Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... BETHLEHEM 67 CHISEL is the general-purpose, tungsten-type of shock-resisting tool steel. It has excellent properties for cold battering tools and hot-work shock applications. It is characterized by unusual toughness, resistance to fatigue and relative ease of heat treatment. This datasheet...
Journal Articles
Alloy Digest (1964) 13 (10): TS-153.
Published: 01 October 1964
... METALS AND ALLOYS ALLEGHENY LUDLUM 602 Prblirbd by Enginecriag Alloys Digest, inc. Upper Montclair, New Jersey (Chisel Steel, Type 55 Mod.) Allegheny Ludlum 602 is a manganese, silica-molybdenum type, shock resisting cool steel recommended for applications where extreme roughness is required along with...
Journal Articles
Alloy Digest (1982) 31 (12): TS-408.
Published: 01 December 1982
...) diameter will water harden to the center. The extreme toughness of Type S2 makes it suitable for use in many applications where no other tool steel will hold up. Its many uses include chisels, rivet busters, spike mauls, screw drivers, punches and sledges. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1984) 33 (4): TS-422.
Published: 01 April 1984
... JESSOP SUPERSHOCK 7 is an air-hardening shock steel having excellent toughness combined with good resistance to softening at temperatures up to 1000 F. It is suitable for both hot and cold-work tooling applications that involve shock. Among its typical applications are dies, shear blades, chisels...
Journal Articles
Alloy Digest (2007) 56 (9): TS-655.
Published: 01 September 2007
... The carbon content in TLS S1, about 0.5%, produces a combination of high strength and high toughness with medium wear resistance. Chisels and rivet sets are typical applications. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture...
Journal Articles
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
... applications. Among its many uses are blanking dies, shear blades, punches and chisels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating...
Journal Articles
Alloy Digest (1983) 32 (7): TS-416.
Published: 01 July 1983
... resistance to abrasion, fatigue and wear. It is used for both hot-work and cold-work applications. Among its many uses are automotive gears, forgings, gun barrels, shafts, wrenches, chisels, punches, lathe spindles, axes, shear blades, dies, files, reamers and drills. This datasheet provides information on...
Journal Articles
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... chromium and molybdenum. It is used for both cold and hot tooling applications. Its many uses include shear blades, swaging dies, chisels and dies for molding plastics below 1000 F (538 C). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1985) 34 (8): TS-445.
Published: 01 August 1985
... within the range 400 to 600 F. Among its many applications are shear blades, punches, hand chisels and pneumatic tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS...
Journal Articles
Alloy Digest (1986) 35 (3): TS-455.
Published: 01 March 1986
... withstand repeated heating to 700-800 F, when used in lower temperature hot-work applications. Among its many uses are shear blades, hand chisels, pneumatic tools, coining dies, hot-heading dies, forging dies and machine parts. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1978) 27 (8): TS-337.
Published: 01 August 1978
... FAGERSTA M-2 is a widely used molybdenum-base high-speed steel. It is suitable for all general-purpose cutting-tool applications and it has an excellent combination of toughness and wear resistance. Its many applications include boring tools, chisels, lathe tools and shear blades. This datasheet...
Journal Articles
Alloy Digest (1979) 28 (7): TS-352.
Published: 01 July 1979
... CYCLOPS S1 (formerly Alco M) was originally developed for chisel and pneumatic tool purposes. It is now used for many other cold and hot work applications because of its outstanding toughness and resistance to fatigue. It gives excellent results in those instances where shock and impact are major...
Journal Articles
Alloy Digest (1972) 21 (9): TS-246.
Published: 01 September 1972
... AISI Type S1 is a chromium-tungsten alloy steel for general use for chisels and other cold-battering tools. Its great toughness and strength also enable it to handle many hot and cold-work tooling jobs. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2007) 56 (8): TS-654.
Published: 01 August 2007
... Thyrodur 2826 is a shock-resistant tool steel of average hardenability and intermediate alloy content compared with other tool steels with high toughness and resistance to shock. Shock-resistant steels are used primarily for chisels, rivet sets, punches, driver bits, and other applications...
Journal Articles
Alloy Digest (1987) 36 (4): TS-473.
Published: 01 April 1987
... high toughness with the advantages of oil-hardening non-deforming steels. Its relatively high hardenability coupled with high toughness makes it extremely useful for larges shear blades in severe service. Other applications include pneumatic tools, punches, hand chisels, rivet sets and pipe cutters...
Journal Articles
Alloy Digest (1987) 36 (5): TS-475.
Published: 01 May 1987
... is used for impact and shock-resisting tools. Its many uses include shear blades, chisels, punches, rivet sets and mold dies for plastics. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1979) 28 (12): TS-357.
Published: 01 December 1979
... be water quenched successfully with proper precautions. Its many uses include hammers, hand chisels, boiler punches, shear blades and pneumatic tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1982) 31 (3): TS-396.
Published: 01 March 1982
... GUTERL S-1 is a chromium-tungsten steel for general use for chisels and other cold-battering tools. It also is used for numerous other cold and hot-work applications because of its excellent toughness, high hardness and strength, and resistance to fatigue. Its many applications include...
Journal Articles
Alloy Digest (1982) 31 (6): TS-400.
Published: 01 June 1982
..., it is hardened by austenitizing and quenching in oil. Among the many uses of Mosil are hand chisels, hammers, rivet sets, concrete breakers and heavy-duty punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on...
Journal Articles
Alloy Digest (1960) 9 (1): TS-88.
Published: 01 January 1960
... chisels or other pneumatic tools, it is generally best to consider tbe three parts of the chisel separately, that is. tbe shank end, the bit or cutting end and the body of the chisel which includes the tillet portion. In many cases chisels forged from unannealed stock will be sufficiently hard on the...