Skip Nav Destination
Close Modal
Search Results for
coil springs
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 137 Search Results for
coil springs
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (5): SA-496.
Published: 01 May 1998
... Inland DuraSpring is a high-strength microalloyed spring steel for use in high stress coil springs for automobile and light truck suspension systems. This bar product offers significant improvements in tensile strength, fatigue properties, and fracture toughness compared to conventional spring...
Abstract
View article
PDF
Inland DuraSpring is a high-strength microalloyed spring steel for use in high stress coil springs for automobile and light truck suspension systems. This bar product offers significant improvements in tensile strength, fatigue properties, and fracture toughness compared to conventional spring steels. This datasheet provides information on composition, hardness, and tensile properties as well asfracture toughness and fatigue. Filing Code: SA-496. Producer or source: Ispat Inland Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (8): Ti-87.
Published: 01 August 1987
..., aggressive environments containing ferric chloride, sodium chloride, carbon dioxide and hydrogen sulfide. Its applications include coil springs, fasteners, rivets and downhole oil-production equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Abstract
View article
PDF
RMI Beta C is a heat-treatable titanium-base alloy that develops a tensile strength of over 200,000 psi in the solution-treated-and-aged condition. It has good ductility and toughness, good fabricability and a low elastic modulus. It has good resistance to general corrosion and it resists hot, aggressive environments containing ferric chloride, sodium chloride, carbon dioxide and hydrogen sulfide. Its applications include coil springs, fasteners, rivets and downhole oil-production equipment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-87. Producer or source: RMI Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (8): Cu-563.
Published: 01 August 1991
... heading, coining, stamping, roll threading and knurling. Joining by soldering, brazing, gas shielded arc and resistance methods produce excellent results. Forms Available: Strip, sheet, rod, wire, tube, pipe, shapes in a variety of tempers. Applications: Springs, connectors and coil springs where good...
Abstract
View article
PDF
Copper Alloy No. C72600 is a wrought copper-nickel alloy. It has excellent capacity for cold work and may be readily joined by soldering, brazing, arc and resistance welding. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on forming, heat treating, and joining. Filing Code: Cu-563. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (11): Co-4.
Published: 01 November 1971
... properties. The alloy is used mainly for various types of springs. Forms Available: Strip, wire, cable and tube. Applications: Main springs, power springs, coil springs, torsion bars, ball bearings, textile thread guides, valve parts, textile cutting wire, pivot points, high-temperature aircraft cable...
Abstract
View article
PDF
EIGILOY is a cobalt-base alloy that is characterized by high tensile and fatigue strength and good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-4. Producer or source: Elgiloy Company. Originally published August 1953, revised November 1971.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (4): Cu-230.
Published: 01 April 1971
..., switch gear, resistance welding tip holders, flat leaf and coil springs, switch parts, contacts, relays, fuse clips, components for railroad equipment. Manufacturer: Practically all copper alloy mills. ...
Abstract
View article
PDF
COPPER ALLOY No. 647 is an age-hardenable copper-nickel-silicon alloy which can be age hardened to strength levels equivalent to those of many alloy steels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-230. Producer or source: Copper and copper alloy mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (7): Ti-134.
Published: 01 July 2004
... bar, rolled and/or drawn rod and wire. Applications: Allvac 38-644 finds use in high-strength aerospace and com- mercial applications, structural parts, gas and petroleum down- hole piping systems and tooling, and high-strength coil springs and fasteners. This alloy can be used for extended periods...
Abstract
View article
PDF
Allvac 38-644 is a metastable beta titanium alloy known for its ductility in the solution treated condition and its high strength and ductility in the solution treated and aged condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TI-134. Producer or source: Allvac Metals Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (4): SS-372.
Published: 01 April 1980
...) DOI: 10.31399/asm.ad.ss0372 Copyright © ASM International® 1996 Conv. 17 Cr- cryotech 302 7 Ni 302 Spring Rate (lb/in.) 66 66 66 Free Length (in.) 3.0 3.01 3.01 Mean Coil Dia. (in.) 1.15 1.13 1.13 Inside Dia. (in.) 0.997 0.992 1.0 Wire Dia. (in.) 0.153 0.138 0.130 Solid Height (in.) 1.33 0.98 0.73...
Abstract
View article
PDF
CRYOTECH 302 is a new, cryogenically processed stainless steel wire with the same composition as AISI Type 302. The cryogenic processing gives tensile and torsional properties that are independent of wire diameter (thus simplifying spring design calculations) and markedly greater than those of conventional stainless steels. Cryotech 302 has uniformly high properties: 290,000 psi tensile strength and 145,000 psi minimum torsional yield strength. Thus it provides greater design flexibility than conventional stainless steels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: SS-372. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (10): SA-121.
Published: 01 October 1961
.... Applications: Gears, splined shafts, hand tools, and miscellaneous machinery parts. Pinions, spindles, drill stems, reamer pins, leaf and coil springs, shovels, shafts. Manufacturer: Practically all alloy steel mills. ...
Abstract
View article
PDF
AISI 4650 is an oil hardening, medium-carbon alloy steel having high mechanical properties, endurance limit and shock resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-121. Producer or source: Alloy steel mills and foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (8): SS-354.
Published: 01 August 1978
... processing UCAR 302 has ample ductility for fabrication into springs and other wire products. UCAR 302 passes the ductility wrap test as described in general in ASTM A 370. The test for UCAR 302 wire particularly consists of coiling the wire closely on its own diameter for a minimum of five wraps...
Abstract
View article
PDF
UCAR 302 is a cryogenically processed stainless steel wire with the same composition as AISI Type 302. The processing gives tensile and torsional properties that are independent of wire diameter and markedly greater than those of conventional stainless steels. UCAR 302 has uniformly high properties: 290,000 psi tensile strength and 145,000 psi minimum torsional yield strength. Thus it provides greater design flexibility than conventional stainless steels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: SS-354. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (9): SS-1248.
Published: 01 September 2016
... condition, the ratio of 0.2% offset proof strength/tensile strength will be about 0.87. After tempering, the ratio will be about 0.95. Note that tension springs coil with initial tension must not be tempered at the same high temperature as other types of springs. The producer recommends batch annealing...
Abstract
View article
PDF
Sandvik 9RU10 is a precipitation hardening stainless steel with the highest relaxation resistance of all of the Sandvik wire grades. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes information on forming and heat treating. Filing Code: SS-1248. Producer or source: Sandvik Steel Company. Originally published July 2016, revised September 2016.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (9): SS-1309.
Published: 01 September 2019
... GPa (106 ksi), As delivered 71 (10.3) Tempered 73 (10.6) See also Table 1 and Fig. 1 3. Mechanical properties are in the as-delivered condition. For Fig. 1, the curve is valid for springs coiled from wire 1 mm (0.04 in.) in diameter and represents a 90% certainty against failure. Shear stress range...
Abstract
View article
PDF
Sandvik 12R10L is fully austenitic with a very low cobalt content for nuclear applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength as well as fatigue. It also includes information on high temperature performance as well as heat treating. Filing Code: SS-1309. Producer or source: Sandvik Steel Company and Sandvik AB.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (8): SS-1074.
Published: 01 August 2010
... °F). In the as delivered condition the ratio proof strength/tensile is approximately 0.80. After tempering, the ratio will be approximately 0.85. Please note that tension springs coiled with an initial tension must not be tempered at the same high temperature as other types of springs. The producer...
Abstract
View article
PDF
Sandvik T302 HS is a general purpose austenitic stainless steel with respect to corrosion resistance only in a spring temper for higher strength. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes information on forming and heat treating. Filing Code: SS-1074. Producer or source: Sandvik Steel Company and Sandvik AB.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (7): SS-935.
Published: 01 July 2005
... in uneven tempering. In the as-delivered condition, 0.2% offset yield strength to tensile strength ratio is about 0.809. After tempering the ratio will be about 0.85. Note that tension springs coiled with initial tension must not be tempered at the same high temperature as other types of springs. Sandvik...
Abstract
View article
PDF
Sandvik 13RM19 combines high mechanical strength with a nonmagnetic structure. This combination of properties has previously been found mainly in Co-Ni-base or Cu-Be alloys. The steel has very good corrosion resistance comparable to that of AISI Type 302. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength It also includes information on low temperature performance as well as forming, heat treating, and joining. Filing Code: SS-935. Producer or source: Sandvik Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (10): Ni-627.
Published: 01 October 2005
... 25 345 50 1050 1100 1920 2010 345 50 1100 1150 2010 2100 275 40 1150 1200 2100 2190 205 30 DOI: 10.31399/asm.ad.ni0627 Heat Treatment: Heat treatment is done after the spring coiling operation. Depending on the desired mechanical properties and service tem- perature...
Abstract
View article
PDF
Sandvik Sanicro 75X1 is a nickel-base age-hardenable spring wire. This datasheet provides information on composition, physical properties, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-627. Producer or source: Sandvik Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (8): SS-1100.
Published: 01 August 2011
... the ratio proof strength/tensile is approximately 0.85. After tempering the ratio will be approximately 0.90. Please note that tension springs coil with initial tension and must not be tempered at the same high temperature as other types of springs. The producer recommends batch annealing at 250 °C (480 °F...
Abstract
View article
PDF
Sandvik Bioline 11R51 HV is the vacuum remelted version of the alloy required for higher cleanliness. This datasheet provides information on composition, physical properties, elasticity, and shear and bend strength It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1100. Producer or source: Sandvik Materials Technology.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (2): Cu-291.
Published: 01 February 1975
... and excellent abrasion resistance. Alloy 664 is resistant to both general and stress corrosion. It is used for such applications as electrical springs and terminals, bearings and switch blades for switches. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Abstract
View article
PDF
OLIN Alloy 664 is a fine-grained copper-zinc-iron-cobalt alloy developed to economically replace the tin brasses. It exhibits properties comparable to or better than the more popular tin brasses. It possesses a favorable combination of strength and ductility, superior bad-way-bend properties and excellent abrasion resistance. Alloy 664 is resistant to both general and stress corrosion. It is used for such applications as electrical springs and terminals, bearings and switch blades for switches. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on wear resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-291. Producer or source: Olin Corporation, Brass Group.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (7): Cu-704.
Published: 01 July 2003
... coils are available with coil weights up to 1.5 Tonnes. Applications: Typical applications include use in relay and switch springs, con- nectors, and connector pins for switches and relays. Producer: Wieland Metals, Inc. Wheeling, IL 60090 (847) 537-3990 (847) 537-4085 (fax) In Germany Wieland-Werke AG...
Abstract
View article
PDF
Wieland-B16 has excellent strength and cold-working properties. It is largely used in connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as deformation and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-704. Producer or source: Wieland Metals Inc., Wieland-Werke AG.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2014) 63 (12): Co-124.
Published: 01 December 2014
..., this process involves a decrease of approximately 10% of the UTS compared to the coil form. Applications: Medical: prosthesis and fixation screws, pacemaker electrodes, vascular stent, vena cava filter, orthodontic, ancillary Aerospace industries: springs, torsion bar, gyroscope parts Naval equipment...
Abstract
View article
PDF
UGI KC35N is a nonmagnetic nickel-cobalt-chromium-molybdenum alloy with a fully austenitic structure. This datasheet provides information on composition, physical properties, elasticity, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-124. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (9): Cu-639.
Published: 01 September 1999
... WRM alloy 4222 is a copper-zinc alloy of the tin-brass family with a good combination of conductivity, strength, and forming characteristics. A typical application is in high-performance conductive springs. This datasheet provides information on composition, physical properties, tensile properties...
Abstract
View article
PDF
WRM alloy 4222 is a copper-zinc alloy of the tin-brass family with a good combination of conductivity, strength, and forming characteristics. A typical application is in high-performance conductive springs. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-639. Producer or source: Waterbury Rolling Mills Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (9): Cu-723.
Published: 01 September 2004
... mm. The strip width is from 3 mm with a minimum of 10 times the thickness. Transverse-wound strip with coil weights of up to 1.5 T are available. Tinned strip and contour-milled strip are also available. Applications: Typical uses of strip and sheet include electrical switch springs, terminals...
Abstract
View article
PDF
Wieland-S12 has good cold working properties. Spring properties are higher than phosphor bronzes and stress-corrosion cracking (SCC) sensitivity is lower than that of copper-zinc alloys. Applications include connectors in the automobile industry. This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-723. Producer or source: Wieland Metals Inc., Wieland-Werke AG.