Alloy Digest (1979) 28 (5): SS-364.
Published: 01 May 1979
... SEA-CURE is a ferritic stainless steel designed to provide high resistance to pitting and crevice corrosion in condensers cooled by saline or brackish water. It is used for condenser tubes and has great potential for many other uses. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1969) 18 (8): Cu-204.
Published: 01 August 1969
... Revere No. 464 is a copper-zinc alloy having good strength, toughness, and resistance to corrosion. It is recommended for steam condensers, marine equipment and oil refinery equipment, most especially in the form of sheet and plate, the latter as the heads for condensers and similar heat...
Journal Articles
Alloy Digest (1982) 31 (12): Cu-449.
Published: 01 December 1982
... Copper Alloy No. C72200 was developed to improve on the performance of the copper-nickel condenser tube alloys. It is essentially 85-15 copper-nickel with additions of 0.8% iron, 0.5% chromium and 0.5% manganese. It has exceptionally high resistance to erosion and corrosion by flowing seawater...
Journal Articles
Alloy Digest (1978) 27 (4): SS-349.
Published: 01 April 1978
... for condenser tubing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-349. Producer or source...
Journal Articles
Alloy Digest (1974) 23 (9): Cu-284.
Published: 01 September 1974
... Copper No. 142 is an arsenical copper deoxidized with phosphorus. Its capacity is excellent for hot forming or cold working and it has excellent joinability characteristics for soldering, brazing and gas-shielded arc welding. Its leading use is tubing for condensers and heat exchangers...
Journal Articles
Alloy Digest (1976) 25 (6): Cu-313.
Published: 01 June 1976
... Copper Alloy No. 687 is a copper-zinc-aluminum alloy with high resistance to corrosion and erosion; in addition, it has good strength and ductility and can be cold worked and cold formed readily. It is chiefly used in the form of tubes for various types of equipment such as condensers and heat...
Journal Articles
Alloy Digest (2006) 55 (1): Cu-739.
Published: 01 January 2006
... Brush Wellman Q-Max tube is a high-strength age-hardening copper alloy with excellent biological resistance for use in waters as condenser tubing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1994) 43 (11): Cu-599.
Published: 01 November 1994
... addition of inhibitor is made to minimize the alloy’s susceptibility to dezincification and stress corrosion. They are used for condenser, evaporator and heat-exchanger tubes and associated applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1956) 5 (1): Cu-34.
Published: 01 January 1956
... ADMIRALTY METAL is a corrosion resistant brass alloy recommended especially for condenser tubing. It is better known as Inhibited Admiralty. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also...
Journal Articles
Alloy Digest (1981) 30 (3): Cu-414.
Published: 01 March 1981
... stems and condenser plates. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (1981) 30 (6): Cu-418.
Published: 01 June 1981
... its many uses are architectural applications, trim, hot forgings, condenser plates and heat exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1959) 8 (7): Cu-77.
Published: 01 July 1959
... CUPRO NICKEL, 10%-755 is a highly ductile, malleable and corrosion resisting alloy, suitable for condenser tubes and many other engineering applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1959) 8 (9): Cu-81.
Published: 01 September 1959
... Revere No. 508 is a highly ductile, malleable and corrosion resistant copper-nickel alloy suitable for condenser and heat exchanger tubes and many engineering applications such as salt water piping aboard ship, many components of salt water and fresh water stills, feed water heater tubes...
Journal Articles
Alloy Digest (1961) 10 (12): Cu-111.
Published: 01 December 1961
... Bridgeport Alloy 77 is a modified copper-zinc brass having improved resistance to bio-fouling, dezincification, and other forms of copper attack. It is recommended for condenser and heat exchanger tubes for marine use. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1970) 19 (3): Cu-213.
Published: 01 March 1970
... AMBRALOY-687 is an aluminum brass alloy containing arsenic as an inhibitor to dezincification. It is recommended for condenser and heat exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1962) 11 (3): Cu-114.
Published: 01 March 1962
... REVERE No. 429 is an aluminum bronze having good physical properties and high resistance to acids as well as fresh and salt waters. It is recommended for condenser tubes, bolts and tie rods. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1981) 30 (10): Cu-424.
Published: 01 October 1981
... with higher zinc contents. Typical uses are plumbing pipe and condenser and heat-exchanger tubes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1981) 30 (9): Cu-422.
Published: 01 September 1981
... alkaline. It also prossesses good resistance to corrosion by waters containing sulfides. It has moderate strength and good ductility. For a long time, this alloy has been considered a standard for condenser and heat-exchanger tubes. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1982) 31 (4): Ta-5.
Published: 01 April 1982
... is comparable to or better than that of pure tantalum. Typical appalications are heaters, condensers and multi-tube heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1982) 31 (8): Cu-443.
Published: 01 August 1982
... in such equipment as condensers, evaporators and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-443...