1-20 of 43 Search Results for

copper alloy no. 655

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1972) 21 (1): Cu-248.
Published: 01 January 1972
... COPPER ALLOY No. 655 is a high-silicon copper alloy which has good mechanical properties and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-510.
Published: 01 May 1986
... Copper Alloy No. C86100 is a copper-zinc-aluminum-manganese-iron alloy, sometimes classified as a high-strength yellow brass. The principal strengthening element is aluminum. Its tensile strength is typically 95,000 psi (655 MPa). It has a good combination of strength and ductility along with good...
Journal Articles
Alloy Digest (1994) 43 (6): Cu-598.
Published: 01 June 1994
...: AMETEK Specialty Metal Products Copyright © ASM International® 1996 1996 ASM International chemical composition COPPER ALLOY No. C72650 elasticity electrical contacts hardness heat treatability joinability physical properties springs tensile properties workability wrought copper...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-588.
Published: 01 September 1993
... COPPER ALLOY NO. C72900 is a spinodal alloy that develops exceptionally high elastic strength levels; dimensional stability and relaxation resistance at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi. It has an excellent combination of strength and ductility along with good resistance...
Journal Articles
Alloy Digest (1980) 29 (6): Cu-397.
Published: 01 June 1980
... Copper Alloy No. C95800 is a copper-aluminum-nickel-iron-manganese alloy with high strength and hardness. It also is characterized by excellent resistance to corrosion and good resistance to fatigue and wear. It is suited for service up to 750 F. Typical uses comprise hubs and blades of ship...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-509.
Published: 01 May 1986
... I74 is the preferred spring material where traditional copper-base alloys are inadequate. *BRl!SH is a registered trademark of Brush Wellman Inc. Chemical Composition: Copper Allo> No. C I 7300 Cl7410 Iron 0.2 max. 0.2 mas. Cobalt 0. I S-O. 35 0.35-0.60 Silicon 0.2 max. 0.2 max. Beryllium 0.15-O. 50...
Journal Articles
Alloy Digest (1985) 34 (8): Ni-319.
Published: 01 August 1985
... Equivalents: QQ-N-28 I D. AUS 7233C. ASTM B 164-81. UNS No. NO4400. General Characteristics: As mentioned in the introduction, Carpenter Nickel-Copper AUoy 400 is a solid-solution binary alloy, combining high strength (comparable to structural steel) and toughness over a wide temperature range, with excellent...
Journal Articles
Alloy Digest (1999) 48 (3): Cu-631.
Published: 01 March 1999
... provided by Olin in the mill-hardened condition. No further heat treatment by users is necessary. During the thermal aging of C7025, alloying elements held in solid solu- tion precipitate from the copper matrix. Nickel and silicon atoms, in a specific ratio, combine as fine particles. This produces a...
Journal Articles
Alloy Digest (1999) 48 (5): Cu-635.
Published: 01 May 1999
... Park, Ohio 44073-0002 440-338-5151 Fax 440-338-4634 Mem-Serv@po.ASM-Intl.org Filing Code: Cu-635 Copper May 1999 OLIN ALLOY 186 Table 1 Comparison of Electrical Conductivity of Olin Alloy 186 with Other Connector Alloys Alloy No. Nominal composition, % Minimum conductivity, %IACS C15100 0.1Zr 90 C15500...
Journal Articles
Alloy Digest (1996) 45 (10): SS-655.
Published: 01 October 1996
... information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-655. Producer or source: Creusot-Marrel. Producer or Source: Creusot-Marrel...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-843.
Published: 01 November 2015
... AM388 is a copper-base spinodal alloy with high strength combined with formability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on forming and heat treating. Filing Code: Cu-843. Producer or...
Journal Articles
Alloy Digest (2000) 49 (10): Cu-29.
Published: 01 October 2000
... CMW 100 is a copper alloy that combines high tensile strength with high electrical and thermal conductivity. It responds to age-hardening heat treatment. It is used for flash welding dies, springs, electrical components, high-strength backing material for brazed assemblies, and wire guides. This...
Journal Articles
Alloy Digest (2002) 51 (8): Cu-687.
Published: 01 August 2002
... CN8) (Hardenable Copper Alloy) Swissmetal alloy SM275H is a hardenable Cu-Ni-Sn alloy with good workability and corrosion resistance. It is often used in the automotive industry for springs, contacts, and clips. Swissmetal is a registered trademark of The Swissmetal Group. Table 1 Mechanical...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-660.
Published: 01 March 2001
... Equivalents: UNS C70250 Olin Brass 7025 No DIN or EN equivalent standards General Characteristics: Wieland-K55 is a high-reliability copper containing small per- centages of nickel and silicon. Mill hardened K55 strip exhibits high strength and good isotropic bend formability. At high cur- rents and high...
Journal Articles
Alloy Digest (2017) 66 (12): Cu-867.
Published: 01 December 2017
... Alloy C688 is a high-performance copper alloy with very high conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming and joining...
Journal Articles
Alloy Digest (2000) 49 (7): Cu-650.
Published: 01 July 2000
... Brushform 290 is a high-strength beryllium-copper alloy used in electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1994) 43 (12): Ni-473.
Published: 01 December 1994
...: Nickel Alloy Ni-473 DECEMBER 1994 DATA ON WORLD WIDE METALS AND ALLOYS Phtshdby: Alg Di@W. Inc IZQ1677-6161 NICORROS = AL 27 Canliild SImeI. Or;moe. NJ. 07050 I U.S.A. (Age-hardenable nlokel-copper alloy) NICORROS AL is age-hardenable by virtue of the alloying additions of aluminum and titanium. The...
Journal Articles
Alloy Digest (2010) 59 (2): Al-428.
Published: 01 February 2010
... The 7xxx series alloys contain zinc as the main alloying element, usually in combination with magnesium and copper. Alcoa’s high-strength 7055 alloy is supplied as plate and extrusions and used for compressive strength applications. This datasheet provides information on composition, tensile...
Journal Articles
Alloy Digest (1994) 43 (11): Ni-471.
Published: 01 November 1994
... 1000 B+C 1000 INCONEL alloy 7 18SPF A+C 1000 A+C 1000 A = 1750°F (954 C)/2 h/Muffle Cool in Ar B = 1950°F (1066oc)no min/MuffIe Cool in Ar C = 1325 F (718oc)ls h/K: at loooF (56q/h to 1150°F (621oc)/8 h/AC 316 95n9 655/331 316 loorz0 689/l 38 316 1 lot22 7581152 316 1 lOR2 7581152 316 14OR8 %5/l 93 316...