1-20 of 2101

Search Results for chromium-molybdenum steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1993) 42 (9): SA-468.
Published: 01 September 1993
... for plastic mold base material and for holder blocks for die casting dies. It can also be used in non- critical molds where a #2 finish is acceptable. Composition, Nominal Wt, %: Carbon 0.40 Manganese 0.88 Silicon 0.30 Sulfur 0.15 max. Phosphorus 0.035 max. Chromium 1.0 Molybdenum 0.20 Iron Remainder Physical...
Journal Articles
Alloy Digest (1956) 5 (5): SA-42.
Published: 01 May 1956
... (NickeLChrome-Molybdenum Steel) I-W-TEN M is a triple alloy electric furnace steel recommended for parts requiring great hardness, wear, and high strength combined with toughness. Composition: Cartwo Nominal 0.70 Tempering Temperature, F. 325 ::x 800 1000 Tensile Strength psi 302000 %L%! 25iOtiO 191000...
Journal Articles
Alloy Digest (1988) 37 (9): SA-18.
Published: 01 September 1988
... AISI 4140 is a through-hardening chromium-molybdenum medium carbon steel. It is not subject to temper embrittlement. It is recommended for heavy duty service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1975) 24 (6): SA-316.
Published: 01 June 1975
... SAE 4135 is a medium-carbon chromium-molybdenum alloy steel for heavy-duty service. Although nominally an oil-hardening grade, it may be water hardened if proper precautions are exercised. It is used for a wide variety of engineering applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1957) 6 (7): SA-58.
Published: 01 July 1957
... DM-2 is a low-carbon chromium-molybdenum steel recommended for use at temperatures up to 1100 deg. F. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1957) 6 (7): SA-59.
Published: 01 July 1957
... AISI 4150 is a through hardening chromium-molybdenum medium carbon steel not subject to temper embrittlement. It is recommended for heavy duty service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1958) 7 (6): SA-69.
Published: 01 June 1958
... RYCUT 40 is a leaded chromium-molybdenum alloy steel having high machinability rating. It is especially recommended for high production automatic machine products. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2009) 58 (4): SA-597.
Published: 01 April 2009
... treatability joinability tensile properties workability UNS K31835 CROMELSO® 22V (Chromium-Molybdenum Steel for High-Temperature Service) CromElso 22V is a specially designed low-alloy Cr-Mo steel for high-temperature hydrogen service, particularly hydro treating reactors up to 482 °C (900 °F). CromElso...
Journal Articles
Alloy Digest (2009) 58 (5): SA-600.
Published: 01 May 2009
... CromElso 91 fracture toughness heat treatability high-temperature alloys joinability tensile properties workability UNS K90901 CROMELSO® 91 (Chromium-Molybdenum Steel for High-Temperature Service) CromElso 91 is a specially designed martensitic CrMoVNb steel for high-temperature creep resistance...
Journal Articles
Alloy Digest (1968) 17 (9): SA-230.
Published: 01 September 1968
... Rycut 50 is a leaded chromium-molybdenum alloy steel having high machinability rating combined with good tensile and fatigue properties. It is recommended for gears, shafts, bolts, and other machinery parts. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1968) 17 (10): SA-232.
Published: 01 October 1968
... ISO-CAST 8 is a cast chromium-molybdenum steel recommended as a general purpose structural alloy of wide application with wide range of mechanical properties. It is used for aircraft and railroad car parts, machine tool and hammermill equipment, gears and shafts. This datasheet provides...
Journal Articles
Alloy Digest (1965) 14 (3): SA-14.
Published: 01 March 1965
... AISI 4340 steel is a tough, shock resisting, oil hardening nickel-chromium-molybdenum steel. In the heat treated condition it has the highest combination of tensile and endurance strengths along with ductility. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1974) 23 (2): SA-301.
Published: 01 February 1974
... CRUCIBLE HOLDER BLOCK is a medium-carbon chromium-molybdenum steel which affords superior machinability because of its sulfur content. It is used in such applications as holders or backers for forging dies and frames for plastic molds. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1978) 27 (1): SA-340.
Published: 01 January 1978
... UNIFLUX VCM 125 is a continuous flux-cored welding electrode (wire) that is used to deposit 1 1/4% chromium-1/2% molybdenum steel for which it was developed. Welding is protected by a shielding atmosphere of 100% carbon dioxide. This electrode also may be used to weld other low-alloy steels...
Journal Articles
Alloy Digest (1994) 43 (8): SA-478.
Published: 01 August 1994
... includes information on heat treating. Filing Code: SA-478. Producer or source: Kobe Steel Ltd. Producer or Source: Kobe Steel Ltd Copyright © ASM International® 1996 1996 ASM International chemical composition chromium-molybdenum steel fracture toughness heat treatability tensile...
Journal Articles
Alloy Digest (1994) 43 (9): SA-479.
Published: 01 September 1994
... International chemical composition chromium-molybdenum steel creep properties fracture toughness hardness heat treatability joinability tensile properties UNS K38130 3 Cr-1 Mo-1/4V-Ti-B Filing Code: Steel Alloy W-479 SEPTEMBER 1994 ALLOYS Publish&by: AWoyDiges~ Incl201~77-9161 27 CsnMd SlreeC...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... AISI 4161 is a low-alloy steel of the chromium-molybdenum type; it contains nominally 0.61% carbon. It has relatively high hardenability and good resistance to abrasion, impact and fatigue. It is an oil-hardening grade and is recommended for moderately heavy-duty service. This steel has...
Journal Articles
Alloy Digest (2020) 69 (3): TS-789.
Published: 01 March 2020
... Finkl Steel Durodi is a nickel-chromium-molybdenum-vanadium, alloy hot work tool steel that hardens deeply and uniformly to a high hardness that holds up exceedingly well under impact and thermal shock. It is designed to provide maximum abrasion and heat resistance over a full range of service...
Journal Articles
Alloy Digest (1995) 44 (6): SS-598.
Published: 01 June 1995
...-nickel steel) SANDVIK 3R65 is a molybdenum type 18-12 austenitic stainless steel having good resistance to acids. Sanclvikm is a trademark of Sandvik AB. Chemical composition, wt. % (nominal): Carbon 0.030 max. Manganese 1.7 Silicon 0.4 Phosphorus 0.040 max. SUlflX 0.030 max. Chromium 17 Nickel 11.5...
Journal Articles
Alloy Digest (1961) 10 (8): SA-118.
Published: 01 August 1961
... AISI 94B30 is a mild carbon, nickel-chromium-molybdenum-boron alloy steel having good hardenability, toughness, and shock resistance for heavy duty service. AISI 94B30H is the corresponding H-Steel which has specified hardenability limits with some modification of chemical ranges. This datasheet...