Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... BOFORS BP20-2 is a vacuum-degassed (BOVAC) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat...
Journal Articles
Alloy Digest (1987) 36 (9): CS-114.
Published: 01 September 1987
... SAE 1025 is a plain carbon steel for general-purpose construction and engineering. It is used in the hot-worked, cold-worked, normalized or water-quenched-and-tempered condition. It also is carburized and used for case-hardened parts. Its many uses include bolts, forgings, axles, machinery...
Journal Articles
Alloy Digest (1981) 30 (1): CS-85.
Published: 01 January 1981
... AISI 1043 is a carbon steel that provides medium strength and medium toughness at relatively low cost. It can be used in the hot-rolled, normalized, oil-quenched-and-tempered or water-quenched-tempered condition for general-purpose construction and engineering. Its manganese content is a little...
Journal Articles
Alloy Digest (1976) 25 (5): CS-59.
Published: 01 May 1976
... SAE 1044 is a medium-carbon steel suitable for use in the hot-rolled, normalized, oil-quenched-and-tempered, or water-quenched-and-tempered conditions. It provides medium strength and toughness at low cost and is a general-purpose construction and engineering steel. It is frequently used for flame...
Journal Articles
Alloy Digest (1979) 28 (4): SA-357.
Published: 01 April 1979
... condition (depending on section thickness and tempering temperature). Its uses include railway cars, bridge construction and carburized parts such as gears. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... of a fully killed, low-carbon, vacuum-degassed, columbium-alloyed steel. This special composition and processing practice minimize harmful nonmetallic inclusions that hamper formability. Typical applications include automotive reinforcements, truck parts and construction components. This datasheet provides...
Journal Articles
Alloy Digest (1980) 29 (3): CS-81.
Published: 01 March 1980
... SAE 1046 can be used in a variety of conditions: hot rolled, annealed, normalized, oil quenched and tempered, water quenched and tempered or austempered. It is a general-purpose construction and machinery steel. It furnishes medium strength and toughness at a low cost. It is frequently used...
Journal Articles
Alloy Digest (1981) 30 (6): CS-86.
Published: 01 June 1981
... AISI 1029 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. Its...
Journal Articles
Alloy Digest (1976) 25 (2): CS-58.
Published: 01 February 1976
... SAE 1016 is a low-carbon steel combining good machinability, good workability and good weldability. It is used for components case-hardened by carburizing. It is also used in the hot-rolled, annealed, normalized or cold-worked condition for a variety of construction and engineering applications...
Journal Articles
Alloy Digest (1976) 25 (6): CS-60.
Published: 01 June 1976
... SAE 1026 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. It has...
Journal Articles
Alloy Digest (1977) 26 (11): CS-69.
Published: 01 November 1977
... suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1971) 20 (10): CS-44.
Published: 01 October 1971
... conditions: hot rolled, normalized, oil quenched and tempered or water quenched and temper- ed. It is a general-purpose engineering and construction steel and provides medium strength and toughness at low cost. It is commonly used for flame- or induction-hardened parts. Composition: Carbon 0.43-0.50...
Journal Articles
Alloy Digest (1985) 34 (4): CS-104.
Published: 01 April 1985
... UNS No. G10460 is a general-purpose construction and machinery steel. It can be used in a variety of conditions: hot rolled, annealed, normalized, oil quenched and tempered, water quenched and tempered or austempered. It furnishes medium strength and toughness at a low cost. It is frequently used...
Journal Articles
Alloy Digest (1985) 34 (8): CS-108.
Published: 01 August 1985
... for a variety of construction and engineering applications. It has a relatively high manganese content (0.60-0.90%) for a low-carbon steel; this provides increased hardenability which is reflected in all uses and gives increased hardness and strength in the core of carburized parts and in uncarburized...
Journal Articles
Alloy Digest (1987) 36 (10): CS-115.
Published: 01 October 1987
... in fourconditions: hot rolled, normalized, oil quenched and tempered or water quenched and tempered. It is a general-purpose construction and engineering steel and provides medium strength and medium toughness at low cost. It is suitable for flame- or induction-hardened parts. Among its many uses are axles. shafts...
Journal Articles
Alloy Digest (1964) 13 (6): SS-157.
Published: 01 June 1964
... Uniloy 1409 TB is turbine quality 12% chromium stainless steel developed to meet the exacting demands of highly stressed parts where good strength and ductility along with corrosion resistance are required. It is recommended for applications in turbine construction. This datasheet provides...
Journal Articles
Alloy Digest (1988) 37 (11): CS-123.
Published: 01 November 1988
... UNS G10260 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. It has...
Journal Articles
Alloy Digest (1959) 8 (8): SA-88.
Published: 01 August 1959
... in oil or water. Temper at 250.300°F. Procedure No. 3 -Cool slowly in carburizing box or from the gas carburizer. Heat to 1475 F. and quench in oil or water. Temper at 250-300°F. &iRDEIUING WITHOUT CAREURZING: It may be used for certain constructional parts such as studs, bolts, pins, etc., that require...
Journal Articles
Alloy Digest (2010) 59 (2): SS-1054.
Published: 01 February 2010
... and calibers for plastics extrusion and constructional parts Producer: Bohler-Uddeholm North America Rolling Meadows, IL 60008 Tel: 800/652-2520 Tel: 847/577-8028 Fax: 905/813-8659 Web: www.bucorp.com In Austria: Bohler Edelstahl GmbH & Co KG A-8605 Kapfenberg, Austria Tel: +43-3862/20-7181 Fax: +43-3862/20...
Journal Articles
Alloy Digest (1970) 19 (2): SA-249.
Published: 01 February 1970
... constructional alloy steels. This enables weight reduction within the limits imposed by rigidity considerations for such applications as plate girders for bridges and buildings, parts of construction machinery. railroad cars, mobile equipment. etc. The notch toughness is considered to be satisfactory for general...