1-20 of 3505 Search Results for

cold workability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1981) 30 (11): Cu-425.
Published: 01 November 1981
... MUELLER Alloy 3300 is a brass containing 0.5% lead for improving machinability. The lead detracts somewhat from its cold workability; however, despite the lead, cold workability is rated as excellent. Overall, the alloy has a good to excellent combination of machinability and cold workability...
Journal Articles
Alloy Digest (1978) 27 (4): CS-72.
Published: 01 April 1978
... SAE 1019 is a carbon steel that combines good machinability, good hot and cold-workability, and good welding characteristics. It is used in the annealed, hot-worked, normalized, cold-worked or water-quenched-and-tempered condition for many automotive and metal-working applications. It may be used...
Journal Articles
Alloy Digest (1980) 29 (10): CS-84.
Published: 01 October 1980
... and cold workability, good machinability and good weldability. Typical applications are carburized parts, bolts, trusses and cold-extruded parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1986) 35 (1): CS-109.
Published: 01 January 1986
... and cold workability, good machinability and good weldability. Typical applications are carburized parts, bolts, trusses and cold-extruded parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1979) 28 (2): Al-126.
Published: 01 February 1979
... ALUMINUM 5056 is a non-heat-treatable wrought aluminum-magnesium-manganese-chromium alloy possessing high strength and ductility along with good hot and cold workability. It is recommended for such applications as rivets and screen wire. It may be used with or without cladding. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-400.
Published: 01 August 1980
... ANACONDA Copper 122 is deoxidized copper with high residual phosphorus. It is a medium-strength material with high ductility and excellent hot and cold workability. It is the copper-base material used most widely in the production of tube and pipe for a wide variety of uses including the air...
Journal Articles
Alloy Digest (1975) 24 (10): Cu-302.
Published: 01 October 1975
... COPPER ALLOY No. 782 is a copper-zinc-nickel alloy with good cold workability, good machinability, excellent strength and good resistance to corrosion. It is used for a variety of industrial and decorative applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1995) 44 (6): Ti-107.
Published: 01 June 1995
... SP 700 is a high strength, beta-rich alpha-beta titanium alloy. It was developed with the following attributes: (1) excellent hot- and cold-workability; (2) enhanced hardenability with a wide range of mechanical properties that can be obtained by heat treatment; and (3) superior superplastic...
Journal Articles
Alloy Digest (2002) 51 (6): Cu-683.
Published: 01 June 2002
... Swissmetal alloy SM158N (Boillat 61B) is a free-machining brass with both machinability and cold workability. The alloy has been called heavy-leaded brass, clock brass, and engraver’s brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... has high strength and ductility, good weldability, good hot and cold workability, and good machinability. This datasheet provides information on composition, physical properties, microstructure, tensile properties. It also includes information on high temperature performance and corrosion resistance...
Journal Articles
Alloy Digest (1962) 11 (12): Ni-77.
Published: 01 December 1962
... RAonel 600 is a corrosion and heat resisting nickel-base alloy having a combination of high strength and oxidation resistance along with hot and cold workability. It is recommended for component parts in the aircraft, chemical, petroleum and paper pulp industries. This datasheet provides...
Journal Articles
Alloy Digest (1963) 12 (11): Cu-135.
Published: 01 November 1963
... Amphos is a phosphorized oxygen-free copper having free-scaling properties, freedom from hydrogen embrittlement, improved cold workability, and desirable high softening temperature. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1991) 40 (10): Cu-565.
Published: 01 October 1991
... Copper Alloy No. C43500 is a tin containing brass. It has strength and ductility comparable to low brass (80% copper, 20% zinc). It has excellent cold workability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1977) 26 (2): Ni-240.
Published: 01 February 1977
.... General Characteristics: Nimag 60 is a solid-solution, nonmagnetic, high corrosion and heat-resistant nickel-base alloy. It has an excellent com- bination of high strength, hot and cold workability, resistance to ordinary forms of corrosion, good heat resistance, and freedom from aging or stress corrosion...
Journal Articles
Alloy Digest (1969) 18 (12): Ni-149.
Published: 01 December 1969
... Pyromet 600 is a corrosion-resisting nickel-base alloy, having a very desirable combination of high strength and workability, both hot and cold. It has high strength and resistance to oxidation at high temperatures. It is designed to meet the highest quality of the nuclear industry. This datasheet...
Journal Articles
Alloy Digest (1991) 40 (1): Ni-391.
Published: 01 January 1991
... UNS No. N06600 is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with good workability. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1972) 21 (7): Ni-176.
Published: 01 July 1972
...-machining stainless steel. The alloy is best handled on heavy-duty equipment using cutting tools large and heavy enough to withstand the loads and to quickly dissipate the heat generated. Tools must be sharp and have the proper geometry. Workability: INCQNEL aBoy 600 is workable, both hot and cold...
Journal Articles
Alloy Digest (1980) 29 (1): Al-161.
Published: 01 January 1980
.... Workability: The hot-working characteristics of Aluminum 5252 are good and its hot-working temperature range is 950-500oF. Aluminum 5252 has excellent cold workability in the annealed condition. It is well suited to the production of drawn shapes and blanked and peirced parts Although this alloy...
Journal Articles
Alloy Digest (1991) 40 (5): Cu-560.
Published: 01 May 1991
... rating of Copper Alloy No. C27400 is 35 on a scale where free cutting brass is 100. Workability: Cold workability of Copper Alloy No., C27400 is excel- lent. Common fabrication processes include blanking, forming and bending, roll threading and knurling, shear- ing, spinning, squeezing and swaging...
Journal Articles
Alloy Digest (1992) 41 (4): Cu-570.
Published: 01 April 1992
... is not hardenable by heat ueatment. It may be annealed at 840-102oOF (450-550°C). Machinability: The machinability rating of Copper Alloy No. C 192 10 is 20 on a scale where free cutting brass is 100. Workability: Copper AlIoy No. Cl9210 has excellent hot and cold workability. Commonly used fabrication processes...