Alloy Digest (1978) 27 (10): Al-33.
Published: 01 October 1978
... ALUMINUM 5083 is a non-heat-treatable wrought aluminum alloy possessing high strength, excellent welding characteristics and excellent resistance to corrosion. Among its many applications are structural towers, mobile cranes and chemical storage tanks. This datasheet provides information...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... and 2. Specification Equivalents: ISO AlMg3Mn(A) ANSI/AWS A5.10 Similar to DIN AlMg2.7Mn UNS 95554 General Characteristics: Alcotec Weld Wire 5554 was developed as a filler alloy, primari- ly for alloy 5454, which is widely used in the manufacture of chemical storage tanks, automotive wheels, and those...
Journal Articles
Alloy Digest (2016) 65 (9): Al-446.
Published: 01 September 2016
... that is widely used in the manufacture of chemical storage tanks, and in particular, those that may be subjected to stress corrosion cracking (SCC) at elevated temperatures. Product Forms Available: Altigweld filler rods in 914 mm (36 in.) straight lengths designed for gas tungsten arc (GTA) welding or brazing...
Journal Articles
Alloy Digest (1964) 13 (8): CS-21.
Published: 01 August 1964
... JLX-W is a columbium-bearing carbon steel produced in four grades according to the minimum yield point. It has good forming characteristics and excellent weldability. It is recommended where high strength and weight saving are required, such as freight cars, trucks, storage tanks, etc...
Journal Articles
Alloy Digest (1979) 28 (9): Al-157.
Published: 01 September 1979
... maximum service temperature is about 3000F. Forms Available: Sheet, plate, and tube (seamless and extruded). Applications: Hydrogen peroxide service, chemical storage vessels, unfired pressure vessels, piping, heat exchangers, steam- jacketed kettles, pumps, stills, condensers, shipping drums, tanks...
Journal Articles
Alloy Digest (1967) 16 (2): CS-26.
Published: 01 February 1967
... USS CHAR-PAC is a heat treated carbon steel having exceptionally good notch toughness as well as high strength. It is recommended for pressure vessels, low temperature storage containers, earth moving equipment, offshore drilling rigs, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (6): P-35.
Published: 01 June 1992
... applications where good corrosion resistance and some ignition resistance is useful Applications include absorption towers, storage tanks, piping and exhaust stacks. Producer: Dow Chemical USA Dow Plastics Group Midland, Minnesota 48674 Phone: 80044 14369 ...
Journal Articles
Alloy Digest (1971) 20 (7): CS-42.
Published: 01 July 1971
... BETHLEHEM RQC-60 is a heat-treated carbon steel having up to 60,000 psi yield strength in combination with good notch toughness and excellent weldability. It is engineered specifically for pressure vessels, storage tanks, and structures where low-temperature service is required. This datasheet...
Journal Articles
Alloy Digest (2013) 62 (3): SA-673.
Published: 01 March 2013
... 10028-4 X7Ni9 (1.5663) or X8Ni + QT680 (1.5662) ASTM/ASME A/SA 553 Type 1 J15 G3127 SL9N590Q General Characteristics: This alloy is an alloyed steel grade containing 9% nickel intended for the fabrication of Liquefied Natural Gas (LNG) storage tanks and welded pressure vessels designed for extra low...
Journal Articles
Alloy Digest (1982) 31 (5): SS-408.
Published: 01 May 1982
...-temperature scaling. Its many uses include architectural trim, nitric acid storage tanks and kitchen appliances. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high...
Journal Articles
Alloy Digest (1968) 17 (7): SA-228.
Published: 01 July 1968
... CREUSOT-9D6 is a weldable 9% nickel steel recommended for low temperature applications such as storage and transportation tanks, liquified gas equipment, and cryogenic structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1958) 7 (3): Al-64.
Published: 01 March 1958
... satisfac- torily by either process. Corrosion Resistance: Ahoy 5154 exhibits the same good resistance to cor- rosion as alloys 1100, 3003, 5052 and 6061, and provides inaeased strength in welded construction. Typical storage and tank car applications indude high strength hydrogen peroxide, fuming nitric...
Journal Articles
Alloy Digest (2013) 62 (4): SA-675.
Published: 01 April 2013
... Availability: CryElso 5 is available in plates 5 to 50 mm (0.2 to in.) thick. Applications: The main application is gas storage for transpiration at very low temperature, down to 120 ºC ( 184 ºF). A typical use is ethylene transpiration in bilobe tanks (LEG carrier). This alloy is typically used...
Journal Articles
Alloy Digest (2011) 60 (9): Fe-155.
Published: 01 September 2011
.... Filing Code: Fe-155. Producer or source: Nippon Yakin Kogyo Company Ltd. Producer or Source: Nippon Yakin Kogyo Company Ltd Copyright © ASM International® 2011 2011 ASM International chemical composition corrosion-resistant alloys elasticity NAS 36LG physical properties tensile...
Journal Articles
Alloy Digest (2002) 51 (7): Al-379.
Published: 01 July 2002
... controls on the elements that make up aluminum alloys used to contain the chemicals. Alloy 5654 was originally developed in 1968 to pro- vide controlled low limits of manganese and copper. The result was a filler alloy that can be used to weld tanks for storage of hydrogen peroxide. Because this alloy...
Journal Articles
Alloy Digest (2007) 56 (10): SS-1000.
Published: 01 October 2007
..., sheet, and strip product forms and is listed in ASTM A 240. Applications: Typical applications include liquefied gas storage vessels and portable gas storage tanks. This alloy is also suited for many ambient temperature structural applications such as railroad freight cars, truck trailers, coal handling...
Journal Articles
Alloy Digest (2016) 65 (1): SS-1237.
Published: 01 January 2016
..., and strip. See size availability in Fig. 5. Applications: NSSMC-NAR-SN-1: Nitric acid manufacturing equipment, 98% nitric acid storage tanks, shipping containers, and mixed acid (nitric acid sulfuric acid) tanks NSSMC-NAR-SN-5: Concentrated nitric acid heat exchangers NSSMC-NAR-SN-5: Medium...
Journal Articles
Alloy Digest (1984) 33 (9): SS-451.
Published: 01 September 1984
.... Annealed bars were cold worked and tested without stress relieving or straightening. Forms Available: Billets. bar. rod. sheet and plate Applications: Typical applications of CRllClBLE 442 comprise decorative trim. nitric acid storage tanks and tank cars. nitrogen fixationequipment and nozzles for zinc die...
Journal Articles
Alloy Digest (2010) 59 (5): SS-1064.
Published: 01 May 2010
... A manufacturing plants, carbon black manufacturing plants. Pulp and paper mills: bleaching devices, scrubbers Medical and pharmaceutical product plants: soy sauce fermentation tanks, salty mirin tanks, dressing production equipment. Salt production lines: Concentrated salt storage tanks, heated cans, evaporators...
Journal Articles
Alloy Digest (1953) 2 (5): Cu-8.
Published: 01 May 1953
... pins, forgings, iurdwm, kettles, lock washus. range boilers. springs, tanks. marine fittings, and welding wire; also welded tanks, u&red pressure VSS&, gasoline tanks, pipe, and oil storage tanks. Manmfachrer: The American Brass Company Waterbury 20, Cortnectkut ...