Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (4): SS-780.
Published: 01 April 2000
... Allegheny Ludlum AL 304DA is a composite of three plies consisting of carbon steel surrounded on both sides with type 304 stainless steel. This combination supplies corrosion resistance with good ductility for applications like cookware. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (4): Al-174.
Published: 01 April 1968
... rakes a pure white anodized finish. Colors are reproduced without darkening. This alloy does not respond to an age- hardening precipitation heat treatment. Forms Available: Ingots, sand castings, permanent mold castings, die castings. Applications: Dairy, agriculture, cookware, outdoor hardware...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (12): Fe-166.
Published: 01 December 2016
... 0.35 µm. Surface free from scratch, oxidation, or defects that might be detrimental to use. For thicknesses 0.4 mm (0.016 in 0.5 mm (0.020 in and 0.6 mm (0.024 in.) with ± 7% tolerance: strip widths and diameters on request. Applications: Phytherm 230 and Phytherm 260 are used in cookware for induction...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (9): Fe-165.
Published: 01 September 2016
... to +10 mm ( 0 to +0.4 in.) See also Table 3. Phytherm 120. For soft/hard temper, width: 10 640 mm (0.4 25.2 in length: 500 3500 mm (19.7 137.8 in.) Applications: Phytherm 55. Magnetic shunts (tachometers, watt hour meters) Phytherm 120. Cookware for induction heating Table 2 Mechanical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (4): SS-1346.
Published: 01 April 2022
... stainless steel in most mild environments; non-magnetic in the annealed condition but becomes magnetic when cold worked. Product Forms Plate, sheet, strip. Applications Air bag containers; cookware bodies/lids; hose clamps; piston rings; thermal window spacers; transit car roofing/siding; transit car...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (7): SS-1095.
Published: 01 July 2011
... ArcelorMittal K45 is a ferritic stainless steel with good resistance to pitting corrosion and oxidation to 950 deg C (1740 deg F), mostly used as a stable price, lower-cost substitute for nickel-containing austenitic stainless steels in a variety of applications. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (9): SS-997.
Published: 01 September 2007
.... Product Forms Available: The alloy is available in plate, sheet, and strip product forms. Applications: Applications involving formability include cookware bodies and lids, hose clamps, piston rings, and washing machine baskets. Applications requiring structural strength include transit car structural...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (7): SS-825.
Published: 01 July 2001
...: Allegheny Ludlum 201L is available in plate, sheet, and strip product and is listed in ASTM A 240 as type 201-2. Applications: Applications using the formability of the alloy include cookware bodies and lids, hose clamps, piston rings, and washing machine baskets. Applications using structural strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (3): SS-1332.
Published: 01 March 2021
... ATI 201 HP is a 200-series, Cr-Mn-Ni austenitic stainless steel. It is comparable to the Cr-Ni stainless steel types 301, 304, and 304L in many respects, and can even provide some advantages over the 18-8 grades in certain applications. Because it possess a very desirable combination of economy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (1): SS-266.
Published: 01 January 1972
... ALLEGHENY TYPE 211 is a copper-bearing, austenitic, chromium-nickel-manganese stainless steel with a low work-hardening rate. It is used for many deep-drawing applications, such as automotive trim, and broiler pans, mixing bowls, sinks, and door hardware. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (12): Cu-224.
Published: 01 December 1970
... produced from strip. Applications: Springs, relay parts. integrated circuit lead frames, headers and cans for glass sealed assemblies, high temperature terminals and connectors, Teflon coated cookware. Manufacturer: Olin Brass East Alton. Illinois 62024 ...