1-20 of 742 Search Results for

consistent properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2009) 58 (10): SS-1045.
Published: 01 October 2009
... Aminox AS-1 is an austenitic stainless steel with a very controlled composition to have consistent properties and machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2007) 56 (3): Ni-647.
Published: 01 March 2007
... Allvac 718Plus alloy is a variant of alloy 718 (Alloy Digest Ni-90, April 1964) made by adding new elements and adjusting others. The triple melting produces a stronger alloy with consistent properties in strength, stability, and forgeability. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1974) 23 (4): Ni-203.
Published: 01 April 1974
... on careful control of production processes to achieve high and consistent properties. Its primary usage is in gas turbine compressor and turbine components. This datasheet provides information on composition, physical properties, microstructure, and elasticity as well as fracture toughness, creep...
Journal Articles
Alloy Digest (2003) 52 (10): SA-523.
Published: 01 October 2003
...-based material, which results in a clean product with minimal inclusions. These consistent properties begin taking shape in the molten state where the chemical composition in carbon, manganese, and sulfur are adjusted to provide the desired yield strength. Further strength improvements are achieved...
Journal Articles
Alloy Digest (2013) 62 (6): Ti-150.
Published: 01 June 2013
... are used when higher toughness is desired. The second solution treatment is done at 800 ºC (1475 ºF) followed by a water quench. Fan air-cooling may be used for thinner sections; however, higher and more consistent properties may be obtained by water quenching. Beta processed material receives a single...
Journal Articles
Alloy Digest (2004) 53 (11): Ti-135.
Published: 01 November 2004
... toughness is desired. The second solution treatment is done at 800 °C (1475 °F) followed by a water quench. Fan air cooling may be used for thinner sec- tion but higher and more consistent properties may be obtained by water quenching. Beta processed material receives a single solution anneal at 800 °C...
Journal Articles
Alloy Digest (2012) 61 (1): Ti-149.
Published: 01 January 2012
... followed by rapid air cooling. The higher temperatures are used when higher toughness is desired. The second solution treatment is done at 800 ºC (1475 ºF) followed by a water quench. Fan air-cooing may be used for thinner sections; however, higher and more consistent properties may be obtained by water...
Journal Articles
Alloy Digest (1967) 16 (7): Ni-125.
Published: 01 July 1967
..., care must be taken to ensure that the entire coil reaches a uniform temperature for consistent properties throughout. Batch treatments are optimized by rapid heat up times and minimum temperature gradients in the material. SG-100 should be treated under sulphur free furnace atmospheres since sulphur...
Journal Articles
Alloy Digest (2023) 72 (8): Ti-195.
Published: 01 August 2023
.... The second solution treatment is done at 800 °C (1475 °F) followed by a water quench. Fan air-cooling may be used for thinner sections; however, higher and more consistent properties may be obtained by water quenching. Beta processed material receives a single solution anneal at 800 °C (1475 °F) for 4 h...
Journal Articles
Alloy Digest (2010) 59 (4): TS-689.
Published: 01 April 2010
..., milling, and grinding. General Characteristics: Uddeholm Nimax is characterized by: Excellent machinability Very good welding properties Good polishing and texturing properties Good resistance against indentations High impact and fracture toughness Consistent properties through large sections...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... value. Algoma 130 is produced with a certified notch toughness average level (CVNT) of 27 J at 40 °C (20 ft lbf at 40 °F). Notch toughness testing is conducted and reported on a per thickness per heat basis. Workability: Forming. Low alloy levels and consistent properties make Algoma 130 ideal...
Journal Articles
Alloy Digest (1986) 35 (10): Cu-516.
Published: 01 October 1986
... BRUSH PHOSPHOR BRONZE is precision rolled and thermally treated to produce a material with consistent formability and properties. The product offers design advantages, improved service life and reduced fabrication problems. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2005) 54 (11): Ti-137.
Published: 01 November 2005
... Allvac Titanium 6Al-4V ELI is an alloy with extra-low interstitials to produce cleanliness and consistency in properties. It is used in surgical instruments and implants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1973) 22 (3): Ni-188.
Published: 01 March 1973
... BLENDALLOY 25-5000 is a nickel-iron alloy with a rectangular hysteresis loop and low coercive force. It is a powder metallurgy product and this helps to provide it with uniform and consistent magnetic properties, exceptional purity and cleanliness, precise chemcial composition and guaranteed...
Journal Articles
Alloy Digest (1973) 22 (9): Cu-270.
Published: 01 September 1973
... GLIDCOP is a powder-metallurgy product consisting of high-purity copper with submicroscopic particles of insoluble aluminum oxide finely dispersed throughout the copper matrix. It is particularly suited for applications that require a combination of high strength and high conductivity...
Journal Articles
Alloy Digest (2021) 70 (8): Co-139.
Published: 01 August 2021
.... This alloy consists of a CoCrMo alloy matrix containing dispersed hard carbides that strengthen the alloy and increase its hardness, but that also decrease its ductility. The type, shape, size, and distribution of the carbides are strongly influenced by the processing history of the alloy...
Journal Articles
Alloy Digest (1956) 5 (11): CI-17.
Published: 01 November 1956
... BISBO is a pearlitic malleable iron readily cast in thick sections with consistently high mechanical properties. It has high yield strength, excellent wear resistance, and adaptability to selective hardening. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1994) 43 (12): SA-481.
Published: 01 December 1994
... NAK 55 is a very clean steel for use in plastic and rubber molds were impact resistance is not critical in design. Its age-hardening gives very high strength and good wear resistance. Tight tolerance are obtained with consistent expansion and contraction properties. This datasheet provides...
Journal Articles
Alloy Digest (1994) 43 (1): SS-561.
Published: 01 January 1994
... CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY offers much of the properties of 430 stainless steel, but through composition and processing maintains consistently high magnetic permeability and low residual induction. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1985) 34 (8): SS-462.
Published: 01 August 1985
... ALLEGHENY LUDLUM AL 2205 ALLOY is in the family of duplex alloys in which added nitrogen significantly improves corrosion resistance, especially in the welded condition. The microstructure consists of a balanced mixture of austenitic and ferritic phases. Its corrosion resistance to many...