (2004) 53 (2): Co-95.
Published: 01 February 2004
... 607 88.0 807 117.0 39 64 DOI: 10.31399/asm.ad.co0095 Corrosion Resistance: Figure 1 provides a comparison of the cyclic oxidation resistance of various Inconel and Incoloy alloys. The oxidation rate of alloy 783 is slightly greater than alloy 718 at 704 ºC (1300 ºF). The results of salt fog testing...
Journal Articles
Alloy Digest (2003) 52 (2): Ni-601.
Published: 01 February 2003
... resistance. The addition of molybdenum and copper gives the alloy resistance to reducing chemicals and to pitting and crevice corrosion. The high chromium content provides resistance to oxi- dizing conditions, while the nickel protects the alloy from chlo- ride ion stress-corrosion cracking. The alloy...
Journal Articles
Alloy Digest (2012) 61 (10): Cu-813.
Published: 01 October 2012
... of B16. See Alloy Digest Cu-704. It has a combination of properties, particularly for the connector market. WIELAND-B16 SUPRALLOY® (Phosphor Bronze) WIELAND-B16 SUPRALLOY® Chemical Composition, wt (Reference chemistry) Copper 94 Tin 6 Physical Properties: Density, kg/m3 (lb/in.3) 8800 (0.32) Coefficient...
Journal Articles
Alloy Digest (2019) 68 (12): Cu-902.
Published: 01 December 2019
... Concast C95900 is a cast nickel-aluminum-bronze alloy. Aluminum bronze is the highest strength standard copper-based alloy. The nickel content in C95900 enhances its mechanical strength, wear, and corrosion resistance, making it suitable for heavy-duty applications. This datasheet provides...
Journal Articles
Alloy Digest (2003) 52 (7): Cu-704.
Published: 01 July 2003
...-working properties. The cold-working properties make it very suitable for applications requiring blanking, drawing, forming, shearing, and stamping. The alloy has excellent solder- ing, brazing, and resistance spot welding characteristics. It is WIELAND-B16 Filing Code: Cu-704 Copper July 2003 WIELAND-B16...
Journal Articles
Alloy Digest (2010) 59 (1): Cu-777.
Published: 01 January 2010
... Luvata C6476 is a copper alloy developed by Kobe Steel for the next generation of automotive terminals. Its designation is (CuNi1.8Si0.4Zn1.1Sn0.1Mg). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also...
Journal Articles
Alloy Digest (2009) 58 (7): Ni-671.
Published: 01 July 2009
... 19.0 21.0 Iron 0.7 Molybdenum 5.6 6.1 Copper 0.20 Titanium 1.9 2.3 Aluminum 0.3 0.6 Carbon 0.04 0.08 Manganese 0.60 Phosphorus 0.015 Sulfur 0.007 Silicon 0.40 Physical Properties: Density, kg/m3 (lb/in.3) 8360 (0.302) Mechanical Properties: Typical mechanical properties for Altemp 263 alloy are listed...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-595.
Published: 01 December 2002
... Nickelvac K-500 is a nickel-copper alloy with age-hardening properties imparted by alloying additions of aluminum and titanium. The alloy is characterized by excellent corrosion resistance in an extensive range of natural and chemical environments, excellent resistance to chloride-ion stress...
Journal Articles
Alloy Digest (2012) 61 (9): Ni-701.
Published: 01 September 2012
... NAS NW400 is a corrosion resistant nickel copper alloy that has resistance to reducing environments and sea water. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2017) 66 (3): Ni-728.
Published: 01 March 2017
...) 649 °C (1200 °F) 338 (49) 704 °C (1300 °F) 248 (36) 760 °C (1400 °F) 145 (21) See Fig. 1 for elevated temperature properties. Copyright © 2017, ASM International®. All rights reserved. NIMONIC® PE11 (Precipitation Hardened Nickel Alloy) Filing Code: Ni-728 Nickel :: March 2017 Materials Park, Ohio...
Journal Articles
Alloy Digest (1991) 40 (8): Ti-98.
Published: 01 August 1991
... ALLVAC 6A1-6V-2Sn is a highly beta stabilized alpha + beta titanium alloy, a modification of the 6 A1-4V system. Added vanadium plus copper and iron produce the stabilizing effect. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2012) 61 (12): Ni-704.
Published: 01 December 2012
... December 2012 Ni-704 DMV 825 is a nickel alloy with 21% Cr. The alloy has a balanced composition for use in both oxidizing and reducing conditions. DMV 825 (Nickel Alloy) DMV 825 Chemical Composition, wt (Typical values) Carbon 0.025 max Silicon 0.50 max Manganese 1.00 max Phosphorus 0.020 max Sulfur 0.01...
Journal Articles
Alloy Digest (2015) 64 (4): SS-1205.
Published: 01 April 2015
... Böhler (or Boehler) T200 is an age-hardenable austenitic Fe-Ni-Cr alloy designed for service up to 704 deg C (1300 deg F) on jobs requiring high strength and good corrosion resistance at the operating temperature. The alloy offers high ductility in notched sections. The alloy is used in jet...
Journal Articles
Alloy Digest (2016) 65 (8): Cu-849.
Published: 01 August 2016
... between 649 704 ºC (1200 1300 ºF). The alloy has excellent soldering, brazing, cold working, and plating characteristics. Forgeability is rated as 95% and welding as 70%. Copyright © 2016, ASM International®. All rights reserved. MUELLER ALLOY C27451 (No Lead Plumbing Brass) Filing Code: Cu-849 Copper...
Journal Articles
Alloy Digest (2010) 59 (3): Cu-780.
Published: 01 March 2010
... CustomerService@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Copper March 2010 Cu-780 Luvata C510 is a very common and frequently used alloy. The 5% Sn and 95% Cu alloy is deoxidized with 0.2% P. It is often called CuSn5. LUVATA C510 (Phosphor Bronze) LUVATA C510 Chemical...