1-20 of 1003 Search Results for

compressibility

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2010) 59 (3): CS-153.
Published: 01 March 2010
... Ancorsteel 50 HP is a water-atomized, prealloyed low-alloy steel powder for high-performance applications. The prealloyed 0.50 wt.% Mo addition results in high compressibility and provides good response to heat treatment. In the powder production process used to make Ancorsteel, molten steel...
Journal Articles
Alloy Digest (2010) 59 (2): CS-152.
Published: 01 February 2010
... Ancorsteel 1000 is the workhorse of the Ancorsteel series. It has low levels of carbon and oxygen and good compressibility. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles that are then annealed to produce uniform, dependable...
Journal Articles
Alloy Digest (2015) 64 (10): CS-192.
Published: 01 October 2015
... Ancorsteel DWP200 is a water-atomized low apparent density powder for structural applications. The atomizing process imparts a more irregular spongy morphology to the powder particles, giving DWP200 a superior combination of green strength and compressibility compared to other atomized powders...
Journal Articles
Alloy Digest (2018) 67 (1): SA-809.
Published: 01 January 2018
... processing to maintain good compressibility while enabling high hardness and toughness in sinter-hardened parts. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on powder metal forms. Filing Code: SA...
Journal Articles
Alloy Digest (2019) 68 (12): Cu-888.
Published: 01 December 2019
... Wieland-UB5 is complex aluminum bronze that has excellent machinability, high hardness, and high compressive strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on high temperature...
Journal Articles
Alloy Digest (2016) 65 (2): CS-196.
Published: 01 February 2016
... Ancorsteel phosphorus alloys are ferrous base powders for PM parts requiring superior electromagnetic performance. Compared with parts made from pure, high compressibility iron powders, those made from the phosphorus alloys have higher resistivity, permeability and induction, and reduced coercive...
Journal Articles
Alloy Digest (1977) 26 (9): TS-323.
Published: 01 September 1977
... ONTARIO is an air-hardening die steel of the high-carbon high-chromium type. It has high hardness, high resistance to abrasion and excellent nondeforming characteristics. It is suited for a wide range of applications in which high abrasion resistance must be combined with high compressive strength...
Journal Articles
Alloy Digest (1991) 40 (10): Cp-18.
Published: 01 October 1991
... ZYMAXX provides outstanding compressive creep resistance, toughness and chemical inertness at high temperatures and pressures and under adverse conditions. They have a wide range of uses beyond chemical processing, including aerospace and automotive applications, general industrial equipment, home...
Journal Articles
Alloy Digest (1977) 26 (3): TS-315.
Published: 01 March 1977
... UHB RIGOR AR is a chromium-molybdenum-vanadium tool steel characterized by high surface hardness, high hardenability, high dimensional stability after hardening and tempering, high compression resistance, good machinability, good resistance to tempering and good wear resistance. Its many uses...
Journal Articles
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
... VASCO WEAR is an air-hardening, cold-work die steel developed to provide high resistance to wear at exceptionally good levels of toughness. It also has the high compressive strength necessary for maximum resistance to upsetting. Its many uses include such applications as thread-rolling dies...
Journal Articles
Alloy Digest (2015) 64 (4): Cu-836.
Published: 01 April 2015
... Wieland-UB7 is an aluminum bronze alloy with high hardness and compressive strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-836...
Journal Articles
Alloy Digest (1967) 16 (1): TS-188.
Published: 01 January 1967
... VERSASTEEL is a tool steel designed to provide an unusual combination of fine grain structure, high secondary hardness, and compressive yield strength together with good toughness and high wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2010) 59 (2): Al-428.
Published: 01 February 2010
... The 7xxx series alloys contain zinc as the main alloying element, usually in combination with magnesium and copper. Alcoa’s high-strength 7055 alloy is supplied as plate and extrusions and used for compressive strength applications. This datasheet provides information on composition, tensile...
Journal Articles
Alloy Digest (1957) 6 (12): TS-65.
Published: 01 December 1957
... VENANGO SPECIAL is a low-alloy high-strength tool steel of the silico-manganese type having high impact and high compression strength plus high wear resistance. It is similar to AISI Type S2 but with higher carbon content. This datasheet provides information on composition, hardness, tensile...
Journal Articles
Alloy Digest (1979) 28 (11): TS-356.
Published: 01 November 1979
... UHB SVERKER 21 is a high-carbon, high-chromium cold-work tool steel alloyed with molybdenum and vanadium. It has high hardenability and high surface hardness after hardening. It has excellent wear resistance and high compressive strength along with moderate toughness (shock resistance). This steel...
Journal Articles
Alloy Digest (1979) 28 (1): CI-47.
Published: 01 January 1979
... it has a tensile strength of about 95,000 psi and a compressive strength of 360,000 psi. Typical applications are pump parts, mixers and coal-gasification components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1954) 3 (3): TS-19.
Published: 01 March 1954
... PRESSURDIE-3, developed particularly for injection and compression molding, has high compression strength, wear resistance, and corrosion resistance. It is a ASM Class IV-B type alloy. This datasheet provides information on composition and hardness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1964) 13 (7): Ti-40.
Published: 01 July 1964
... Kentanium K138-A is a high temperature titanium carbide that greatly widens the scope of the engineering design where conditions of intermittent or continuous high temperatures in oxidizing atmospheres are combined with abrasion, and compressive or tensile loads. This datasheet provides...
Journal Articles
Alloy Digest (1969) 18 (4): TS-217.
Published: 01 April 1969
... EB alloy is a high-carbon chromium alloy steel for general hot-work applications. It possesses good compressive strength and hot mechanical properties. It is recommended for hot header and gripper dies, shear blades, hot rivet sets, forging dies, cold forming and embossing dies. This datasheet...
Journal Articles
Alloy Digest (1969) 18 (4): TS-218.
Published: 01 April 1969
... Ultradie 3 is a high production tool and die steel of the high-carbon high-chromium type. It is deep hardening, non-deforming, and has high resistance to wear and compression. It is recommended for heavy duty tools and dies. This datasheet provides information on composition, physical properties...