Publisher: Journals Gateway
Alloy Digest (2007) 56 (5): TS-649.
Published: 01 May 2007
... Thyrodur 2550 is a cold-work steel with very good toughness. It is dimensionally stable, impact-resistant, and has a high hardening capacity. It is similar to AISI S1. A typical application is as cold shear knives. This datasheet provides information on composition, physical properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (11): TS-390.
Published: 01 November 1981
..., rotary slitters, shear knives and cold-forming rolls. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-390. Producer or source...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (2): SA-160.
Published: 01 February 1964
... vcty readily and can be cast to shape. Forms Available: Tubes, bats, and forgings. Applications: Beatings, machine parts, cold shears, knives. srraight- ener rolls. sizing tables. Manufacturer: Tiiken Roller Bearing Co. Steel & Tube Division Canron, Ohio TRANSFORMATION TIME - MINUTES ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (3): TS-346.
Published: 01 March 1979
... CYCLOPS SCK is a cold-work tool steel with a balanced composition to provide air hardening and an optimum combination of toughness, wear resistance and minimum distortion during heat treatment. Typical applications are shear blades, trimming dies and forming rolls, including grade rolls...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (5): TS-648.
Published: 01 May 2007
... mechanisms. Examples include screws and barrels for plastic processing, cold and hot forming rolls, hot shearing knives, circular slitting knives, hot-forming trimming dies, wear parts, engineering applications. Producer: Bohler-Uddeholm North America Rolling Meadows, IL 60008 (800) 652-2520 (847) 577-8028...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (4): TS-361.
Published: 01 April 1980
... blanking and cold-drawing dies, punches, burnishing tools, slitter knives and gages. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating and machining. Filing Code: TS-361. Producer or source: Guterl Special Steel Corporation...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (8): TS-774.
Published: 01 August 2019
..., cold piercing punches, preforming punches, shear blades, chipping knives, pneumatic chisels, coining tools, cold shear blades, and ejectors. Fig. 1 Tempering diagram Fig. 2 Time temperature transformation diagram ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (1): TS-188.
Published: 01 January 1967
.... Rockwell hardness CS8-60: In applications where the complete relief of residual stresses provides a superior edge-holding ability (resistance co spalling) such as slitter knives, hoc and cold shears, valve extrusion die inserts which require the ultimate in high temperature abrasiaa resistance. Versasteel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (11): TS-593.
Published: 01 November 2001
... coining dies, rotary shears, slitter knives, chipper knives, and blanking dies. Producer: Carpenter Specialty Alloys Carpenter Technology Corporation P.O. Box 14662 Reading, PA 19612-4662 (610) 208-2000 (610) 208-2802 (fax) ISSN: 002-614X TS-593BFig. 1 Hardening versus tempering temperature ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (1): TS-602.
Published: 01 January 2004
...: punches, rotary shears, blanking dies, chipper knives, slitter knives, and thread-rolling dies. Producer: Carpenter Specialty Alloys Carpenter Technology Corporation Reading, PA 19612-4662 (610) 208-2000 (610) 208-2802 (fax) ISSN: 002-614X TS-602B ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (8): TS-427.
Published: 01 August 1984
... at temperatures shown. Average of at least 5 specimens. Forms Available: Billets. bars. rods and forgings. Applications: Cobalt Chrome can be used for blanking dies. burmshing tools. cold-formmg dies. thread-rolling dies. drawing dies. gages. knurls. lamination dies. punches. rolls. shear knives and slitter...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1997) 46 (5): TS-555.
Published: 01 May 1997
...=F.Holdat126CPFfor4h andfumacecoolto8OO T.Thisatme&ngcycIeshouIdresultina hdness of approximately 255 HR. For Bar Shear Knives It is recommended that knives be machined to grinding tolerances before heat neatmem Observe usual precautions to prevent oxi- dation, carbarizaton or decarburixation. IhltiRg: 1...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (7): TS-320.
Published: 01 July 1977
... demanding applications. Forms Available: Billets, bars and forgings. Applications: Thread rolling dies, knurls, slitter knives, lathe centers, cold-finishing rolls, cold-forming rolls, punches, trim dies, blanking dies, shear blades, lamination dies and granulating knives. Manufacturer: Teledyne VAX0...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (10): TS-275.
Published: 01 October 1974
... per cent carbon content and balanced alloy content of Cromo-W55 make it adaptable to many applications where improved wear resistance over the standard AK1 H12 type is needed. Forms Available: Forgings, billets and bars. Applications: Typical cold-working applications are shear knives, rotary slitters...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... because of alternate heating and cooling or where breakage is the primary cause of failure. Forms Available: Billets, bars, rods, sheet, plate and forgings. Applications: Hotform No. 3 is used for shear knives, rotary slitters, cold-forming dies, heavy-duty blanking and heading dies, punches, coining...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (1): TS-807.
Published: 01 January 2021
... Uddeholm Viking is a medium-carbon, chromium-molybdenum-vanadium, alloy cold-work tool steel that is characterized by an excellent combination of wear resistance and toughness required for chipper-knives and for heavy-duty blanking and forming. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (11): TS-356.
Published: 01 November 1979
...). It is used for a wide range of cold-working tools for blanking, punching, cropping, shearing, trimming, shredding, clipping and forming (cold-working dies of many types and uses). Other uses include circular shears, knives, woodmilling cutters, reamers, broaches, mandrels, master hobs for cold hobbmg, gages...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (11): TS-341.
Published: 01 November 1978
... UNS No. T30402 is an air-hardening high-carbon, high-chromium cold-work die steel that offers excellent wear resistance. It is a deep-hardening steel but hardens with a minimum change in size and volume. Typical uses are cold-work dies, slitting cutters, shear blades and wood-working tools...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... of chromium and molybdenum. It is used for both cold and hot tooling applications. Its many uses include shear blades, swaging dies, chisels and dies for molding plastics below 1000 F (538 C). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (8): SA-461.
Published: 01 August 1991
... for spinning machines, cams for knitting machines. Knives: Paper shearing, paper slitting rolls, circular slit- ting, rubber and tire trimming, spacers for slitting lines. Manufacturer: Uddeholm Corporation Rolling Meadows, Illinois 60008 Copyright ┬ę ASM International┬« 1996DOI: 10.31399/asm.ad.sa0461 ...