Alloy Digest (1971) 20 (2): Ni-162.
Published: 01 February 1971
... TOPHET H is a heating-element alloy specifically designed for use in duct heaters and clothes dryers where hot strength and long life are of most importance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1971) 20 (2): SS-250.
Published: 01 February 1971
..., casket shells, clothes dryer drums, sink strainers, gas range burner rings, office furniture, and other uses where corrosion resistance at minimum cost and good surface finish are important factors. Manufacturer: Armco Steel Corporation Advanced Materials Division Baltimore. hlary!and ? 1203 ...