Alloy Digest (1976) 25 (6): CS-60.
Published: 01 June 1976
... SAE 1026 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. It has...
Journal Articles
Alloy Digest (1981) 30 (6): CS-86.
Published: 01 June 1981
... AISI 1029 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. Its...
Journal Articles
Alloy Digest (1982) 31 (7): SA-385.
Published: 01 July 1982
... with quenched-and-tempered steel plate. BethStar 80 plate can be machined, formed and welded readily. It is used in several constructional applications and has the potential for many more applications. This datasheet provides information on composition, physical properties, microstructure, elasticity...
Journal Articles
Alloy Digest (1988) 37 (11): CS-123.
Published: 01 November 1988
... UNS G10260 is a low-to-medium-carbon steel used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for a variety of engineering and construction applications. It combines good workability (hot or cold), good machinability and good weldability. It has...
Journal Articles
Alloy Digest (1970) 19 (2): SA-249.
Published: 01 February 1970
... USS CON-PAC is a quenched and tempered carbon steel for constructional applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and bend strength as well as fracture toughness. It also includes information on corrosion...
Journal Articles
Alloy Digest (2013) 62 (12): CS-176.
Published: 01 December 2013
... AlgoTuf 400F is designed for superior wear resistance and is one in a full range of heat-treated plate products for construction, mining, manufacturing, and military applications. This alloy is more formable with less preheat than the other abrasion-resistant heat-treated steel plates...
Journal Articles
Alloy Digest (2004) 53 (4): CS-142.
Published: 01 April 2004
... Algoma 100 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for construction, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (2004) 53 (2): CS-140.
Published: 01 February 2004
... AlgoTuf 440F is designed for wear resistance and is one in a full range of heat-treated plate products by Algoma Steel for construction, mining, manufacturing, and military applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1979) 28 (3): SA-356.
Published: 01 March 1979
... of a fully killed, low-carbon, vacuum-degassed, columbium-alloyed steel. This special composition and processing practice minimize harmful nonmetallic inclusions that hamper formability. Typical applications include automotive, construction and farm-equipment components. This datasheet provides information...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... isotropy, ductility and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2004) 53 (7): Al-391.
Published: 01 July 2004
... Originally developed as a high-strength alloy for the aircraft industry, this alloy was further developed and optimized to satisfy the most demanding applications of the mold construction industry. The resulting mold construction alloy, Hokotol, exhibits very high strength and wear resistance...
Journal Articles
Alloy Digest (2002) 51 (10): SS-863.
Published: 01 October 2002
... AvestaPolarit LDX 2101 is a lean duplex steel for construction purpose. The alloy has low nickel content, but is balanced with manganese and nitrogen. Applications include exposed load-carrying structural materials for bridges as well as rebar for many construction uses. This datasheet provides...
Journal Articles
Alloy Digest (2018) 67 (2): SS-1278.
Published: 01 February 2018
... strength with a good formability result on a very high lightweight construction potential. This lightweight potential, as well as its excellent CO2 footprint, make the grade ideal for a wide range of transportation (e.g., truck, bus, railway vehicles) but mainly automotive applications as an alternative...
Journal Articles
Alloy Digest (2011) 60 (3): SA-621.
Published: 01 March 2011
...: Dillinger Hütte GTS. Producer or Source: Dillinger Hütte GTS Copyright © ASM International® 2011 2011 ASM International chemical composition construction applications DILLINAL 460/630 fracture toughness heat treatability physical properties tensile properties workability DATA...
Journal Articles
Alloy Digest (1976) 25 (2): CS-58.
Published: 01 February 1976
... SAE 1016 is a low-carbon steel combining good machinability, good workability and good weldability. It is used for components case-hardened by carburizing. It is also used in the hot-rolled, annealed, normalized or cold-worked condition for a variety of construction and engineering applications...
Journal Articles
Alloy Digest (1985) 34 (8): CS-108.
Published: 01 August 1985
... for a variety of construction and engineering applications. It has a relatively high manganese content (0.60-0.90%) for a low-carbon steel; this provides increased hardenability which is reflected in all uses and gives increased hardness and strength in the core of carburized parts and in uncarburized...
Journal Articles
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... (BOVAC*) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat treated for a number of applications...
Journal Articles
Alloy Digest (2004) 53 (1): CS-139.
Published: 01 January 2004
... AlgoTuf 450F is one of a full range of heat-treated plate products for construction, mining, manufacturing and military applications. This datasheet provides information on composition as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code...
Journal Articles
Alloy Digest (2005) 54 (2): SA-546.
Published: 01 February 2005
... Docol 450 Wear is an ultra-high strength steel that is used for many wear application in transportation and construction products. This datasheet provides information on composition, physical properties, microstructure, hardness, tensile properties, and bend strength. It also includes information...