Journal Articles
Alloy Digest (1979) 28 (7): Co-23.
Published: 01 July 1979
... of media. Its many uses include scrapper blades, screw conveyor flights and sleeves for seawater pump shafts. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on high...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... applications are cutting knives and blades for many materials, apple-paring knives in canneries and wear strips in conveyor channels. This datasheet provides information on composition, physical properties, elasticity, and compressive strength. It also includes information on wear resistance as well as forming...
Journal Articles
Alloy Digest (1986) 35 (8): SS-473.
Published: 01 August 1986
... INCOLOY Alloy DS is a wrought, austenitic nickel-chromium-iron alloy with high resistance to heat and oxidation. Its many applications include furnace parts, woven-wire conveyor belts for continuous furnaces, radiant heat tubes and gas-turbine components. This datasheet provides information...
Journal Articles
Alloy Digest (1968) 17 (2): CI-35.
Published: 01 February 1968
... PROMAL is a specially processed pearlitic malleable iron recommended for highly stressed applications. It has high strength and good toughness suitable for gears, power shovels, conveyor chains and diesel engine drive pulleys. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1969) 18 (2): SS-221.
Published: 01 February 1969
... Type HH is an iron-chromium-nickel casting alloy having high heat, oxidation and corrosion resistance. It is recommended for furnace parts, salt pots, grate bars, belt conveyors and other parts operating up to 21008 F in intermittent service. It may be supplied in partially ferritic Type I...
Journal Articles
Alloy Digest (1969) 18 (7): Cu-203.
Published: 01 July 1969
... Waukesha Metal No. 3 is a high strength copper-nickel casting alloy having high corrosion resistance along with good ductility. It is recommended for conveyor chain links, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1965) 14 (3): Ni-99.
Published: 01 March 1965
... D-H No. 242 is a nickel-chromium high temperature alloy recommended for furnace components, heating elements and conveyor belts. It is also known as Nichrome V Def. #242. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1998) 47 (7): SS-723.
Published: 01 July 1998
... is conveyor belts in the food processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as heat treating. Filing Code: SS-723. Producer or source: Allegheny...
Journal Articles
Alloy Digest (1994) 43 (5): SA-475.
Published: 01 May 1994
... LUKENS HARDWARE 400F steel was developed from armor steel production technology to have as low a carbon equivalent as possible, consistent with meeting both surface and through-thickness hardness. Uses include truck body liners, bucket lips and conveyor troughs. This datasheet provides information...
Journal Articles
Alloy Digest (1994) 43 (6): SA-476.
Published: 01 June 1994
... LUKENS HARDWEAR 500F steel was developed from armor steel production technology to have as low a carbon equivalent as possible, consistent with meeting both surface and through-thickness hardness. Uses include truck body liners, bucket lips and conveyor troughs. This datasheet provides information...
Journal Articles
Alloy Digest (2010) 59 (2): SS-1052.
Published: 01 February 2010
... Kubota Alloy HI is a heat-resistant stainless steel casting suitable for long-term service at temperatures up to 1105 deg C (2025 deg F). Furnace skids and rail, conveyor roll assemblies, lead pots and retorts are typical applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2011) 60 (9): SA-634.
Published: 01 September 2011
... Dillidur 325L is a wear resistant steel with a surface hardness at room temperature of 325 HB for 10 mm plate thickness. The material is easy to bend, hot work and machine. Due to its increased wear resistance, it is used to produce excavators, conveyors, and materials handling systems as well...
Journal Articles
Alloy Digest (1996) 45 (8): SS-651.
Published: 01 August 1996
... Remainit 4318, similar to type 301LN, is in the family of lowest-alloyed austenitic stainless steels. This type has the highest rate of work hardening. Typical applications include the transportation industry and conveyor belts for food processing. This datasheet provides information...
Journal Articles
Alloy Digest (1964) 13 (10): SA-169.
Published: 01 October 1964
..., plates, and special sections. Applications: Railway truck wear plates, liners for chute and hoppers and conveyor cars, scoop trays and lips for ore bridge buckets, woven wire screen, perforat- ed plate and grizzly decks, screw conveyors and vibrating pan feeders for abrasive materials, magnetic separator...
Journal Articles
Alloy Digest (2003) 52 (4): CS-135.
Published: 01 April 2003
... in the construction industry; dumpers, slurry tubes, refuse vehi- cles, and screw conveyors in the transport industry; transport tubes for grains and seed in agriculture; and fans, pipes for min- eral dust, and conveyors in the mining industry. Producer: SSAB Swedish Steel, Inc. 4700 Grand Ave. Pittsburgh, PA 15225...
Journal Articles
Alloy Digest (1965) 14 (1): SS-13.
Published: 01 January 1965
... RECOMMENDED DESIGN STRESSES CONDITION A. Normal Static Loading-No Impact Slow Temperature Variation- CONDITION B. Impact Loads-Cyclic Heating-Thermal Shock. Conveyor Chains+uench Fixtures- Direct Stress Tension & Compression Pounds per sq. Inch Temperature Condition Temperature Condition OF A B OF A B 1200...
Journal Articles
Alloy Digest (1976) 25 (9): SA-324.
Published: 01 September 1976
... steel com- prise sideboards and guides on conveyors, flumes. chutes, hoppers, conveyor troughs; slope plates; dredge pipe; screens; mixer drums, equipment liner plates: metal baling machines; gravel crushers; coke quenching cars; wear strips on truck beds and on the bottoms of buckets and shovels; farm...
Journal Articles
Alloy Digest (1956) 5 (2): SS-40.
Published: 01 February 1956
... temperature variatmn for smtic loadiug. CycLic hearing and dmrmai shock for dynamic loading For bending saesses i=w besms, =) add 25% Shafn and conveyor rolls continuaUy rotating add 100% Shear mcmbas? pi- riv webs, Iugr, eu reduce by 25% Bearingstressmpinsandpiates reduce by 25% Designshouldbebasedon maximum...
Journal Articles
Alloy Digest (1956) 5 (6): SS-44.
Published: 01 June 1956
... between 1200 and 1600 deg F. loss of ductility resuks from changes within the alloy caused by precipitation of carbides. Forms Available: Centrifugally cast tubes and castings. Applications: Furnace Parts, normalizing discs, conveyor SQCWS, SProckers. salt pots, thermocouple protection tubes, hxtures...
Journal Articles
Alloy Digest (2019) 68 (9): SS-1309.
Published: 01 September 2019
..., the tempering effect will be lower. In continuous conveyor furnaces, where the holding time at temperature is very short (minimum 3 minutes), the temperature can be increased to about 425 °C (797 °F). In the as delivered condition, the ratio proof strength/ tensile strength is about 0.80. After tempering...