Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (6): Cu-256.
Published: 01 June 1972
... COPPER ALLOY No. 226 is a brass containing nominally 87.5% copper. It is used in decorative applications because of its color. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (12): Cu-427.
Published: 01 December 1981
... ANACONDA Alloy 226 nominally contains 87.5% copper and remainder zinc. This composition gives it a pleasing, rich color, hence the old name Jewelry Bronze. It possesses a resistance to dezincification and to stress-corrosion cracking that makes it ideal for all-weather usage as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (2): Cu-226.
Published: 01 February 1971
... properties hardness heat treatability heatsinks joinability lead frames machinability physical properties shear strength switchgears tensile properties waveguides workability Filing Code: Cu-226 CDA COPPER 109 Copper FEBRUARY 1971 - DATA ON WORLD WIDE METALS AND ALLOYS PUbfiJhf by Engineering...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
... COPPER ALLOY NO. C11100 is commonly called anneal-resistant electrolytic copper. It offers resistance to softening at slightly elevated temperatures by the addition of cadmium, which raises the temperature at which recovery and recrystallization occur. Its fabricating characteristics are the same...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (1): Cu-903.
Published: 01 January 2020
... Olin Brass Alloy C10200 is an oxygen-free, high-conductivity copper. It is ideal for applications where extremely high electrical conductivity and resistance to hydrogen embrittlement are vital. Where glass-to-metal seals are required this material also provides the added advantage of developing...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (8): Cu-461.
Published: 01 August 1983
... Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity electrical conductor hardness heat treatability joinability machinability MUELLER COPPER 1100 oxygen content physical properties tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (10): Cu-259.
Published: 01 October 1972
... as creep and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-259. Producer or source: Copper and copper alloy mills. Producer or Source: Copper and copper alloy mills Copyright © ASM International® 1996 1996...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (2): Cu-765.
Published: 01 February 2009
... Luvata C422 is a copper alloy with good spring properties and good electrical and thermal conductivity used in electrical contacts. It is often called Ambronze 422. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (4): Cu-370.
Published: 01 April 1979
... on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Cu-370. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (2): Cu-521.
Published: 01 February 1987
... treating, machining, joining, and surface treatment. Filing Code: Cu-521. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries Copyright © ASM International® 1996 1996 ASM International cast copper alloys castability chemical composition Copper alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... as casting, heat treating, machining, and joining. Filing Code: Al-226. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International cast aluminum alloys castability...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (12): Cu-834.
Published: 01 December 2014
... Ansonia alloy ACB C10100 and C10200 are two of the purest of the copper alloys commercially available and have their own unique properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (1): Cu-794.
Published: 01 January 2011
... alloys elasticity electronic applications hardness heat treatability joinability oxygen free copper physical properties tensile properties WIELAND-K11 workability thermal properties UNS C10100 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2011, ASM International®. All rights reserved...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (10): Cu-852.
Published: 01 October 2016
... heat treatability joinability machinability MUELLER ALLOY C10200 physical properties tensile properties workability thermal properties UNS C10200 Mueller Alloy C10200 has very high conductivity for applications such as bus bars. Chemical Composition, wt (Typical analysis) Copper 99.99 Oxygen...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (8): Cu-608.
Published: 01 August 1996
... alloys joinability physical properties tensile properties thermal conductivity thermal softening resistance workability UNS C15760 1 GLIDCOP@AL-60 1 DATA ON WORLD WlDE METALS AND ALLOYS Filing Code: 01-608 m Copper Alloy u , -m August 1999 GLIDCOP@ AL-60 (Dispersion-Strengthened Copper) GlidCop...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (5): SA-226.
Published: 01 May 1968
... joinability machinability mining equipment physical properties tensile properties weldability workability JLX-5occ Filing Code: SA-226 Steel-Alloy MAY 1968 - DATA ON WORLD WIDE METALS AND ALLOYS Pvblirbed by Engineering Alloys Digest. Ioc Upper Montclair, New Jersey J LX-50CC (High-Strength Low-Alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (5): Cu-199.
Published: 01 May 1969
... Code: Cu-199. Producer or source: Anaconda American Brass Company. Producer or Source: Anaconda American Brass Company Copyright © ASM International® 1996 1996 ASM International boron deoxidized copper 109 chemical composition corrosion-resistant alloys deformation properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (9): Cu-851.
Published: 01 September 2016
... (68 °F), W/m·K (Btu/(h·ft·°F)) 391 (226) Electrical resistivity, annealed, 20 °C (68 °F), m ( circular-mil/ft) 0.017 (10.3) Copyright © 2016, ASM International®. All rights reserved. MUELLER ALLOY C10100 (Oxygen-Free Electronic/High Copper) Filing Code: Cu-851 Copper :: September 2016 Materials Park...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (8): Cu-283.
Published: 01 August 1974
... COPPER ALLOY NO. 953 is an age-hardenable alloy offering high strength and hardness, good resistance to fatigue and wear, and excellent corrosion resistance. It can be used at temperatures up to 750 F. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (5): Cu-278.
Published: 01 May 1974
... strength as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-278. Producer or source: Copper and copper alloy mills. Producer or Source...