Alloy Digest (1967) 16 (1): TS-188.
Published: 01 January 1967
... VERSASTEEL is a tool steel designed to provide an unusual combination of fine grain structure, high secondary hardness, and compressive yield strength together with good toughness and high wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1973) 22 (6): TS-256.
Published: 01 June 1973
... CRUCIBLE VERSASTEEL is a type of tool steel with its composition carefully balanced to provide an unusual combination of fine grain structure, high secondary hardness and compressive yield strength, good toughness and exceptional wear resistance. Its resistance to tempering approaches that of high...
Journal Articles
Alloy Digest (1966) 15 (8): SA-199.
Published: 01 August 1966
... with latest revision of ASTM A-6 Table 2 - TYPICAL MECHANICAL PROPERTIES Charpy impact, ft. lbs. (V-notch) 20 Endurance limit, psi 55% of T.S. Compressive yield strength, psi (0.2%) Equal to T.Y.S. DOI: 10.31399/asm.ad.sa0199 Copyright © ASM International® 1996 Heat Treatment: Normalizing: Not normalized...
Journal Articles
Alloy Digest (1954) 3 (10): Mg-13.
Published: 01 October 1954
... DOWMETAL-C is a heat-treatable magnesium-base alloy suitable for sand and permanent mold castings. It has high tensile strength and good yield strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...
Journal Articles
Alloy Digest (1967) 16 (4): Mg-62.
Published: 01 April 1967
... Tensile yield strength, psi (0.2%) Elongation, % in 2 Brine11 hardness (500 Kg) Compressive yield strength, psi (0.2%) Shear strength, psi Bearing ultimate strength, psi Bearing yield strength, psi Charpy impact, ft. lbs. -F 49000 38000 14 33070; 27000 76000 56000 keyhole notch unnocched Bend rest...
Journal Articles
Alloy Digest (1995) 44 (6): Al-335.
Published: 01 June 1995
... ALUMINUM ALLOY(S) 206.0 and A206.0 are structural castings in the heat treated temper for applications requiring high tensile and yield strengths with moderate elongation. This datasheet provides information on composition, physical properties, tensile properties, and compressive, shear...
Journal Articles
Alloy Digest (1972) 21 (6): SA-275.
Published: 01 June 1972
... Elongation (8 in min, %, ii09 18 Reduction of area, min, % 60 Compressive Yield Strength (Approx. equal to tensile yield strength) Shear strength (Equal to 70% of tensile strength) Fatigue Properties Fatigue strength (107 cycles), psi Hot-rolled surface 33000** Polished surface 3mOo *Yield strengths...
Journal Articles
Alloy Digest (1970) 19 (10): SA-257.
Published: 01 October 1970
... - Hot Rolled Products Compressive yield strength, psi Equals tensile yield strength Shear strength, psi 75% of tensile strength Endurance Limit, psi Polished specimens of V45 and V50 60% of tensile strength Polished specimens of V55 50.60% of tensile strength Polished specimens of V60 and V65 50...
Journal Articles
Alloy Digest (1962) 11 (7): Mg-52.
Published: 01 July 1962
...%) 22400-28100 Elongation, X in 2 4-10 Compressive ultimate strength, psi 53800 Compressive yield strength, psi (0.1%) 22400-28100 Brine11 hardness (500 Kg) 65-80 Fatigue strength, psi (appror.) (50 x 106 cycles) 14600-16300 Table 2 - EFFECT OF MASS ON PROPERTIES (Fully heat treated) 1 Dia -- 4 Dia L...
Journal Articles
Alloy Digest (1967) 16 (6): Mg-63.
Published: 01 June 1967
..., % in 2 Compressive ultimate strength, psi Compressive yield strength, psi (0.1%) Shear strength, psi Brine11 hardness (500 Kg) Fatigue strength, psi (50 x lo6 cycles) 1.. ulameter 4 Diameter 34800-41500 24600-30300 Tensile strength, psi 39300 33600 2-6 Yield strength, psi (0.1%) 28500 26300 58200...
Journal Articles
Alloy Digest (1963) 12 (1): Mg-54.
Published: 01 January 1963
... Magnesium QE-22A is a heat treatable magnesium-silver-zirconium rare earth casting alloy having very high yield strength at temperatures up to 500 F. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well...
Journal Articles
Alloy Digest (1961) 10 (4): Ni-65.
Published: 01 April 1961
... Inconel 718 is an age-hardenable nickel-chromium alloy having exceptionally high tensile, yield, creep, and rupture strength at temperatures up to 1300 F. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well...
Journal Articles
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
... PROPERTIES OF VAX0 WEAR Compressive yield strength, psi 406000* Izod impact (No notch, smooth), ft-lb 72** *At a hardness level of Rockwell C 60. See Fig. 2 for compressive yield strength relative to five other tool steels. **At the typical working hardness in cold-won< applica- tions. See Fig. 3...
Journal Articles
Alloy Digest (1966) 15 (6): Mg-60.
Published: 01 June 1966
... 38000 Tensile yield strength, psi (0.2%) 28000 Compressive yield strength, psi (0.2%) 20000 Elongation, % in 2 4 Table 2 - MINIMUM MECHANICAL PROPERTIES - Tube (-F condition) Tensile strength, psi 34000 Tensile yield strengtk, psi (0.2%) 26000 Compressive yield strength, psi (0.2%) 14000 Elongation...
Journal Articles
Alloy Digest (2010) 59 (2): Al-428.
Published: 01 February 2010
... also Fig. 1 for compressive yield strength data. Corrosion: Exfoliation Corrosion Resistance. Alloy 7055-T7751 plate has shown no exfoliation after 2 years exposure in a seacoast environment at Point Judith, RI. The performance is significantly better than 7075-T651. The current ASTM G32 (EXCO...
Journal Articles
Alloy Digest (2004) 53 (5): Al-388.
Published: 01 May 2004
... strength and corrosion resistance. The alloy is a second-generation version of alloy 7050. Table 1 Guaranteed Minimum Long Transverse Mechanical Properties of 7150-T6151 Thickness Tensile strength Yield strength Compressive yield strength Alloy-temper mm in. MPa ksi MPa ksi MPa ksi Elongation, % 7150-T6151...
Journal Articles
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
... 35000 Tensile yield strength, psi (0.2%) 12000 25000 Elongation, % in 2 2.5 2.5 Brine11 hardness (500 Kg) 65 80 Shear strength, psi 28000 Endurance limit, psi 8500 Compressive yield strength, psi (0.2%) - 26000 Table 2 - TYPICAL SANDCAST PROPERTIES -T51 -T61 Tensile strength, psi 28000 39000 Tensile...
Journal Articles
Alloy Digest (2015) 64 (4): Al-442.
Published: 01 April 2015
... International® :: Data shown are typical, not to be used for specification or final design. Table 1 S basis minimum 7150-T7751 plate properties mm (in.) Ultimate tensile strength, MPa (ksi) Tensile strength, MPa (ksi) Compressive yield strength, MPa (ksi) Elongation, % Klc, MPa m, (ksi in.) 6.35 12.69 (0.250...
Journal Articles
Alloy Digest (1959) 8 (4): Al-77.
Published: 01 April 1959
... strength, psi ( 0.1 s ) 58250 Elongation, $% in 2 12 Brinell hardness (500 Kg) tJi 120 Shear strength, psi 33600 38100 Fatigue strength, psi 18000 18000 IZOditllp~ft.lbS. 16 Bearing yield saength, psi 53800 627: Compressive yield strength, psi (0.1% ) 31400 58200 Table 2- TYPICAL MECHANICAL PROPERTIES...
Journal Articles
Alloy Digest (2000) 49 (6): Al-370.
Published: 01 June 2000
... Mechanical Property Comparisons of 2 in. Plate Tensile strength Tensile yield strength Compressive yield strength Elongation, Alloy-temper MPa ksi MPa ksi MPa ksi % Long transverse test direction 2519-T87 455 66 400 58 414 60 6.0 2219-T87 441 64 352 51 352 51 6.0 Butt welds, longitudinal test direction 2519...