Skip Nav Destination
Close Modal
Search Results for
construction industry
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 165
Search Results for construction industry
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
HOKOTOL: High-Strength Aluminum Alloy
Available to Purchase
Alloy Digest (2004) 53 (7): Al-391.
Published: 01 July 2004
... Originally developed as a high-strength alloy for the aircraft industry, this alloy was further developed and optimized to satisfy the most demanding applications of the mold construction industry. The resulting mold construction alloy, Hokotol, exhibits very high strength and wear resistance...
Abstract
View articletitled, HOKOTOL: High-Strength Aluminum Alloy
View
PDF
for article titled, HOKOTOL: High-Strength Aluminum Alloy
Originally developed as a high-strength alloy for the aircraft industry, this alloy was further developed and optimized to satisfy the most demanding applications of the mold construction industry. The resulting mold construction alloy, Hokotol, exhibits very high strength and wear resistance, as well as excellent uniformity of strength properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance. Filing Code: AL-391. Producer or source: Corus Aluminum Rolled Products USA.
Journal Articles
DOMEX WEAR: Wear-Resistant High-Strength Steel
Available to Purchase
Alloy Digest (2003) 52 (4): CS-135.
Published: 01 April 2003
... Domex Wear is a wear-resistant, very-high-strength steel that can be cold formed. It is used in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also...
Abstract
View articletitled, DOMEX WEAR: Wear-Resistant High-Strength Steel
View
PDF
for article titled, DOMEX WEAR: Wear-Resistant High-Strength Steel
Domex Wear is a wear-resistant, very-high-strength steel that can be cold formed. It is used in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on wear resistance as well as heat treating and joining. Filing Code: CS-135. Producer or source: SSAB Swedish Steel Inc.
Journal Articles
TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
Available to Purchase
Alloy Digest (2007) 56 (1): CS-148.
Published: 01 January 2007
... The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of a finished component or to reduce the thickness. The steel is used in the construction and the automotive industries. This datasheet provides information on composition...
Abstract
View articletitled, TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
View
PDF
for article titled, TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of a finished component or to reduce the thickness. The steel is used in the construction and the automotive industries. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CS-148. Producer or source: Hille & Mueller, USA Inc. See also Alloy Digest CS-173, November 2012.
Journal Articles
DOMEX 100XF: Very High Strength Cold Forming Steel
Available to Purchase
Alloy Digest (2003) 52 (10): SA-523.
Published: 01 October 2003
... Domex 100XF is a very-high-strength steel that can be cold formed. It finds use in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes...
Abstract
View articletitled, DOMEX 100XF: Very High Strength Cold Forming Steel
View
PDF
for article titled, DOMEX 100XF: Very High Strength Cold Forming Steel
Domex 100XF is a very-high-strength steel that can be cold formed. It finds use in the construction and mining industries. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on heat treating and joining. Filing Code: SA-523. Producer or source: SSAB Swedish Steel Inc.
Journal Articles
ARMCO GAINEX STEELS: Hot Rolled Carbon Steels
Available to Purchase
Alloy Digest (1977) 26 (11): CS-69.
Published: 01 November 1977
... suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, ARMCO GAINEX STEELS: Hot Rolled Carbon Steels
View
PDF
for article titled, ARMCO GAINEX STEELS: Hot Rolled Carbon Steels
ARMCO GAINEX Steels comprise a family of five low-cost structural carbon steels. This family includes: GAINEX-35, GAINEX-40, GAINEX-45, GAINEX-50 and GAINEX SA (Strain ageable); the numbers following GAINEX refer to minimum specified (ordered) yield strengths in 1000 psi. These steels are well suited to the automotive, farm and construction equipment, and appliance industries for such applications as truck bodies, light poles, bumper support members and parts for agricultural implements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-69. Producer or source: Armco Inc., Eastern Steel Division.
Journal Articles
ZYMAXX: Chemical and Creep Resistant Parts
Available to Purchase
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... chemical processing, including aerospace and automotive applications, general industrial equipment, home appliances, farm and construction equipment. *ZYMAXX is a trademark of DuPont for chemical and creep resistant parts. Chemical Characterization: ZYMAXX is comprised of resins made from fluorocarbons...
Abstract
View articletitled, ZYMAXX: Chemical and Creep Resistant Parts
View
PDF
for article titled, ZYMAXX: Chemical and Creep Resistant Parts
ZYMAXX provides outstanding compressive creep resistance, toughness and chemical inertness at high temperatures and pressures and under adverse conditions. They have a wide range of uses beyond chemical processing, including aerospace and automotive applications, general industrial equipment, home appliances, farm and construction equipment. This datasheet provides information on physical properties, hardness, tensile properties, and compressive strength as well as fracture toughness and creep. It also includes information on corrosion resistance. Filing Code: Cp-18. Producer or source: E. I. Dupont de Nemours & Company Inc..
Journal Articles
TENFORM XF350: Hot-Rolled High-Strength Low-Alloy Steel
Available to Purchase
Alloy Digest (2006) 55 (12): CS-147.
Published: 01 December 2006
... The high strength of Tenform XF350, a hot-rolled high-strength low-alloy (HSLA) steel, allows the user to increase the strength of the finished component or to reduce the thickness. The material finds use in the construction and the automotive industries. This datasheet provides information...
Abstract
View articletitled, TENFORM XF350: Hot-Rolled High-Strength Low-Alloy Steel
View
PDF
for article titled, TENFORM XF350: Hot-Rolled High-Strength Low-Alloy Steel
The high strength of Tenform XF350, a hot-rolled high-strength low-alloy (HSLA) steel, allows the user to increase the strength of the finished component or to reduce the thickness. The material finds use in the construction and the automotive industries. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue. It also includes information on forming. Filing Code: CS-147. Producer or source: Hille & Mueller, USA Inc.
Journal Articles
BÖHLER L312 VMR: Nickel Alloy
Available to Purchase
Alloy Digest (2012) 61 (6): Ni-697.
Published: 01 June 2012
... Böhler (or Boehler) L312 VMR is a nickel base alloy with good resistance to stress-corrosion cracking. The alloy is used in the construction of industrial furnaces. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture...
Abstract
View articletitled, BÖHLER L312 VMR: Nickel Alloy
View
PDF
for article titled, BÖHLER L312 VMR: Nickel Alloy
Böhler (or Boehler) L312 VMR is a nickel base alloy with good resistance to stress-corrosion cracking. The alloy is used in the construction of industrial furnaces. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Ni-697. Producer or source: Böhler-Uddeholm Corporation.
Journal Articles
BÖHLER L329 VMR: Nickel Alloy
Available to Purchase
Alloy Digest (2012) 61 (8): Ni-699.
Published: 01 August 2012
... Böhler (or Boehler) L329 VMR is a nickel base alloy with good resistance to stress-corrosion cracking. The alloy is used in the construction of industrial furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Abstract
View articletitled, BÖHLER L329 VMR: Nickel Alloy
View
PDF
for article titled, BÖHLER L329 VMR: Nickel Alloy
Böhler (or Boehler) L329 VMR is a nickel base alloy with good resistance to stress-corrosion cracking. The alloy is used in the construction of industrial furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Ni-699. Producer or source: Böhler-Uddeholm North America.
Journal Articles
TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
Available to Purchase
Alloy Digest (2012) 61 (11): CS-173.
Published: 01 November 2012
... The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of the finished component or to reduce the thickness. Construction and the automotive industries offer uses. This datasheet provides information on composition, physical...
Abstract
View articletitled, TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
View
PDF
for article titled, TENFORM XF450: Hot-Rolled High-Strength Low-Alloy Steel
The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of the finished component or to reduce the thickness. Construction and the automotive industries offer uses. This datasheet provides information on composition, physical properties, and bend strength as well as fatigue. It also includes information on forming and joining. Filing Code: CS-173. Producer or source: Hille & Mueller, USA Inc.. See also Alloy Digest CS-148, January 2007.
Journal Articles
WIELAND-K42: Low Alloy Copper
Available to Purchase
Alloy Digest (2015) 64 (5): Cu-837.
Published: 01 May 2015
... industry and construction industry. Producer: Wieland Metals, Inc. Wheeling, IL 60090, USA Tel: (847) 537-3990 Fax: (847) 537-4085 www.wielandmetals.com In Germany: Wieland-Werke AG D-89070 Ulm, Germany Tel: +49-0731-944-0 Fax: +49-0731-944-2772 www.wieland.de ISSN: 002-614X Cu-837B Table 1 Mechanical...
Abstract
View articletitled, WIELAND-K42: Low Alloy Copper
View
PDF
for article titled, WIELAND-K42: Low Alloy Copper
Wieland-K42 is a copper alloy with a small amount of zinc for strength without removing its good copper physical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-837. Producer or source: Wieland Metals Inc..
Journal Articles
FORA 360: Wear Resistant Steel
Available to Purchase
Alloy Digest (2015) 64 (3): SA-720.
Published: 01 March 2015
... resistance is from two to three times longer than S355 grade. Moreover, Fora 360 is very easily welded and has good forming properties, thereby contributing to ease of fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel...
Abstract
View articletitled, FORA 360: Wear Resistant Steel
View
PDF
for article titled, FORA 360: Wear Resistant Steel
Fora 360 is wear resistant steel. It is martensitic with a minimum HB hardness of 360. This datasheet provides information on composition, hardness, tensile properties, and bend strength. It also includes information on wear resistance as well as forming, machining, and joining. Filing Code: SA-720. Producer or source: Industeel Belgium.
Journal Articles
FORA 400: Wear Resistant Steel
Available to Purchase
Alloy Digest (2011) 60 (3): SA-622.
Published: 01 March 2011
... is very easily welded and has good forming properties thereby contributing to ease of fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel industry, etc. Product Availability: Plate from 4 mm (3/16 in.) to 60 105 mm (2.4...
Abstract
View articletitled, FORA 400: Wear Resistant Steel
View
PDF
for article titled, FORA 400: Wear Resistant Steel
Fora 400 is a wear resistant, martensitic steel, with a minimum HB hardness of 400. This datasheet provides information on composition, hardness, tensile properties, and bend strength as well as fracture toughness. It also includes information on wear resistance as well as forming, machining, and joining. Filing Code: SA-622. Producer or source: Industeel Belgium.
Journal Articles
ARCELORMITTAL K03: Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2009) 58 (8): SS-1042.
Published: 01 August 2009
... and hot rolled, according to thickness Applications Applications are the classic construction, transport equipment, and industrial equipment arenas where a better performance is needed when moderately corrosive environments exist. Producer: Arcelor Stainless Processing LLC Sterling Heights, MI 48312...
Abstract
View articletitled, ARCELORMITTAL K03: Ferritic Stainless Steel
View
PDF
for article titled, ARCELORMITTAL K03: Ferritic Stainless Steel
ArcelorMittal K03 is a ferritic stainless steel, mostly used as a stable price, lower-cost substitute for nickel-containing austenitic stainless steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1042. Producer or source: Arcelor Stainless Processing LLC.
Journal Articles
AVESTAPOLARIT LDX 2101: Lean Duplex Stainless Steel
Available to Purchase
Alloy Digest (2002) 51 (10): SS-863.
Published: 01 October 2002
... in rapid reformation of austenite in weld thermal cycles. Duplex steels have mainly been used because of their good cor- rosion resistance with high strength. Several important applica- tions exist in the process industry. For construction purposes, the focus is more on mechanical properties combined...
Abstract
View articletitled, AVESTAPOLARIT LDX 2101: Lean Duplex Stainless Steel
View
PDF
for article titled, AVESTAPOLARIT LDX 2101: Lean Duplex Stainless Steel
AvestaPolarit LDX 2101 is a lean duplex steel for construction purpose. The alloy has low nickel content, but is balanced with manganese and nitrogen. Applications include exposed load-carrying structural materials for bridges as well as rebar for many construction uses. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: SS-863. Producer or source: AvestaPolarit AB.
Journal Articles
DIWETEN 460: Atmospheric Structural Steel
Available to Purchase
Alloy Digest (2015) 64 (4): SA-724.
Published: 01 April 2015
.... Generally, the corrosion velocity decreases with increasing service life, even after the formation of the patina. However, the patina offers in comparison to unalloyed steels a better protection against atmospheric corrosion in industrial, city, or rural atmosphere, which enables the application of uncoated...
Abstract
View articletitled, DIWETEN 460: Atmospheric Structural Steel
View
PDF
for article titled, DIWETEN 460: Atmospheric Structural Steel
Diweten 460 is a fine-grained structural steel with improved atmospheric corrosion resistance. The alloy is thermomechanically rolled. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-724. Producer or source: Dillinger Hütte GTS.
Journal Articles
DIWETEN 235: Atmospheric Structural Steel
Available to Purchase
Alloy Digest (2015) 64 (2): SA-718.
Published: 01 February 2015
... (0.08 in.) striker in accordance with EN ISO 148-1. Unless otherwise agreed, the test results are documented in a certificate 3.1 in accordance with EN 10204. Applications: This alloy is used in field steel constructions such as bridges, steel towers and masts, buildings, industrial chimneys, silos...
Abstract
View articletitled, DIWETEN 235: Atmospheric Structural Steel
View
PDF
for article titled, DIWETEN 235: Atmospheric Structural Steel
Diweten 235 (minimum yield strength of 235 MPa, or 34 ksi, in thicknesses up to 16 mm, or 0.6 in.) is a structural steel with improved atmospheric corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-718. Producer or source: Dillinger Hütte GTS.
Journal Articles
DIWETEN 355: Atmospheric Structural Steel
Available to Purchase
Alloy Digest (2015) 64 (3): SA-721.
Published: 01 March 2015
...: This alloy is used for in the field steel constructions like bridges, steel towers and masts, buildings, industrial chimneys, silos, and monuments. Producer: Dillinger Hütte GTS D-66763 Dillingen/Saar Germany Tel: +49 6831 47 0 Fax: +49 6831 47 2212 httpwww.dillinger.de ISSN: 002-614X SA-721B ...
Abstract
View articletitled, DIWETEN 355: Atmospheric Structural Steel
View
PDF
for article titled, DIWETEN 355: Atmospheric Structural Steel
Diweten 355 (minimum yield strength of 355 MPa, or 51 ksi, in thicknesses up to 16 mm, or 0.6 in.) is a structural steel with improved atmospheric corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-721. Producer or source: Dillinger Hütte GTS.
Journal Articles
REMANIT 4401: Austenitic Stainless Steel
Available to Purchase
Alloy Digest (1996) 45 (12): SS-664.
Published: 01 December 1996
... resistance to nonoxidizing acids and to pitting corrosion. Architects make use of it for external cladding. Remanit 4401 is approved for use as wall ties in the building industry. This steel has a wide field of application in the construction of apparatus for textile finishing. in the chemi- cal industry...
Abstract
View articletitled, REMANIT 4401: Austenitic Stainless Steel
View
PDF
for article titled, REMANIT 4401: Austenitic Stainless Steel
Remanit 4401 is a chromium-nickel-molybdenum austenitic stainless steel. The molybdenum (2 to 2.5%) gives it resistance to pitting corrosion, more than most of the standard grades of austenitic stainless steels. This extra measure of corrosion resistance makes this grade particularly suitable for uses involving severe corrosive conditions. The alloy has high strength and good resistance to creep at elevated temperatures. Its many applications include the nuclear, chemical, food, paper, and textile industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SS-664. Producer or source: Thyssen Stahl AG.
Journal Articles
ARMCO HIGH STRENGTH No. 5: High Strength Low Alloy Steel
Available to Purchase
Alloy Digest (1964) 13 (9): SA-168.
Published: 01 September 1964
... car frames, truck bodies and related vehicles requiring high strength but only moderate corrosion resistance are examples of practical applications for this material. Other uses include construction and industrial equipment. In plate form, this grade normally conforms to the same tensile properties...
Abstract
View articletitled, ARMCO HIGH STRENGTH No. 5: High Strength Low Alloy Steel
View
PDF
for article titled, ARMCO HIGH STRENGTH No. 5: High Strength Low Alloy Steel
Armco High Strength No. 5 is a low-alloy high-strength steel recommended for structural applications requiring high strength but only moderate corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-168. Producer or source: Armco Inc., Eastern Steel Division.