Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... blanking and cold-drawing dies, punches, burnishing tools, slitter knives and gages. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating and machining. Filing Code: TS-361. Producer or source: Guterl Special Steel Corporation...
Journal Articles
Alloy Digest (2002) 51 (3): TS-597.
Published: 01 March 2002
... sheet) or structural parts (thicker sheet). Typical applications include general blanking and forming, heavy-duty blanking and forming, deep drawing, coining, cold-extrusion dies with complicated geometry, rolls, shear blades, and prototype tooling. Producer: Bohler Uddeholm North America 4202 Tollview...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... twist parts of the casting through 90 degrees or more. Up co 40% reduction in area, cold swaging improves the tensile strength and ductility. Cold swaging does not make the alloy sensitive to subsurface network corrosion. Corrosion Resistance: Good resistance to atmospheric corrosion, but readily at...
Journal Articles
Alloy Digest (1985) 34 (9): TS-447.
Published: 01 September 1985
... grindability. Among its many uses are punches and dies for blanking and forming thin sheet, milling cutters, twist drills, reamers, forming rolls, cold-extrusion punches and draw dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1975) 24 (4): TS-287.
Published: 01 April 1975
... AISI Type O6 is a free-machining, oil-hardening tool steel designed for cold-work dies. Because about one-third of its carbon is present as graphite, it has excellent machinability and exceptional resistance to galling and seizing. It is primarily used on drawing, forming and shaping operations...
Journal Articles
Alloy Digest (1969) 18 (3): TS-215.
Published: 01 March 1969
... Truwear is a high-carbon high-chromium cold work tool steel having extremely high resistance to abrasion and wear. It is recommended for deep drawing dies, brick mold liners, valve seats, master gages, etc. This datasheet provides information on composition and hardness as well as fracture...
Journal Articles
Alloy Digest (1997) 46 (4): SS-679.
Published: 01 April 1997
... to 350 C (652 F). This grade is particular suitable for high degrees of cold working and for sequential drawing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1969) 18 (4): TS-217.
Published: 01 April 1969
...&18500F, cool in a dry air blast. When maximum hardness is required, as for a cold work application, bring up to 1750 to 18500F and quench in oiL Tempering: The hardness falls off rather slowly with draws up to lOOOoF. Average hot work applications call for draws from 900 to 115OoF. Dies used on cold work...
Journal Articles
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-roll dies. draw dies. forming rolls. hot and cold-piercing punches. shear blades and coining dies. Manufacturer: AL Tech Specialty Steel Corporation Dunkirk. New York 14048. ...
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
...) Blanking, stamping, and cold-forming dies and punches for long runs, (2) Lamination dies, (3) Bending, forming and seaming rolls, (4) Cold trimmerdies. (5) Burnishing dies or rolls. (6) Plug gages, (7) Drawing dies for bars or wire, (8) Slitting cutters and (9) Lathe centers subject to severe wear...
Journal Articles
Alloy Digest (1985) 34 (12): TS-451.
Published: 01 December 1985
... ATMODIE* 4 (Cold-Work Tool Steel; AISI Type D4) ATMODIE 4 is an air-hardening steel containing high percentages of carbon and chromium. It possesses exceptional wear resistance which makes it ideally suited to long-run production requirements. Its strength is very high and its toughness is good when...
Journal Articles
Alloy Digest (1980) 29 (10): TS-371.
Published: 01 October 1980
... bar draw dies, cold-extrusion dies, broaches, metal spinning tools, master gages, closure dies, meat chopper plates, Sendzimer MiIl rolls, ceramic tile dies and punches, valve seats (cast), valve rings for coal pipe lines (cast), stainless steel and aluminum blanking dies, and slitter knives (silicon...
Journal Articles
Alloy Digest (1985) 34 (4): TS-439.
Published: 01 April 1985
..., machine tool ways, pottery tools, tube and bar draw dies, cold-extrusion dies, broaches, metal spinning tools, master gages, closure dies, meat chopper plates, Sendzimer Mill rolls, ceramic tile dies and punches, valve seats (cast), valve rings for coal pipe lines (cast), stainless steel and aluminum...
Journal Articles
Alloy Digest (1969) 18 (6): TS-220.
Published: 01 June 1969
... retains the lubricant, it possesses excellent non-seizing and non-galling qualities. Forms Available: Billets. bars, rods and forgings. Applications: Blanking dies. punches, trimming shear blades, spindle arbors, forming rolls, cold forming dies, gages, drawing dies. stripper and wear plates. Manufacturer...
Journal Articles
Alloy Digest (1986) 35 (1): TS-454.
Published: 01 January 1986
... immediately. Tempering: Place work in a cold furnace and heat slowly to the tempering temperature, normally 300- 550°F. Hold at temperature for one hour per inch of thickness. DOI: 10.31399/asm.ad.ts0454 Copyright © ASM International® 1996 2 4 6102045602 4 6 102045602 46 102045 SCOfldS Minutes Hours TIME Fig...
Journal Articles
Alloy Digest (1982) 31 (9): TS-404.
Published: 01 September 1982
... a wide range of cold-working tools such as broaches, blanking dies, punches, thread-rolling dies, paper knives and wood-working tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and...
Journal Articles
Alloy Digest (1987) 36 (10): TS-482.
Published: 01 October 1987
... SUPERDIE is a superior oil-hardening cold-work die steel of the high-carbon, high-chromium type. It has outstanding wear resistance combined with high hardenability and exceptional size stability. SUPERDIE is especially suited for tools and dies where dimensional limits are close, and high...
Journal Articles
Alloy Digest (1970) 19 (3): TS-228.
Published: 01 March 1970
...: Rectangular or round sintered blanks. Applications: Regressive dies, perforation dies for expanded metals, cold drawing dies for steel bar stock, turning tools for semi-sintered ceramics. Blanking and piercing dies, cold heading and forming dies, crimpers, shears, cutting tools, bearings, gages, nozzles...
Journal Articles
Alloy Digest (1965) 14 (8): TS-168.
Published: 01 August 1965
..., rods and forgings. Applications: Blanking and trimming dies, cams, engravers tools, cutters, circular thread rook, cold drawing dies, feed rolls, shear blades, broaches, coining dies, forming dies, gauges, lamination and plastic cut dies, thread rolling dies, master tools, burnishing tools, slirring...
Journal Articles
Alloy Digest (1962) 11 (9): TS-124.
Published: 01 September 1962
... much less pronounced. Forms Available: Billers, bars, and forgings and castings. Applications: Shear blades, cold press tools, heavy duty punching dies, broaches, mandrels, rolls, blanking and forming dies, coining and drawing dies, gauges, spinning CoOlS, pulverizing blades, burnishing tools...