1-20 of 95 Search Results for

constructional castings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1961) 10 (6): Cu-102.
Published: 01 June 1961
... NI-VEE TYPE B is a precipitation hardening nickel bronze alloy suitable for constructional castings. This alloy provides the advantage of maximum strength in contact with steel or similar hard and strong coostruction material. It has improved machinability compared with Ni-Vee Type A (Alloy Digest...
Journal Articles
Alloy Digest (1958) 7 (8): Cu-66.
Published: 01 August 1958
... NI-VEE TYPE A is a precipitation hardening nickel bronze alloy suitable for constructional castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on casting, heat treating...
Journal Articles
Alloy Digest (1959) 8 (3): Cu-72.
Published: 01 March 1959
... NI-VEE TYPE C is a leaded precipitation hardening nickel bronze alloy suitable for constructional, pressure, and bearing metal castings. Its strength is superior to red brass; its mechanical properties are comparable to those of lead-free G-bronze. This datasheet provides information...
Journal Articles
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... BOFORS BP20-2 is a vacuum-degassed (BOVAC) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat...
Journal Articles
Alloy Digest (1987) 36 (9): CS-114.
Published: 01 September 1987
... SAE 1025 is a plain carbon steel for general-purpose construction and engineering. It is used in the hot-worked, cold-worked, normalized or water-quenched-and-tempered condition. It also is carburized and used for case-hardened parts. Its many uses include bolts, forgings, axles, machinery...
Journal Articles
Alloy Digest (2018) 67 (3): Cu-869.
Published: 01 March 2018
... standards) General Characteristics This alloy is a proved standard cast copper tin zinc alloy for any slide bearing used in machine construction and subjected to medium stress. It has excellent sliding and emergency running properties as well as high wear resistance. This alloy can also be used...
Journal Articles
Alloy Digest (1997) 46 (8): SA-486.
Published: 01 August 1997
... bodies, bucket components, and mining and construction equipment. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-486. Producer or source: Oregon Steel Mills. Producer or Source...
Journal Articles
Alloy Digest (1997) 46 (9): SA-487.
Published: 01 September 1997
... bodies, bucket components, and mining and construction equipment. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-487. Producer or source: Oregon Steel Mills. Producer or Source...
Journal Articles
Alloy Digest (1988) 37 (2): CS-119.
Published: 01 February 1988
... SAE 1015 is a low-carbon steel used in the annealed, cold-worked, hot-rolled or normalized condition for general purpose construction and engineering. It is also used for case-hardened components. It combines good machinability, good workability and good weldability. This datasheet provides...
Journal Articles
Alloy Digest (1963) 12 (6): SA-147.
Published: 01 June 1963
... to the elimi- nation of stress concentration areas, due to drastic changes in sections. Casting shape and complexity will determine limits of di- mensional tolerances. Pattern construction should allow ?4 inch shrinkage allowance, with an additional finish allowance of l/8 inch to % inch on surfaces which...
Journal Articles
Alloy Digest (1957) 6 (9): Al-56.
Published: 01 September 1957
... is used in the construction of the die casting die deper&ng on the type of casting being made. The approximate solidification range is 1065 to 1080°F. Machinability: The high silicon content of this alloy accounts for some problems in machining. Where high accuracy. and smoothness of the machined surface...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... isotropy, ductility and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2017) 66 (8): SA-795.
Published: 01 August 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (2017) 66 (9): SA-797.
Published: 01 September 2017
... Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting rods...
Journal Articles
Alloy Digest (1989) 38 (11): P-12.
Published: 01 November 1989
... molecular structure may be represented as follows: I-p : -C-O-H&- H-CIR*-CH,- H-CH,-G- i x - cc =CH, %O H H cl *R is derived from the epoxy component (epoxy novolac in the case of Derakane 470-36). PROPERTIES Table 1 -TYPICAL ROOM-TEMPERATURE PROPER- TIES OF l/8 CLEAR 470-36 and 47045 CASTINGS Tensile...
Journal Articles
Alloy Digest (2017) 66 (5): SA-785.
Published: 01 May 2017
... Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles Gear manufacture for rolls, gears, and pinions Engine construction for crankshafts, connecting rods...
Journal Articles
Alloy Digest (2017) 66 (7): SA-791.
Published: 01 July 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (2017) 66 (10): SA-802.
Published: 01 October 2017
... carbonitriding. Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...
Journal Articles
Alloy Digest (2017) 66 (11): SA-806.
Published: 01 November 2017
... carbonitriding Product Forms Available: Ingots and continuously cast products are formed to bars as required. Applications: Plastic processing for cylinders in pressing, pistons, worm gears, and injection nozzles; gear manufacture for rolls, gears, and pinions; engine construction for crankshafts, connecting...