Sort by
Journal Articles
Alloy Digest (1971) 20 (11): Cu-244.
Published: 01 November 1971
... COPPER ALLOY No. 675 is a copper-zinc alloy having excellent mechanical properties and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-384.
Published: 01 November 1979
... should be avoided. Specification Equivalents: UN.3 No. C67500. CDA Alloy 675. ASTM: B 124, Copper Alloy 675; B 138 Copper Alloy 675; B 283, Copper Alloy 675. FEDERAL: QQ-B-728, Class A. SAE: J461, J463. General Characteristics: Mueller alloy 6750 is a wrought manganese bronze containing nominally 58.5...
Journal Articles
Alloy Digest (2004) 53 (6): Cu-715.
Published: 01 June 2004
...-copper alloys. Product Forms Available: Strip Applications: Typical applications are automotive connectors where the strength and relaxation resistance are needed at higher tempera- tures than most bronze alloys can retain. Producer: Olin Brass East Alton, IL 62024-1197 (618) 258-5255 (618) 258-2769 (fax...
Journal Articles
Alloy Digest (1993) 42 (11): Cu-592.
Published: 01 November 1993
... COPPER ALLOY NO. C76200 is a nickel silver alloy with good fabricability, forming and brazeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2002) 51 (1): Cu-675.
Published: 01 January 2002
... composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties tensile properties WIELAND-Z35 workability thermal properties UNS C35330 Chemical Composition, wt (Reference Chemistry) Copper 62 Lead 2.5 Arsenic 0.1 Zinc bal Physical...
Journal Articles
Alloy Digest (2009) 58 (5): Cu-770.
Published: 01 May 2009
... Ansonia alloy C21000 is a 5% Zn alloy. It is red in color and the least expensive copper alloy to be used as gilding, an imitation gold leaf. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1961) 10 (7): Cu-104.
Published: 01 July 1961
... Cunisil-837 is a copper-nickel-silicon alloy having high strength and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (2016) 65 (5): Cu-848.
Published: 01 May 2016
... Wieland-C19700 is a copper alloy with a small amount of zinc for strength without removing its good copper physical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1987) 36 (11): Cu-530.
Published: 01 November 1987
... includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-530. Producer or source: Copper and copper alloy mills. See also Alloy Digest Cu-590, October 1993. Producer or Source: Copper and copper alloy mills Copyright © ASM International® 1996 1996...
Journal Articles
Alloy Digest (2008) 57 (12): SS-1025.
Published: 01 December 2008
... tools from sliding over the alloy. This alloy produces a good surface finish. Corrosion Resistance: The resistance of this alloy to intergranular attack is excellent even when sensitized at 675 °C (1250 °F) for 1 h to simulate the heat-affected zone of heavy weldments. Material annealed at 1065 °C (1950...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... COPPER ALLOY NO. C11100 is commonly called anneal-resistant electrolytic copper. It offers resistance to softening at slightly elevated temperatures by the addition of cadmium, which raises the temperature at which recovery and recrystallization occur. Its fabricating characteristics are the same...
Journal Articles
Alloy Digest (2003) 52 (4): Cu-699.
Published: 01 April 2003
... Outokumpu 5119, or KLF-7, is a high performance copper tin alloy with excellent combination of strength and stress relaxation resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. Filing Code: CU-699...
Journal Articles
Alloy Digest (1966) 15 (6): Cu-164.
Published: 01 June 1966
... CUNISIL-647 is a copper-nickel-silicon precipitation-hardening alloy having high strength, hardness, wear and corrosion resistance. Typical applications include electrical hardware and fasteners. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2018) 67 (5): Cu-871.
Published: 01 May 2018
... Alloy CuSn5 (UNS C51000) is a high-performance copper alloy. The alloy is characterized by good tensile strength, good electrical conductivity, and very good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2012) 61 (8): Cu-810.
Published: 01 August 2012
... EC70600 is a 90/10 copper-nickel alloy commonly used for applications in both fresh and saline waters. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (2008) 57 (8): Cu-757.
Published: 01 August 2008
..., and joining. Filing Code: CU-757. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2008 2008 ASM International Ansonia Alloy C54400 bearing properties chemical composition elasticity hardness heat...
Journal Articles
Alloy Digest (2003) 52 (9): Cu-709.
Published: 01 September 2003
... specific conditions of service, copper is generally less subject to corrosion than other engineering metals. Copper often is used where resistance to corrosion is of prime importance. Sometimes it is better to use a copper alloy rather than an unal- loyed copper. In general, copper resists nonoxidizing...
Journal Articles
Alloy Digest (2005) 54 (12): Cu-738.
Published: 01 December 2005
... Wieland K-88 is a copper alloy with very high electrical and thermal conductivity, good strength, and excellent stress relaxation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2009) 58 (2): Cu-766.
Published: 01 February 2009
..., heat treating, machining, and joining. Filing Code: CU-766. Producer or source: Ansonia Copper & Brass Inc. Producer or Source: Ansonia Copper & Brass Inc. Copyright © ASM International® 2009 2009 ASM International aircraft hydraulic lines ANSONIA ALLOY C65100 chemical...
Journal Articles
Alloy Digest (1985) 34 (6): Cu-498.
Published: 01 June 1985
... hard (cold worked 50%) followed by one-hour stress relief at 572OF (300 0 Heat Treetment: Machinability: Annealing: After Copper Alloy No. C61500 has been cold worked, it can be softened (recrystallized) by heating to l15~1250°F (620-675 C) and cooling at any desired rate. Annealing time...