Alloy Digest (1975) 24 (6): Fe-52.
Published: 01 June 1975
... ALLOY 48 is a vacuum-melted, 48% nickel-iron alloy designed for high permeability, and low core losses. It is ideal in applications requiring efficient magnetic core materials, such as audio and instrument transformers, instrument relays, and many other communication equipment devices...
Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... devices in which extremely high permeability at low magnetizing forces greatly increases the efficiency and effecrive- ness of the equipment. Because of its high permeability, it is used in solenoid cores in light, sensitive relays char must operate and respond co weak currents that induce low magnetizing...
Journal Articles
Alloy Digest (1963) 12 (1): Fe-10.
Published: 01 January 1963
... readily. The exceptional magnetic and electrical properties of Armco Magnetic Ingot Iron make it especially suitable for d-c applications. It offers high density, purity and consistant uniformity. It is supplied in heavy heavy sheet and strip gages, as well as bar form, for d-c equipment. Ir has a wide...